The role of surface roughness on hydrogen embrittlement of electron beam powder bed fusion Ti−6Al−4V

Paula Endrös, Nima Razavi, Liesbet Deconinck, Roy Johnsen, Xu Lu

Abstract

Hydrogen−assisted cracking remains a critical challenge for titanium alloys exposed to hydrogen environments. In this study, the hydrogen−assisted cracking of electron beam powder bed fusion (PBF−EB) Ti−6Al−4V was investigated, focusing on the effect of surface condition. Slow strain rate tests (at 10 −6 s −1 ) were carried out under in−situ electrochemical charging at −5 mA cm −2 in a 3.5 wt.% NaCl solution on specimens with machined (Ra of 3 μm) and as−built (Ra of 27 μm) surface conditions. Fracture behavior and hydrogen−affected microstructural features were characterized using scanning electron microscopy and scanning transmission electron microscopy. Hydrogen−assisted degradation was observed for both surface conditions. However, the depth of the hydrogen−affected fracture zone decreased from approximately 2 mm in machined specimens to approximately 0.5 mm in as−built specimens. Correspondingly, the reduction in ductility was lower in as−built specimens (20 ± 13%) compared to machined specimens (35 ± 25%). Fracture morphology exhibited a transition with increasing distance from the surface. Within 100 to 500 μm from the surface, regions of higher hydrogen content showed hydride−assisted quasi−cleavage fracture. In contrast, regions at greater depths dominated by solute hydrogen showed mainly transgranular cracking controlled by phase−dependent plasticity within the lamellar α/β microstructure. The continuous β−phase network characteristic of the PBF–EB microstructure appeared to promote hydrogen transport, leading to a relatively high apparent effective hydrogen diffusivity of approximately 1.6 × 10 −11 m 2 s −1 . Under the investigated conditions, the results indicate that the as−built surface condition reduces the extent of hydrogen−assisted cracking in PBF−EB Ti−6Al−4V. • As-built surfaces reduced H-affected fracture depth (2 mm to 0.5 mm). • As-built specimens showed lower HE index than machined (20% vs 35%). • Fracture changed from hydride-assisted quasi-cleavage to transgranular as H decreased. • The β-phase network enhanced H transport (D eff of 10 -11 m 2 s -1 ).
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Pulsed Power Technology Applications · High Entropy Alloys Studies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (64)

Show source-provided references
1. 2023
2. U.S. Energy Information Administration, International Energy Outlook 2023 (IEO2023), U.S. Department of Energy, n.d. https://www.eia.gov/outlooks/ieo/.
3. The Paris Agreement (COP21) · 2018
4. Green hydrogen-based E-fuels (E-methane, E-methanol, E-ammonia) to support clean energy transition: a literature review10.1016/j.ijhydene.2023.03.240 ↗
5. Ceu · 2022
6. Hydrogen embrittlement as a conspicuous material challenge─comprehensive review and future directions10.1021/acs.chemrev.3c00624 ↗
7. Lee · 2016
8. Lûtjering · 2007
9. Structure and properties of titanium and titanium alloys
10. The mechanism of hydride formation during electrochemical hydrogen charging of Ti–6Al–4V
11. Insights into the formation of titanium hydrides from first principles calculations10.1016/j.actamat.2024.119921 ↗
12. Hydrogenation-induced lattice expansion and its effects on hydrogen diffusion and damage in Ti–6Al–4V10.1016/j.actamat.2020.02.029 ↗
13. Hydriding of titanium: recent trends and perspectives in advanced characterization and multiscale modeling10.1016/j.cossms.2022.101020 ↗
14. 1992
15. Hydrogen embrittlement in Ti–6Al–4V: a comparative review of conventional and additive manufacturing10.1016/j.ijhydene.2025.151710 ↗
16. In-situ hydrogen embrittlement evaluation of as-built and heat treated laser powder bed fused Ti-6Al-4V versus conventionally cold rolled Ti-6Al-4V
17. The effects of hydrogen on the deformation and fracture of β-titanium10.1016/S1359-6454(01)00301-9 ↗
18. Hydrogen-Assisted degradation of titanium based alloys10.2320/matertrans.45.1594 ↗
19. The synergistic action and interplay of hydrogen embrittlement mechanisms in steels and iron: localized plasticity and decohesion10.1016/j.engfracmech.2019.106528 ↗
20. Stress corrosion cracking (SCC) and hydrogen-assisted cracking in titanium alloys
21. Interplay between H atoms and characteristic microstructure features in 2100 MPa grade full pearlite steel wire for bridge cable10.1016/j.ijhydene.2025.151226 ↗
22. Additive manufacturing of Ti6Al4V alloy: a review10.1016/j.matdes.2018.107552 ↗
23. Mechanical behavior of electrochemically hydrogenated electron beam melting (EBM) and wrought Ti–6Al–4V using small punch test10.1016/j.ijhydene.2021.11.231 ↗
24. Hydrogen effects on electrochemically charged additive manufactured by electron beam melting (EBM) and wrought Ti–6Al–4V alloys10.1016/j.ijhydene.2020.06.277 ↗
25. Hydrogen trapping in additive manufactured Ti–6Al–4V alloy10.1016/j.msea.2021.141050 ↗
26. The mechanism behind the effect of building orientation and surface roughness on hydrogen embrittlement of laser powder bed fused Ti-6Al-4V
27. Surface roughness improvement of Ti-6Al-4V alloy overhang structures via process optimization for laser-powder bed fusion10.1016/j.jmapro.2024.01.008 ↗
28. Roughening improves hydrogen embrittlement resistance of Ti-6Al-4V10.1016/j.actamat.2021.117304 ↗
29. Anisotropy and heterogeneity of microstructure and mechanical properties in metal additive manufacturing: a critical review10.1016/j.matdes.2017.11.021 ↗
30. Improvement of fatigue resistance and ductility of TiAl6V4 processed by selective laser melting10.1016/j.jmatprotec.2015.01.025 ↗
31. Microstructure evolution and enhanced wear and corrosion resistance of additively manufactured TA1 pure titanium by hybrid electric-ultrasonic burnishing10.1016/j.engfailanal.2026.110667 ↗
32. Effect of additive manufacturing and subsequent heat and/or surface treatment on the hydrogen embrittlement sensitivity of 316L austenitic stainless steel10.1016/j.ijhydene.2023.05.215 ↗
33. The hydrogen embrittlement of pure Ni fabricated by additive manufacturing10.1016/j.ijhydene.2023.01.167 ↗
34. Electrochemical hydrogen-charging effect on the microstructural evolution and mechanical behavior of deformed Ti alloy10.3390/ma18030518 ↗
35. A review of the data on the interlamellar spacing of pearlite10.1007/BF02644694 ↗
36. Effect of part thickness and build angle on the microstructure, surface roughness, and mechanical properties of additively manufactured IN-93910.1007/s11661-022-06940-7 ↗
37. Effect of strain rate on hydrogen embrittlement of Ti6Al4V alloy10.3390/ma17051100 ↗
38. Uncovering the hydride orientation-mediated hoop fatigue mechanism in a zirconium alloy cladding tube10.1016/j.ijplas.2022.103440 ↗
39. Hydrogen embrittlement of α titanium: in situ tem studies10.1016/0001-6160(88)90032-6 ↗
40. Directed energy deposition versus wrought Ti‐6Al‐4V: a comparison of microstructure, fatigue behavior, and notch sensitivity10.1002/adem.201900220 ↗
41. Heat treatment effects on the hydrogen embrittlement of Ti6Al4V fabricated by laser beam powder bed fusion
42. Tensile deformation mechanism and micro-void nucleation of Ti-55531 alloy with bimodal microstructure10.1016/j.jmrt.2020.11.008 ↗
43. Influence of high-pressure gaseous hydrogen on the low-cycle fatigue and fatigue crack growth properties of a cast titanium alloy10.1016/j.msea.2014.06.060 ↗
44. Hydrogen embrittlement10.1016/B978-0-12-341825-8.50014-3 ↗
45. Influence of electrochemically charged hydrogen on mechanical properties of Ti-6Al-4V alloy additively manufactured by laser powder bed fusion (L-PBF) process10.1016/j.msea.2022.144339 ↗
46. Microvoids in electrochemically hydrogenated titanium-based alloys10.1016/j.ijhydene.2021.05.187 ↗
47. Hydrogen effects in titanium alloys
48. Crystallographic orientation dependence of hydride precipitation in commercial pure titanium10.1016/j.actamat.2019.11.027 ↗
49. Microstructural evolution and formation mechanism of FCC titanium hydride in Ti–6Al–4V–xH alloys10.1016/j.jallcom.2006.02.058 ↗
50. Surface concentration and microscale distribution of hydrogen and the associated embrittlement in a near α titanium alloy10.1016/j.jallcom.2021.158669 ↗
51. Rhodes · 1979
52. Effect of hydrogen and strain rate upon the ductility of mill-annealed Ti6Al4V10.1016/S0010-938X(98)00109-7 ↗
53. Effects of hydrogen as a solid solution element on the deformation behavior of a near-alpha titanium alloy10.1016/j.msea.2021.141269 ↗
54. The formation of hydride and its influence on Ti–6Al–4V alloy fracture behavior10.1016/j.ijhydene.2023.05.226 ↗
55. Hydrogen embrittlement of a metastable β-titanium alloy10.1016/j.actamat.2004.05.030 ↗
56. Hydrogen-dislocation interaction in relation to hydrogen embrittlement and enhanced plasticity of metals10.1016/j.ijhydene.2023.10.303 ↗
57. An investigation on structure, deformation and fracture of hydrides in titanium with a large range of hydrogen contents10.1016/j.actamat.2004.04.024 ↗
58. Hydrogen-surface interaction from first-principles calculations and its implication to hydrogen embrittlement mechanisms of titanium10.1016/j.apsusc.2023.156871 ↗
59. Structure and mobility of -type screw dislocation in presence of H in α-Ti from first-principles10.1016/j.actamat.2023.118842 ↗
60. Probing the effect of solute hydrogen and hydrides on the prismatic slip of [ 2 1 ‾ 1 ‾ 0 ] -orientated alpha titanium using in-situ micropillar compression10.1016/j.scriptamat.2025.116859 ↗
61. Improving the mechanical processing of titanium by hydrogen doping: a first-principles study10.1016/j.ijhydene.2018.02.066 ↗
62. Influence of nonmetallic interstitials on the phase transformation between FCC and HCP titanium: a density functional theory study10.3390/met12101607 ↗
63. Influence of defects, surface roughness and HIP on the fatigue strength of Ti-6Al-4V manufactured by additive manufacturing10.1016/j.ijfatigue.2018.07.020 ↗
64. Additive manufacturing: effects of defects