Effects of heat treatment on microstructure and high-temperature tensile property of a LPBF fabricated IN939G superalloy with the high-carbon content
Bibliographic record
Abstract
No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.
Source: Not provided · Quality: missing
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · High Temperature Alloys and Creep · High Entropy Alloys Studies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (55)
Show source-provided references
1. Effect of temperature on tensile behavior, fracture morphology, and deformation mechanisms of Nickel-based additive manufacturing 939 superalloy10.1016/j.jallcom.2023.170559 ↗
2. Additive manufacturing of CMSX-4 Ni-base superalloy by selective laser melting: influence of processing parameters and heat treatment
3. High-temperature mechanical properties of IN718 alloy: Comparison of additive manufactured and wrought samples10.3390/cryst10080689 ↗
4. Effect of remelting on cracking of inconel 939 fabricated via laser powder bed fusion10.1016/j.matchar.2024.114087 ↗
5. Enhanced crack resistance and mechanical properties of laser powder bed fusion Inconel 939 via carbon-induced carbide precipitation10.1016/j.msea.2025.149229 ↗
6. Metal 3D printing as a disruptive technology for superalloys10.1038/s41467-020-16188-7 ↗
7. Multiscale evolution of TiC particles in GH3536-based composites fabricated via laser powder bed fusion: coarsening mechanisms and hierarchical distribution10.1088/2631-7990/ae3b82 ↗
8. Effect of Zr content on crack formation and mechanical properties of IN738LC processed by selective laser melting10.1016/S1003-6326(21)65582-6 ↗
9. Combining alloy and process modification for micro-crack mitigation in an additively manufactured Ni-base superalloy
10. A criterion for cracking during solidification10.1016/j.actamat.2015.01.034 ↗
11. Alloys-by-design: application to new superalloys for additive manufacturing10.1016/j.actamat.2020.09.023 ↗
12. Additive manufacturing of Ni-based superalloys: residual stress, mechanisms of crack formation and strategies for crack inhibition10.1016/j.nanoms.2022.08.001 ↗
13. Additive manufacturing of strong and ductile In939+TiB2 by laser powder bed fusion10.1016/j.msea.2025.148446 ↗
14. Grain refinement and crack inhibition of hard-to-weld Inconel 738 alloy by altering the scanning strategy during selective laser melting10.1016/j.matdes.2021.109940 ↗
15. The influence of the process parameters on the densification and microstructure development of laser powder bed fused inconel 93910.3390/met10070882 ↗
16. Cracking behaviour and its suppression mechanisms with TiB2 additions in the laser additive manufacturing of solid-solution-strengthened Ni-based alloys10.1016/j.compositesb.2023.111023 ↗
17. Selective laser melting of Hastelloy X nanocomposite: effects of TiC reinforcement on crack elimination and strength improvement10.1016/j.compositesb.2020.108442 ↗
18. Crack reduction in Inconel 939 with Si addition processed by laser powder bed fusion additive manufacturing
19. The effect of boron and zirconium on the microcracking susceptibility of IN-738LC derivatives in laser powder bed fusion10.1016/j.apsusc.2021.151541 ↗
20. Effect of carbon content on the microstructure, tensile properties and cracking susceptibility of IN738 superalloy processed by laser powder bed fusion
21. Hot cracking mechanism affecting a non-weldable Ni-based superalloy produced by selective electron Beam melting10.1016/j.actamat.2017.09.047 ↗
22. Laser powder bed fusion of high-strength crack-free Al7075 alloy with the in-situ formation of TiB2/Al3Ti-reinforced phases and nucleation agents10.1016/j.compositesb.2024.111940 ↗
23. Defects caused by powder spattering and entrainment in laser powder bed fusion process: high-fidelity modeling of gas, melt pool and powder dynamics10.1016/j.actamat.2025.120816 ↗
24. Versatile fluidity test model for cast superalloys and comparison between IN718 and IN93910.1016/S1003-6326(24)66582-9 ↗
25. The dynamics of reinforced particle migration in laser powder bed fusion of Ni-based composite10.1016/j.powtec.2021.09.005 ↗
26. Review of data for the surface tension of pure metals10.1179/imr.1993.38.4.157 ↗
27. Multiphysics modelling of lack-of-fusion voids formation and evolution in IN718 made by multi-track/multi-layer L-PBF10.1016/j.ijheatmasstransfer.2019.05.003 ↗
28. On conventional versus direct ageing of Alloy 71810.1016/j.actamat.2018.06.034 ↗
29. Mechanical properties of pure Ni and Ni-alloy substrate materials for Y–Ba–Cu–O coated superconductors10.1016/j.cryogenics.2006.01.014 ↗
30. Modeling solid solution strengthening in nickel alloys10.1007/s11661-997-0268-2 ↗
31. On the prediction of the yield stress of unimodal and multimodal γ′ Nickel-base superalloys10.1016/j.actamat.2015.07.048 ↗
32. Dynamic mechanical behaviour and dislocation substructure evolution of Inconel 718 over wide temperature range10.1016/j.msea.2011.04.079 ↗
33. Tailoring the strength and ductility of T91 steel by partial tempering treatment10.1016/j.actamat.2019.02.043 ↗
34. Influence of scandium addition on microstructure and mechanical properties in nickel-based superalloys: an integrated multiscale modeling and experimental approach10.1016/j.ijplas.2023.103703 ↗
35. Modeling the competition between solid solution and precipitate strengthening of alloys in a 3D space10.1016/j.ijplas.2021.103152 ↗
36. Mesoscopic simulation of thermal dynamics in melt pool and melting behavior of individual powder particles during NiTi alloys fabrication by μ-LPBF
37. Anomalous anisotropy in an additively manufactured solid-solution-strengthened superalloy from room to elevated temperatures10.1016/j.ijplas.2025.104409 ↗
38. Enhancing tensile and creep properties of Inconel 617 superalloy via regulating the synergistic evolution of M23C6 carbides and γ′ phases10.1016/j.msea.2024.147523 ↗
39. Superior mechanical properties for an additively manufactured crack-free Ni-based superalloy with an inherited metastable microstructure after heat treatment10.1016/j.jmrt.2025.05.064 ↗
40. Understanding the high-temperature deformation behavior of additively manufactured γ'-forming Ni-based alloys by microstructure heterogeneities-integrated creep modelling
41. Portevin-Le Châtelier effect in wrought Ni-based superalloys: experiments and mechanisms10.1016/j.jmst.2020.03.023 ↗
42. Effect of heat treatment and hot isostatic pressing on the structure and mechanical properties of Inconel 939 manufactured via casting and LPBF10.1016/j.jmapro.2025.04.082 ↗
43. Two-step heat treatment for laser powder bed fusion of a nickel-based superalloy with simultaneously enhanced tensile strength and ductility
44. Laser powder bed fusion of GH4099 superalloy: parameter optimization and effect of heat treatment on microstructure and mechanical properties
45. High-temperature behavior of additively manufactured Haynes 214: ductility loss and deformation mechanisms transition
46. Using post-processing heat treatments to elucidate precipitate strengthening of additively manufactured superalloy 718
47. Thin-wall effects and anisotropic deformation mechanisms of an additively manufactured Ni-based superalloy
48. Unveiling the temperature-dependent tensile behavior of additively manufactured superalloys with varying carbon contents10.1016/j.msea.2025.147897 ↗
49. High resolution electron back-scatter diffraction analysis of thermally and mechanically induced strains near carbide inclusions in a superalloy10.1016/j.actamat.2010.09.030 ↗
50. Design of a novel crack-free precipitation-strengthened nickel-based superalloy and composites for laser powder bed fusion10.1080/17452759.2023.2224769 ↗
51. Dupont · 2011
52. Microstructural evolution and high-temperature strengthening mechanisms of the IN 738LC superalloy prepared by selective laser melting10.1016/j.jmrt.2024.02.219 ↗
53. Dislocation network in additive manufactured steel breaks strength–ductility trade-off10.1016/j.mattod.2017.11.004 ↗
54. Laser powder bed fusion of a novel crack-free γ′ phase-strengthened Ni-Based alloy10.3390/ma18020237 ↗
55. Shear banding mediated fracture mechanisms in additively manufactured IN738 superalloys under low-strain-rate loading10.1016/j.ijplas.2025.104296 ↗