journal article·2026-09

Microstructure-dependent slip activation and transfer governing the strength-ductility synergy in L-PBF TC4 alloy

Wang Changshun, Li Chenglin, Han Yuting, Zheng Wenqiong, Wang Danyang, Liu Shiqi, Zhang Guodong, Yang Bing

Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Microstructure and mechanical properties · High Temperature Alloys and Creep · Orthopaedic implants and arthroplasty

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (85)

Show source-provided references
1. Effect of heat treatment on the tensile behavior of selective laser melted Ti-6Al-4V by in situ X-ray characterization10.1016/j.actamat.2020.03.003 ↗
2. Deformations of Ti-6Al-4V additive-manufacturing-induced isotropic and anisotropic columnar structures: insitu measurements and underlying mechanisms
3. In-situ investigation on the anisotropic behavior of the additively manufactured dual-phase Ti-6Al-4V alloy10.1016/j.matchar.2022.112003 ↗
4. The reverse transformation mechanism of β phase and its stability of Ti-6Al-4V alloy fabricated via laser powder bed fusion10.1016/j.matdes.2024.112926 ↗
5. Naturally high fatigue performance of a 3D printing titanium alloy across all stress ratios
6. Fatigue behavior of porous biomaterials manufactured using selective laser melting10.1016/j.msec.2013.08.006 ↗
7. Unveiling grain-scale deformation and damage and their correlations with microstructure for laser powder bed fusion Ti6Al4V10.1016/j.jallcom.2025.182878 ↗
8. Tailoring hierarchical microstructures to improve the strength and plasticity of a laser powder bed fusion additively manufactured Ti-6Al-4V alloy
9. As-Fabricated and heat-treated microstructures of the Ti-6Al-4V alloy processed by selective laser melting10.1007/s11661-011-0731-y ↗
10. Additive manufacturing of strong and ductile Ti–6Al–4V by selective laser melting via in situ martensite decomposition10.1016/j.actamat.2014.11.028 ↗
11. Micro-and meso-structures and their influence on mechanical properties of selectively laser melted Ti-6Al-4V10.1016/j.actamat.2018.05.044 ↗
12. Deciphering the transformation pathway in laser powder-bed fusion additive manufacturing of Ti-6Al-4V alloy
13. Effect of subtransus heat treatment on the microstructure and mechanical properties of additively manufactured Ti-6Al-4V alloy10.1016/j.jallcom.2017.11.263 ↗
14. Microstructural control across multiple length scales in additively manufactured Ti-6Al-4V via cyclic heat treatments10.1016/j.actamat.2025.121372 ↗
15. Effects of post-heat treatments on the microstructure and mechanical properties of Ti–6Al–4V alloy fabricated by selective laser melting10.1016/j.jmrt.2024.09.141 ↗
16. Towards isotropic behaviour in Ti–6Al–4V fabricated with laser powder bed fusion and super transus hot isostatic pressing10.1016/j.msea.2023.145094 ↗
17. Heat treatment of Ti-6Al-4V alloy manufactured by laser-based powder-bed fusion: process, microstructures, and mechanical properties correlations10.1016/j.jallcom.2021.162618 ↗
18. The microstructure and tensile properties of additively manufactured Ti–6Al–2Zr–1Mo–1V with a trimodal microstructure obtained by multiple annealing heat treatment10.1016/j.msea.2021.142241 ↗
19. Static coarsening behaviour of lamellar microstructure in selective laser melted Ti–6Al–4V10.1016/j.jmst.2019.04.008 ↗
20. Strength/ductility trade-off of laser powder bed fusion Ti-6Al-4V: synergetic effect of alpha-case formation and microstructure evolution upon heat treatments
21. Realizing superior ductility of selective laser melted Ti-6Al-4V through a multi-step heat treatment10.1016/j.msea.2020.140367 ↗
22. Optimal tensile properties of laser powder bed fusion hereditary basket-weave microstructure in additive manufactured Ti6Al4V
23. Improving the mechanical performance of L-PBF Ti-6Al-4V alloy by thermal cycling for trimodal α+α′ structure formation10.1016/j.msea.2025.149472 ↗
24. Globularization using heat treatment in additively manufactured Ti-6Al-4V for high strength and toughness10.1016/j.actamat.2018.09.064 ↗
25. Selective laser melting of near-α titanium alloy Ti-6Al-2Zr-1Mo-1V: parameter optimization, heat treatment and mechanical performance10.1016/j.jmst.2020.05.004 ↗
26. Effects of annealing-tailored microstructure on mechanical properties and deformation behaviors of additively manufactured Ti-6Al-4V alloy
27. Effects of the morphology of grain boundary α-phase on the anisotropic deformation behaviors of additive manufactured Ti–6Al–4V10.1016/j.matdes.2022.111150 ↗
28. Investigation of inhomogeneous plastic deformation behavior of LDED TA15 alloy using in-situ EBSD tensile technique10.1016/j.msea.2025.148301 ↗
29. In situ EBSD investigation of microtexture evolution and slip activation of α macrozones during tensile deformation in Ti-6Al-4V alloy
30. In-situ investigation of tensile behaviors of Ti–6Al alloy with extra low interstitial10.1016/j.msea.2021.140958 ↗
31. In-situ investigation into the deformation behavior of Ti-6Al-4V processed by laser powder bed fusion10.1016/j.matchar.2022.112434 ↗
32. Deformation and failure mechanisms of Ti–6Al–4V as built by selective laser melting10.1016/j.msea.2019.138456 ↗
33. Slip band–grain boundary interactions in commercial-purity titanium10.1016/j.actamat.2014.05.015 ↗
34. In situ SEM investigation of slip transfer in Ti-6Al-4V: effect of applied stress10.1016/j.msea.2017.10.058 ↗
35. A microstructure-based fatigue model for additively manufactured Ti-6Al-4V, including the role of prior β boundaries10.1016/j.ijplas.2023.103569 ↗
36. Influence of friction and back stresses evolution on cyclic softening of laser powder bed fusion Ti-6Al-4V ELI alloy
37. Oxygen-mediated high uniform plasticity in α-β titanium alloys10.1038/s41467-025-65851-4 ↗
38. Accurate determination of active slip systems for improved geometrical criteria of basal-to-basal slip transfer at grain boundaries in pure Mg10.1016/j.actamat.2022.118536 ↗
39. Underlying slip/twinning activities of Mg-xGd alloys investigated by modified lattice rotation analysis10.1016/j.jma.2021.06.008 ↗
40. Refinement of the grain structure of additive manufactured titanium alloys via epitaxial recrystallization enabled by rapid heat treatment10.1016/j.scriptamat.2020.01.027 ↗
41. Microstructure and mechanical evolution behavior of LPBF (laser powder bed fusion)-fabricated TA15 alloy10.1016/j.jallcom.2021.159639 ↗
42. Microstructure and fatigue crack growth behavior of heat-treated electron beam melted Ti-6Al-4V alloy10.1016/j.ijfatigue.2024.108543 ↗
43. Dynamic α globularization in laser powder bed fusion additively manufactured Ti-6Al-4V10.1016/j.actamat.2023.119076 ↗
44. Phase transformations during cooling in α+β titanium alloys10.1016/S0921-5093(97)00802-2 ↗
45. Deciphering the impact toughening mechanism of α+β titanium alloy with lamellar microstructure: from crack initiation and propagation perspectives10.1016/j.jmst.2025.05.068 ↗
46. Ductility of a Ti‐6Al‐4V alloy produced by selective laser melting of prealloyed powders10.1108/13552541011083371 ↗
47. Influence of minor addition of boron on tensile and fatigue properties of wrought Ti–6Al–4V alloy10.1016/j.msea.2012.01.119 ↗
48. Effects of defects on mechanical properties in metal additive manufacturing: a review focusing on X-ray tomography insights10.1016/j.matdes.2019.108385 ↗
49. New insights on cellular structures strengthening mechanisms and thermal stability of an austenitic stainless steel fabricated by laser powder-bed-fusion10.1016/j.actamat.2020.11.018 ↗
50. Construction of multi-scale heterostructures via localized electropulsing treatment for synergistic strength-ductility enhancement in Cu-Ti alloys10.1016/j.jmst.2025.08.060 ↗
51. High-strength titanium alloy with hierarchical-microstructure design via in-situ refinement-splitting strategy in additive manufacturing
52. Achieving superior ductility for laser solid formed extra low interstitial Ti-6Al-4V titanium alloy through equiaxial alpha microstructure10.1016/j.scriptamat.2017.11.021 ↗
53. Investigating the microstructural evolution during deformation of laser additive manufactured Ti–6Al–4V at 400 °C using in-situ EBSD10.1016/j.msea.2021.141761 ↗
54. Microstructural and texture evolution investigation of laser melting deposited TA15 alloy at 500°C using in-situ EBSD tensile test10.1016/j.msea.2022.144062 ↗
55. Mesoscale deformation mechanisms in relation with slip and grain boundary sliding in TA15 titanium alloy during tensile deformation10.1016/j.jmst.2021.05.008 ↗
56. Deformation mechanism of ferrite in a low carbon Al-killed steel: slip behavior, grain boundary evolution and GND development10.1016/j.msea.2022.143093 ↗
57. Simultaneous improvement of strength and elongation of laser melting deposited Ti-6Al-4V titanium alloy through three-stage heat treatment10.1016/j.jmatprotec.2022.117607 ↗
58. Hierarchical anisotropic material response of directed energy deposited (DED) Ti-6Al-4V alloy10.1016/j.actamat.2024.120080 ↗
59. Deformation modes and fracture behaviors of peak-aged Mg-Gd-Y alloys with different grain structures10.1016/j.jma.2023.09.020 ↗
60. Anisotropic fatigue performance of directed energy deposited Ti-6Al-4V: effects of build orientation10.1016/j.msea.2023.145112 ↗
61. Slip-twinning interdependent activation across phase boundaries: an in-situ investigation of a Ti-Al-V-Fe (α+β) alloy10.1016/j.actamat.2020.116520 ↗
62. Activation of second-order pyramidal slip and other secondary mechanisms in solid solution Mg-Zn alloys and their effect on tensile ductility10.1016/j.actamat.2022.118555 ↗
63. Superior strength-ductility synergy in TiZrNbVAl high entropy alloys via additive manufacturing10.1016/j.actamat.2025.121389 ↗
64. ECCI analysis of shear accommodations at grain boundaries in commercially pure alpha titanium10.1016/j.ijplas.2020.102731 ↗
65. Compatibility of dependence on deformation in two-phase Ti-AI alloys: microstructure and orientation relationships10.1007/BF02670762 ↗
66. Fracture and fatigue in additively manufactured metals10.1016/j.actamat.2021.117240 ↗
67. Discovering the role of the defect morphology and microstructure on the deformation behavior of additive manufactured Ti–6Al–4V10.1016/j.msea.2022.144202 ↗
68. Influence of defects on mechanical properties of Ti–6Al–4V components produced by selective laser melting and electron beam melting10.1016/j.matdes.2015.07.147 ↗
69. High power laser powder bed fusion of Ti6Al4V alloy: the control of defects, microstructure, and mechanical properties10.1016/j.jmrt.2024.10.152 ↗
70. Effects of heat treatment below beta transus temperature on the microstructure and mechanical properties of Ti–6Al–4V alloy fabricated by selective laser melting10.1016/j.jmrt.2025.10.013 ↗
71. Elimination of oxygen sensitivity in α-titanium by substitutional alloying with Al10.1038/s41467-021-26374-w ↗
72. Size effects in strength and plasticity of single-crystalline titanium micropillars with prismatic slip orientation10.1016/j.scriptamat.2011.05.033 ↗
73. Experimental evaluation of critical resolved shear stress for the first-order pyramidal c + a slip in commercially pure Ti by micropillar compression method10.1016/j.actamat.2020.06.043 ↗
74. A study of active deformation systems in titanium alloys: dependence on alloy composition and correlation with deformation texture10.1016/S0921-5093(02)00421-5 ↗
75. Dislocation slip and crack nucleation mechanism in dual-phase microstructure of titanium alloys: a review10.1007/s40195-022-01505-4 ↗
76. Analysis of the different slip systems activated by tension in a α/β titanium alloy in relation with local crystallographic orientation10.1016/j.actamat.2004.09.040 ↗
77. The effect of aluminium on twinning in binary alpha-titanium10.1016/j.actamat.2015.09.048 ↗
78. Grain size effect on deformation mechanisms and mechanical properties of titanium10.1016/j.msea.2019.138721 ↗
79. Texture of nanocrystalline nickel: probing the lower size limit of dislocation activity10.1126/science.1228211 ↗
80. Origin of back stress generation during tensile deformation of a heterostructured titanium alloy: an in-situ EBSD study on local slip system activation10.1016/j.jmrt.2025.07.239 ↗
81. Solid solution strengthening of hexagonal titanium alloys: restoring forces and stacking faults calculated from first principles10.1016/j.actamat.2015.09.041 ↗
82. Ex-situ study on mechanical properties and deformation mechanism of three typical microstructures in TA19 titanium alloy10.1016/j.matchar.2020.110521 ↗
83. Heat treatment of Ti6Al4V produced by selective laser melting: microstructure and mechanical properties10.1016/j.jallcom.2012.07.022 ↗
84. Effect of heat treatment on the phase transformation and mechanical properties of Ti6Al4V fabricated by selective laser melting10.1016/j.jallcom.2018.06.076 ↗
85. Microstructural analysis on boundary sliding and its accommodation mode during superplastic deformation of Ti–6Al–4V alloy10.1016/S0921-5093(98)01157-5 ↗