journal article·2026-06Open access

On the improvement of the Charpy impact response of high-Mn steel (HMS) alloys via Ti addition for comminution circuits

Abhinav Karanam, Lava Kumar Pillari, Arnab Sarkar, Lukas Bichler

Abstract

High-Mn Steel (HMS) alloys due to their high impact toughness see extensive use in the comminution circuits in the mineral processing and bulk material handling industries. Higher throughput, a common practice being observed in the mineral processing plants, has increased the typical in-service stress conditions. Thus, the motivation for the current work was the need to improve the impact toughness of the commonly used steels in this application. This current work focuses on the influence of Ti addition to HMS alloys, on the microstructural characteristics and the deformation behaviour of the alloys when subjected to Charpy impact testing. The addition of Ti to the alloy composition of the HMS alloys, resulted in the in-situ formation of Titanium Carbide (TiC) particles during solidification, which further facilitated the refinement of the austenitic grain size. It was observed that, the refinement of the austenitic grains coupled with the dispersion of the TiC particles in the microstructure, contributed to the enhancement in the impact toughness; however, they concurrently reduced the lateral distortion and limited the extent of plastic deformation during impact loading. A detailed investigation of the strengthening mechanisms contributing to the impact toughness of the 0wt.% Ti and 0.15wt.% Ti alloys revealed that apart from the dispersion strengthening, the presence of the TiC particles in the 0.15wt.% Ti composite material contributed to the strengthening through the mechanisms of Orowan strengthening, load transfer and particle-stimulated nucleation of twins. The combined contribution of these additional strengthening mechanisms in the 0.15wt.% Ti composite bolstered the material's impact properties.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Microstructure and Mechanical Properties of Steels · Powder Metallurgy Techniques and Materials · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (100+)

Show source-provided references
1. Advanced comminution modelling: part 1 – crushers10.1016/j.apm.2020.06.049 ↗
2. Influence of impact velocity on fragmentation and the energy efficiency of comminution10.1016/j.ijimpeng.2006.09.063 ↗
3. Developing an experimental procedure for charge media wear prediction10.1016/S0892-6875(00)00080-7 ↗
4. In-service performance of high-manganese steel clinker crusher hammer10.1007/s40962-021-00646-z ↗
5. Microstructure evolution and austenitic grain refinement of Ti-Modified high Mn steels during solution annealing heat treatment10.1007/s11661-023-07254-y ↗
6. Heat-treatment processing of austenitic manganese steels
7. Subramanyam · 1990 · vol. 1 · 822
8. Chapter 8 - advanced alloys
9. Kuyucak · 2004 · vol. 9 · 701
10. Effect of chemical composition and heat treatments on the microstructure and wear behavior of manganese steel10.1007/s40962-020-00479-2 ↗
11. Microstructural characterization of Hadfield austenitic manganese steel10.1007/s10853-008-2759-y ↗
12. Agunsoye JO, Talabi SI. Properties optimization of hadfield austenitic manganese steel casting. Int. J. Eng. n.d.
13. Peters NW. THE PERFORMANCE OF HADFIELD’S MANGANESE STEEL AS IT RELATES TO MANUFACTURE n.d.
14. Microstructure of cast high-manganese steel containing titanium10.1515/afe-2016-0103 ↗
15. Effect of carbon and manganese content on the microstructure and mechanical properties of high manganese austenitic steel10.2298/JMMB191111009G ↗
16. Enhancing wear performance: the role of in situ TiC formation in austenitic high-Mn steel under dry reciprocating wear conditions10.1007/s10853-025-11058-3 ↗
17. Effect of titanium on the microstructure and mechanical properties of high-carbon martensitic stainless steel 8Cr13MoV10.3390/met6080193 ↗
18. Developments in austenitic steels containing manganese10.1179/imr.1989.34.1.69 ↗
19. Investigating the effect of titanium addition on the wear resistance of hadfield steel10.1051/metal/2014044 ↗
20. Impact wear resistance of in-situ TiC particles reinforced Mn18Cr2 steel dual-scale architecture composites10.1016/j.ceramint.2024.04.246 ↗
21. Development of TiC reinforced austenitic manganese steel10.1179/1879139514Y.0000000140 ↗
22. Austenitic steels: non-stainless
23. Study on work hardening behaviour and mechanism of high silicon austenitic high manganese steel10.3724/SP.J.1037.2012.00221 ↗
24. Effects of impact energy on the wear resistance and work hardening mechanism of medium manganese austenitic steel10.1007/s40544-017-0158-6 ↗
25. On deformation behavior of Fe-Mn based structural alloys10.1016/j.mser.2017.09.002 ↗
26. Strain hardening and heterogeneous deformation during twinning in Hadfield steel10.1016/j.actamat.2009.10.054 ↗
27. Mechanism of work hardening in Hadfield manganese steel10.1007/BF02648339 ↗
28. Strain aging of austenitic Hadfield manganese steel10.1016/S1359-6454(98)00347-4 ↗
29. Critical assessment 19: stacking fault energies of austenitic steels10.1080/02670836.2015.1114252 ↗
30. Stacking fault energy and deformation mechanisms in Fe-xMn-0.6C-yAl TWIP steel10.1016/j.msea.2016.08.106 ↗
31. Effect of stacking fault energy on work hardening behaviors in fe–mn–si–c high manganese steels by varying silicon and carbon contents10.1016/j.matdes.2015.07.072 ↗
32. Temperature effect on stacking fault energy and deformation mechanisms in titanium and titanium-aluminium alloy10.1038/s41598-020-60013-6 ↗
33. Stacking fault energy maps of fe–mn–al–c–si steels: effect of temperature, grain size, and variations in compositions10.1115/1.4033632 ↗
34. Derivation and variation in composition-dependent stacking fault energy maps based on subregular solution model in high-manganese steels10.1007/s11661-009-0050-8 ↗
35. Effect of substitutional alloying elements on the stacking fault energy in austenitic steels10.1134/S0036029521100086 ↗
36. ASTM E23-24 Standard Test Methods for Notched bar Impact Testing of Metallic Materials n.d. https://doi.org/10.1520/E0023-24.10.1520/E0023-24 ↗
37. Porter · 2009
38. Equilibrium partition coefficients in iron-based alloys10.1007/BF02825596 ↗
39. Porter · 2009 · 115
40. Relating microstructures of hierarchical tertiary phases with corrosion performance in a super duplex stainless steel10.1016/j.matchar.2022.112426 ↗
41. Correlations between the calculated stacking fault energy and the plasticity mechanisms in fe–mn–c alloys10.1016/j.msea.2004.01.059 ↗
42. Thermodynamic calculation of stacking fault energy of the Fe-Mn-Si-C high manganese steels10.1016/j.msea.2014.01.046 ↗
43. Calculation of stacking fault energy and its influence on abrasive wear resistance of Hadfield cast steel cooled at different rates10.17580/cisisr.2016.01.06 ↗
44. Stacking fault energy of cryogenic austenitic steels10.1088/1009-1963/11/6/315 ↗
45. Effects of Mn content on austenite stability and mechanical properties of low Ni alumina-forming austenitic heat-resistant steel: a first-principles study10.1038/s41598-023-32968-9 ↗
46. Development and characterization of a novel Ti-Modified High-Si Medium-Mn steel possessing ultra-high strength and reasonable ductility after hot rolling10.1007/s11665-018-3480-x ↗
47. Chapter 5 - dislocations in face-centered Cubic metals
48. Cracks in high-manganese cast steel
49. Common failures of Hadfield steel in application
50. Havel · 2017
51. The effect of the austenite grain refinement on the tensile and impact properties of cast Hadfield steel
52. Effect of grain size and heat treatment upon impact-toughness at low temperatures of medium carbon forging steel10.6028/jres.027.006 ↗
53. Morris · 2001
54. Beyond the dynamic hall-petch effect: mechanical twinning for microscopic strain delocalization10.1016/j.scriptamat.2024.116346 ↗
55. TWIP steels: mechanical and metallurgical properties -A review
56. Fracture appearance and mechanisms of deformation and fracture: references
57. González-Velázquez · 2018 · vol. 3 · 49
58. Failure of metals I: Brittle and ductile fracture10.1016/j.actamat.2015.12.034 ↗
59. Void-induced ductile fracture of metals: experimental observations10.3390/ma15186473 ↗
60. The tensile fracture of ductile metals
61. Ductile fracture in metals10.1080/14786435908238272 ↗
62. A comparison of ductile and fatigue fractures
63. Competing failure mechanisms in metal matrix composites and their effects on fracture toughness10.1016/j.mtla.2019.100238 ↗
64. Microstructures and impact toughness behavior of Al 5083 alloy processed by cryorolling and afterwards annealing10.1007/s12613-013-0794-4 ↗
65. A novel method of tracing the inception and progress of fatigue crack-growth in steel10.4067/S0718-50732015000200005 ↗
66. Activation of a hybrid twinning mechanism in a Cr-Ni-Si-V-N medium manganese austenitic steel containing precipitates10.1016/j.scriptamat.2020.10.011 ↗
67. Roles of reinforcements in twin nucleation and nano-α precipitation in the hybrid TiB/TiC-reinforced titanium matrix composites during high-temperature fatigue10.1016/j.scriptamat.2021.113758 ↗
68. Strengthening triggered by deformation twins in a hot-rolled High-Mn steel: the role of stacking fault energy
69. Enhancing strength–ductility synergy in high-Mn steel by tuning stacking fault energy via precipitation10.1016/j.jmst.2023.11.032 ↗
70. Loss of ductility caused by AlN precipitation in Hadfield steel10.1007/s11661-011-0968-5 ↗
71. In-situ TEM observation of -axis extension twin formation at grain boundaries10.1016/j.scriptamat.2025.116575 ↗
72. Exploring the formation mechanism of deformation twins in CrMnFeCoNi high entropy alloy10.1007/s40195-021-01362-7 ↗
73. Direct observation of the twinning mechanism in an austenitic fe–mn–c steel10.1016/j.scriptamat.2009.03.045 ↗
74. Energy pathways and directionality in deformation twinning10.1063/1.2800806 ↗
75. Twinning-induced high impact toughness of titanium alloy at cryogenic temperature10.1016/j.msea.2022.144258 ↗
76. Dieter · 1988 · 158
77. Hierarchical twinning governed by defective twin boundary in metallic materials10.1126/sciadv.abn8299 ↗
78. Deformation and annealing behaviour of a low carbon high Mn TWIP steel microalloyed with Ti10.1080/14786435.2019.1628371 ↗
79. Hadfield manganese austenitic steel: a review of manufacturing processes and properties10.1088/2053-1591/ab3ee3 ↗
80. The effect of work hardening on the structure and hardness of hadfield steel10.24425/afe.2024.149246 ↗
81. Quantitative evaluation of deformation mechanisms in austenitic hadfield steel under different strain rates
82. In-situ investigation of dislocation tangle–untangle processes in small-sized body-centered cubic Nb single crystals10.1016/j.matlet.2017.03.165 ↗
83. Delving into the intrinsic co-relation between microstructure and mechanical behaviour of fine-/ultrafine-grained TWIP steels via TEM and in-situ EBSD observation10.1016/j.matchar.2024.113780 ↗
84. Superior mechanical properties and strengthening–toughening mechanisms of gradient-structured materials10.1016/j.msea.2022.144365 ↗
85. Strain hardening and stored energy in high-Mn austenitic based low-density steel10.1016/j.msea.2022.144331 ↗
86. Deformation microstructures as well as strengthening and toughening mechanisms of low-density high Mn steels for cryogenic applications10.1016/j.jmrt.2021.05.018 ↗
87. In situ TiC/FeCrNiCu high-entropy alloy matrix composites: reaction mechanism, microstructure and mechanical properties
88. TiNiFeCrCoAl high-entropy alloys as novel metallic binders for TiB2-TiC based composites10.1016/j.msea.2018.08.058 ↗
89. In-situ TiC particles strengthen and ductilize Fe1.2MnNi0.8Cr high entropy alloy10.1016/j.intermet.2021.107398 ↗
90. Grain refinement and strengthening of 316L stainless steel through addition of TiC nanoparticles and selective laser melting10.1016/j.msea.2021.142460 ↗
91. Influence of length-scales on spatial distribution and interfacial characteristics of B4C in a nanostructured Al matrix10.1016/j.actamat.2015.01.062 ↗
92. Effect of particles in promoting twin nucleation in a Mg–5 wt.% Zn alloy10.1016/j.scriptamat.2010.06.026 ↗
93. Deformation mechanisms in austenitic TRIP/TWIP steel as a function of temperature10.1007/s11661-014-2684-4 ↗
94. Twinning and strain-induced f.c.c. → h.c.p. transformation on the mechanical properties of Co Ni Cr Mo alloys10.1016/0025-5416(76)90234-2 ↗
95. Effects of deformation induced phase transformation and twinning on the mechanical properties of austenitic fe–mn–al alloys10.2355/isijinternational.29.868 ↗
96. CEMS study of strain induced phase transformation in manganese Hadfield steel10.1007/BF02395877 ↗
97. Friction-induced martensitic transformation in austenitic manganese steels10.1016/0043-1648(86)90134-1 ↗
98. α′-Martensite formation in deep-drawn Mn-based TWIP steel10.1007/s10853-012-6345-y ↗
99. Atomic-scale understanding of twin intersection rotation and ε-martensite transformation in a high Mn twinning-induced plasticity steel10.1016/j.actamat.2024.119832 ↗
100. Effects of chemical segregation on ductility-anisotropy in high strength Fe-Mn-Al-C lightweight austenitic steels10.1016/j.actamat.2022.118589 ↗