journal article·2026-05

Overcoming abnormal grain growth in friction stir deposited Al-Zn-Mg-Cu alloys via Mn addition for superior strength

Ji-Ang Du, Chengchao Du, Yajing Cui, Jili Wu, Ting Huang, Xudong Ren

Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Advanced Welding Techniques Analysis · Microstructure and mechanical properties · Magnesium Alloys: Properties and Applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (53)

Show source-provided references
1. Microstructural and mechanical properties of precipitation-strengthened Al-Mg-Zr-Sc-Er-Y-Si alloys10.1016/j.actamat.2023.119167 ↗
2. Precipitation strengthening at ambient and elevated temperatures of heat-treatable Al(Sc) alloys10.1016/S1359-6454(02)00201-X ↗
3. Crystallographic orientation-dependent strain hardening in a precipitation-strengthened Al-Cu alloy10.1016/j.actamat.2020.116577 ↗
4. An atomic scale structural investigation of nanometre-sized η precipitates in the 7050 aluminium alloy10.1016/j.actamat.2019.05.041 ↗
5. Alternating Cu segregation and its stabilization mechanism for coherent η ’ precipitates in Al–Zn–Mg–Cu alloys
6. Atomistic mechanism of η’-to-η transformation in Al-Zn-Mg-Cu alloys10.1016/j.scriptamat.2023.115474 ↗
7. Evaluation of strain fields caused by the η′ phase in an Al-Zn-Mg-Cu alloy10.1016/j.msea.2016.10.065 ↗
8. In situ investigation into temperature evolution and heat generation during additive friction stir deposition: a comparative study of Cu and Al-Mg-Si
9. Enhanced thermal stability in additive friction stir deposited ODS IN9052 Al alloy10.1016/j.actamat.2024.120284 ↗
10. A comprehensive review of solid-phase additive techniques: insights into friction stir additive manufacturing (FSAM) and additive friction stir deposition (AFSD)
11. Microstructure and mechanical properties of AFSD-formed 6061–7075 dissimilar aluminum alloys
12. Effect of different cooling conditions on microstructure and mechanical properties of Al-Zn-Mg-Cu alloys repaired by additive friction stir deposition10.1016/j.matchar.2024.114636 ↗
13. New method for fabricating 6061-7075-composite with enhanced microstructure, mechanical properties, and electrochemical resistance using additive friction stir deposition and heat treatment10.1016/j.msea.2025.148326 ↗
14. Characterization of the fatigue behavior of additive friction stir-deposition AA221910.1016/j.ijfatigue.2020.105951 ↗
15. Additive friction stir deposition of al 7075 parts and the effect of heat treatment on microstructure, electroconductivity, and mechanical properties10.1007/s00170-024-14582-9 ↗
16. Influence of repetitious non-isothermal aging on microstructure and strength of Al-Zn-Mg-Cu alloy10.1016/j.jallcom.2016.08.017 ↗
17. Study on microstructure and corrosion behavior of T-joints of 2A12 and 2A97 aluminum alloys by FSW
18. Friction stir welding of high-strength aerospace aluminum alloy and application in rocket tank manufacturing10.1016/j.jmst.2017.11.041 ↗
19. Investigating the microstructure and mechanical properties of Al-TiB2 composite fabricated by friction stir processing (FSP)10.1016/j.msea.2016.07.086 ↗
20. Microstructure and strengthening mechanism of TIG welded joint of AZ31 alloy based on FSP technique10.1016/j.jmapro.2024.06.045 ↗
21. A critical review on process metrics–microstructural evolution–process performance correlation in additive friction stir deposition (AFS-D)10.1007/s40430-022-03729-y ↗
22. In-situ aluminum 7075 metal matrix composites development for additive friction stir deposition10.1016/j.jmrt.2025.05.258 ↗
23. Achieving uniform microstructure and excellent mechanical properties in TiB2/7055 composite via additive friction stir deposition and heat treatment
24. Microstructure and mechanical properties of Al–Li alloy manufactured by additive friction stir deposition10.1016/j.msea.2023.145753 ↗
25. Microstructure, texture and mechanical properties during refill friction stir spot welding of 6061-T6 alloy10.1016/j.matchar.2017.03.023 ↗
26. Correlation between microstructure and mechanical properties of 6061-T6 double-side FSW joint10.1016/j.jmapro.2019.01.010 ↗
27. Microstructure of spray formed Al-Zn-Mg-Cu alloy with Mn addition10.1016/S1003-6326(11)60671-7 ↗
28. The effect of minor addition of Mn in AA7075 Al–Zn–Mg–Cu aluminum alloys on microstructural evolution and mechanical properties in warm forming and paint baking processes
29. Influence of Mn and Zn addition on the formation of dispersoids and mechanical properties of Al-Mg-Sc-Zr alloys10.1016/j.msea.2025.147969 ↗
30. Investigation on in-situ tensile behaviors of 6061 aluminum alloy fabricated by wire additive friction stir deposition10.1016/j.jallcom.2024.176780 ↗
31. The effect of heat treatment on the microstructure and mechanical properties of multilayer AA6061 alloy fabricated by additive friction stir deposition
32. Microstructure and mechanical properties of SiCp/6061 aluminum matrix composites fabricated by additive friction stir deposition10.1016/j.jallcom.2025.182040 ↗
33. Additive friction stir deposition of an Al-Cu-Mg alloy: microstructure evolution and mechanical properties10.1016/j.matchar.2024.114562 ↗
34. Effect of rotation speed on the microstructure and mechanical properties of AFSD 7075 aluminum alloy10.1016/j.msea.2025.148448 ↗
35. The microstructure and corrosion behavior analysis of different aging Al-Zn-Mg-Cu alloys manufactured by additive friction stir deposition10.1016/j.matchar.2025.115187 ↗
36. Influence of aging time to achieve tensile build direction heat treated T74 forging properties in lubricant free AFSD AA7050
37. Microstructure evolution and mechanical properties of high-strength aluminum alloy prepared by additive friction stir deposition10.1016/j.jmrt.2025.03.178 ↗
38. Investigating multi-scale heterogeneity in multi-layer additive friction stir deposition of high-strength aluminum alloys10.1016/j.msea.2025.147979 ↗
39. Aging-driven optimization of precipitate phases: enhancing mechanical strength and corrosion resistance in 7075 aluminum alloy10.1016/j.jallcom.2025.182093 ↗
40. Research on the effect of solution treatment on mechanical properties, electrical conductivity and microstructure of cold-rolled 7075 aluminum alloy10.1016/j.matlet.2025.138532 ↗
41. Effect of cryorolling and ageing on the microstructure and mechanical properties of Al 7085 alloy10.1016/j.msea.2021.142482 ↗
42. Effect of ageing temperature on microstructure, mechanical property and corrosion behavior of aluminum alloy 708510.1016/j.jallcom.2020.153792 ↗
43. Zhou · 2024
44. Effect of various non-isothermal aging on properties and microstructure of 7055 aluminum alloy10.1016/j.jmrt.2023.07.068 ↗
45. Precipitation behaviour of Al–Zn–Mg–Cu alloy and diffraction analysis from η′ precipitates in four variants10.1016/j.jallcom.2014.05.061 ↗
46. Revisiting the evolution of strength and microstructure of aluminum alloy 7055 during continuous retrogression and re-ageing treatment
47. Stabilization of metastable η’ phase in Al-Zn-Mg-Cu-Ti alloy fabricated by laser direction energy deposition10.1016/j.matchar.2025.115368 ↗
48. Revisiting the precipitation mechanisms of guinier-preston zones, η′, and η precipitates in Al-Zn-Mg alloys10.1016/j.actamat.2024.119789 ↗
49. Co-precipitation of T′ and η′ phase in Al-Zn-Mg-Cu alloys10.1016/j.matchar.2020.110610 ↗
50. GP-zones in Al–Zn–Mg alloys and their role in artificial aging10.1016/S1359-6454(01)00251-8 ↗
51. The direct observation of copper segregation at the broad faces of η′ and η precipitates in AA7010 aluminium alloy10.1016/j.matchar.2020.110232 ↗
52. Deformation behavior, paint-bake response and microstructure evolution of pre-hardened 7075 aluminum alloy10.1016/j.msea.2025.148967 ↗
53. Effect of heat treatment on microstructure, mechanical properties and corrosion resistance of 7075 aluminum alloys fabricated by improved friction stir additive manufacturing10.1016/j.jallcom.2024.176512 ↗