Manipulating intergranular secondary phases via Y alloying to achieve crack-free additive manufacturing of high-strength aluminum alloys

Tao Liu, Zuming Liu, Li Zhang, Jiangbin Luo, Shupeng Ye, Daoyan Jiang, Runxing Zhou, Peicheng Mo, Tianxing Huang

Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Aluminum Alloy Microstructure Properties · Solidification and crystal growth phenomena

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (64)

Show source-provided references
1. 3D printing of aluminium alloys: additive manufacturing of aluminium alloys using selective laser melting10.1016/j.pmatsci.2019.100578 ↗
2. Achieving ultrahigh fatigue resistance in AlSi10Mg alloy by additive manufacturing10.1038/s41563-023-01651-9 ↗
3. Alloy design for laser powder bed fusion additive manufacturing: a critical review10.1088/2631-7990/ad1657 ↗
4. Control of grain structure, phases, and defects in additive manufacturing of high-performance metallic components10.1016/j.pmatsci.2023.101153 ↗
5. An improved process scan strategy to obtain high-performance fatigue properties for scalmalloy®10.1016/j.matdes.2022.111410 ↗
6. 3D printing of high-strength aluminium alloys10.1038/nature23894 ↗
7. Exploiting the rapid solidification potential of laser powder bed fusion in high strength and crack-free Al-Cu-Mg-Mn-Zr alloys
8. Inoculation treatment of an additively manufactured 2024 aluminium alloy with titanium nanoparticles10.1016/j.actamat.2020.06.026 ↗
9. Cracking mechanism and its susceptibility to scanning speed during laser power bed fusion processed high-strength 2024Al alloy10.1016/j.matchar.2022.112344 ↗
10. Design strategy for eliminating cracking and improving mechanical properties of Al-Mg-Si alloys fabricated by laser melting deposition
11. Processing and characterization of crack-free aluminum 6061 using high-temperature heating in laser powder bed fusion additive manufacturing
12. Improving the processability and grain structures of additively manufactured Al-Fe-Cu-xZr alloy: experiment and high-fidelity simulation
13. A novel crack-free Ti-modified Al-Cu-Mg alloy designed for selective laser melting
14. Microstructure, mechanical properties and multiphase synergistic strengthening mechanisms of LPBF fabricated AlZnMgZr alloy with high Zn content
15. From crack-prone to crack-free: eliminating cracks in additive manufacturing of high-strength Mg2Si-modified Al-Mg-Si alloys10.1016/j.jmst.2024.04.009 ↗
16. On the Si-induced microstructure evolution, solidification cracking healing and strengthening behavior of laser powder bed fusion additive manufactured Al-Cu-Mg/Si alloys10.1016/j.jmatprotec.2023.117860 ↗
17. Composition-dependent solidification cracking of aluminum-silicon alloys during laser powder bed fusion10.1016/j.actamat.2021.116698 ↗
18. A high strength Al–Li alloy produced by laser powder bed fusion: densification, microstructure, and mechanical properties
19. Recent advances in inoculation treatment for powder-based additive manufacturing of aluminium alloys10.1016/j.mser.2024.100773 ↗
20. Achieving excellent strength of the LPBF additively manufactured Al–Cu–Mg composite via in-situ mixing TiB2 and solution treatment10.1016/j.msea.2022.143531 ↗
21. Dependence of mechanical properties and microstructure on solidification onset temperature for Al2024–CaB6 alloys processed using laser powder bed fusion10.1016/j.msea.2021.142552 ↗
22. Crack initiation mechanism of laser powder bed fusion additive manufactured Al-Zn-Mg-Cu alloy10.1016/j.matchar.2022.112415 ↗
23. New alloy design approach to inhibiting hot cracking in laser additive manufactured nickel-based superalloys10.1016/j.actamat.2023.118736 ↗
24. Unraveling the low thermal conductivity of the LPBF fabricated pure Al, AlSi12, and AlSi10Mg alloys through substrate preheating
25. High-temperature strength sustained by nano-sized eutectic structure of Al–Fe alloy manufactured by laser powder bed fusion10.1016/j.msea.2022.142782 ↗
26. High strength aluminum-cerium alloy processed by laser powder bed fusion
27. A novel high-strength Al-La-Mg-Mn alloy for selective laser melting10.1016/j.jmst.2022.07.046 ↗
28. A high-strength heat-resistant Al−5.7Ni eutectic alloy with spherical Al3Ni nano-particles by selective laser melting10.1016/j.scriptamat.2021.114034 ↗
29. Microstructure characterization and mechanical properties of crack-free Al-Cu-Mg-Y alloy fabricated by laser powder bed fusion
30. Intergranular solidification defects in high-strength 2A14 aluminum alloy fabricated by laser additive manufacturing: role of secondary phases10.1007/s10853-025-12011-0 ↗
31. Eliminating intergranular solidification defects to achieve excellent additive manufacturing processability of aluminium alloy via Y alloying10.1016/j.msea.2024.147638 ↗
32. Cracking behaviour of high-strength AA2024 aluminium alloy produced by laser powder bed fusion
33. Crack-free high-strength AA-7075 fabricated by laser powder bed fusion with inoculations of metallic glass powders
34. Texture coefficient and band gap tailoring of Fe-doped SnO2 nanoparticles via thermal spray pyrolysis10.1007/s12598-019-01278-3 ↗
35. Evidence of carbide-assisted in situ-directional recrystallization of GH4099 superalloy fabricated by laser powder bed fusion10.1016/j.jmst.2024.07.019 ↗
36. An inter-layer remelting strategy to tailor microstructure and mechanical properties of 2219 Al-Cu alloy during wire arc additive manufacturing process and post-T6 heat treatment
37. Heat treatment for metal additive manufacturing10.1016/j.pmatsci.2022.101051 ↗
38. Physics and phenomenology of strain hardening: the FCC case10.1016/S0079-6425(02)00003-8 ↗
39. Editorial board · 2002 · 84
40. A novel approach for tailoring aluminum alloys for additive manufacturing10.1016/j.msea.2025.148179 ↗
41. Laser powder bed fusion of Zr-modified Al–Cu–Mg alloy: Crack-Inhibiting, grain refinement, and mechanical properties10.1016/j.msea.2022.142618 ↗
42. Effect of Zirconium addition on crack, microstructure and mechanical behavior of selective laser melted Al-Cu-Mg alloy10.1016/j.scriptamat.2017.02.036 ↗
43. Er-microalloying mediated hot-crack healing and grain boundary segregation engineering in Al-Cu-Mg-Zr alloy via laser powder bed fusion10.1016/j.msea.2025.148966 ↗
44. A crack-free and high-strength Al-Cu-Mg-Mn-Zr alloy fabricated by laser powder bed fusion10.1016/j.msea.2022.143731 ↗
45. Improving impact toughness of aluminum alloy through scanning strategy during laser powder bed fusion10.1016/j.msea.2025.148244 ↗
46. Deformation faulting in ultrafine-grained aluminum alloys: nucleation mechanisms and critical assessment of strengthening-ductilization contributions10.1016/j.actamat.2025.120750 ↗
47. Thermodynamic description of the Al–Cu–Y ternary system10.1016/j.calphad.2011.09.008 ↗
48. Achieving superior strength-ductility balance in novel heterogeneous lamella structures of Al-Zn-Mg-Cu alloys10.1016/j.jmst.2023.08.074 ↗
49. Effect of combined addition of Zr, Ti and Y on microstructure and tensile properties of an Al-Zn-Mg-Cu alloy10.1016/j.matdes.2022.111129 ↗
50. The Contribution of constitutional supercooling to nucleation and grain formation10.1007/s11661-015-2960-y ↗
51. Grain refinement of aluminium studied by use of a thermal analytical technique10.1016/0040-6031(94)02167-M ↗
52. Effect of Y on the hot tearing susceptibility of 3Y2O3/Al5Cu composite10.1016/j.jallcom.2020.156152 ↗
53. Grain morphologies in additively manufactured alloys: from solidification fundamentals to advanced microstructure control10.1016/j.jmst.2025.02.033 ↗
54. Experimental description of the Al-Cu binary phase diagram10.1007/s11661-019-05286-x ↗
55. An analysis of the relationship between grain size, solute content, and the potency and number density of nucleant particles10.1007/s11661-005-0054-y ↗
56. Superior mechanical properties of a selective-laser-melted AlZnMgCuScZr alloy enabled by a tunable hierarchical microstructure and dual-nanoprecipitation10.1016/j.mattod.2021.11.019 ↗
57. Developing a high-strength Al-Mg-Si-Sc-Zr alloy for selective laser melting: Crack-Inhibiting and multiple strengthening mechanisms10.1016/j.actamat.2020.03.060 ↗
58. Selective laser melting of a high strength Al-Mn-Sc alloy: alloy design and strengthening mechanisms10.1016/j.actamat.2019.04.014 ↗
59. High strength Al-Cu-Mg based alloy with synchronous improved tensile properties and hot-cracking resistance suitable for laser powder bed fusion10.1016/j.jmst.2022.09.027 ↗
60. Effect of heat treatment patterns on porosity, microstructure, and mechanical properties of selective laser melted TiB2/Al–Si–Mg composite10.1016/j.msea.2022.143932 ↗
61. Synergy of strength-ductility in a novel Al-Zn-Mg-Cu-Zr-Sc-Hf alloy through optimizing hierarchical microstructures10.1016/j.jmst.2024.05.071 ↗
62. A precipitation-hardened high-entropy alloy with outstanding tensile properties10.1016/j.actamat.2015.08.076 ↗
63. AlMgScZr alloys for laser powder bed fusion additive manufacturing. A review10.1016/j.matdes.2025.114080 ↗
64. Enhanced plastic stability: achieving high performance in a Al6xxx alloy fabricated by additive manufacturing10.1002/adma.202307825 ↗