Processability and interfacial characteristics in PBF-LB/M-processed nano-B4C/AlSi10Mg composites with superior high-temperature mechanical performance
Source abstract
Abstract
Incorporating nano-scaled ceramic particles into additively manufactured Al-alloys is a validated strategy to simultaneously enhance the elevated-temperature mechanical properties and laser powder bed fusion (PBF-LB/M) processability. While B 4 C exhibits outstanding thermal stability and interfacial compatibility with Al, the integration of nano-B 4 C into Al alloys through PBF-LB/M remains insufficiently investigated. In particular, the underlying mechanisms governing laser-particle interaction, processability, and the consequent microstructural formation have not been comprehensively explored. This study aims to address this gap by investigating the effect of nano-B 4 C additions (1, 3, and 5 wt.%) to AlSi10Mg on PBF-LB/M processability and the alloy behavior. The results demonstrated excellent PBF-LB/M processability of the B 4 C/AlSi10Mg composites at all weight fractions of B 4 C. The as-built B 4 C/AlSi10Mg revealed a remarkable columnar-to-equiaxed transition, featuring an ultrafine grain structure (as small as 1.23 μm) with almost random crystallographic texture. This grain refinement was attributed to a reactive nucleation process, where the interfacial reaction between B 4 C and the matrix results in the coherent AlB 2 core-shell structured phase. Furthermore, this interfacial reaction induced a novel morphological transition, characterized by the spheroidization of irregularly shaped nanoparticles as a consequence of partial reactive melting. The B 4 C nanocomposites exhibited superior elevated-temperature mechanical properties, increasing tensile strength by up to 60% compared to their AlSi10Mg counterparts. This study provides fundamental insights into the design and PBF-LB/M processing of Al-based metal-matrix nanocomposites (AMMNCs) for high-temperature applications. • Nano-B 4 C/AlSi10Mg shows superior PBF-LB/M processability, including 5 wt.% B 4 C conditions. • Reactive nucleation stimulates a full columnar-to-equiaxed grain transition. • Irregularly shaped nano-B 4 C undergoes spheroidization induced by partial reactive melting. • Melt pool evolution is altered by several counteracting heat transfer mechanisms. • Tensile strength at 300 °C increases by 60% over AlSi10Mg while maintaining 11% total elongation.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Aluminum Alloys Composites Properties · High Entropy Alloys Studies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (87)
Show source-provided references
1. Manufacture of nano-sized particle-reinforced metal matrix composites: a review10.1007/s40195-014-0154-z ↗
2. Innovation in metal casting processes: a review of metal matrix nanocomposites in metal and bimetal castings10.3390/cryst15020191 ↗
3. Effect of clustering on particle pushing and solidification behaviour in TiB2 reinforced aluminium PMMCs10.1016/j.compositesa.2004.10.027 ↗
4. A new model for the solidification of metal matrix nanocomposites: wet cluster engulfment of nanoparticles by the solidification front10.1177/0021998317701557 ↗
5. Machining behavior investigation of aluminium metal matrix composite reinforced with TiC particulates10.1007/s12008-023-01378-6 ↗
6. Additive manufacturing of oxide-dispersion strengthened alloys: materials, synthesis and manufacturing10.1016/j.pmatsci.2022.101049 ↗
7. Selective laser melting of TiB2/AlSi10Mg composite: processability, microstructure and fracture behavior10.1016/j.jmatprotec.2021.117386 ↗
8. Synthesis of nanostructured Fe–TiB2 composites with excellent mechanical properties via laser powder bed fusion10.1016/j.jmrt.2025.02.193 ↗
9. Laser powder bed fusion of nano-CaB6 decorated 2024 aluminum alloy10.1016/j.jallcom.2021.158714 ↗
10. Laser powder bed fusion of crack-free TiN/Al7075 composites with enhanced mechanical properties10.1016/j.matlet.2020.128625 ↗
11. A novel crack-free and refined 2195-Ti/CeB6 composites prepared by laser powder bed fusion10.1016/j.matlet.2022.133572 ↗
12. Nanocomposite powder for powder-bed-based additive manufacturing obtained by dry particle coating10.1016/j.powtec.2022.117474 ↗
13. Simultaneous enhancement of strength, ductility, and hardness of TiN/AlSi10Mg nanocomposites via selective laser melting
14. Recent progress of aluminum alloys and aluminum matrix composites produced via laser powder bed fusion: a review10.1007/s10853-024-09368-z ↗
15. Recent progress on the additive manufacturing of aluminum alloys and aluminum matrix composites: microstructure, properties, and applications10.1016/j.ijmachtools.2023.104047 ↗
16. Laser powder-bed fusion of ceramic particulate reinforced aluminum alloys
17. Processing and mechanical properties of B4C reinforced Al matrix composites10.1016/j.jallcom.2009.04.065 ↗
18. Wettability of 2519Al on B4C at 1000–1250°C and mechanical properties of infiltrated B4C–2519Al composites10.1016/j.ceramint.2013.07.120 ↗
19. Wettability of low weight borides by commercial aluminum alloys − A basis for metal matrix composite fabrication10.1002/adem.201600297 ↗
20. Boron carbide reinforced aluminium matrix composite: physical, mechanical characterization and mathematical modelling10.1016/j.msea.2016.01.114 ↗
21. Preparation of B4Cp/Al composites via selective laser melting and their tribological properties10.3390/ma15238340 ↗
22. Microstructure and dynamic microhardness of additively manufactured (TiB2+TiC)/AlSi10Mg composites with AlSi10Mg and B4C coated Ti powder10.1016/j.jallcom.2023.168718 ↗
23. In-situ chemical reaction mechanism and non-equilibrium microstructural evolution of (TiB2 + TiC)/AlSi10Mg composites prepared by SLM-CS processing10.1016/j.jallcom.2020.157553 ↗
24. Role of B4C in the directed energy deposition of aluminum alloy 6061/B4C composite using core-shell powder for crack annihilation, pore mitigation, and grain refinement
25. Thermally stable microstructures and mechanical properties of B4C-Al composite with in-situ formed Mg(Al)B210.1016/j.jmst.2019.04.019 ↗
26. Towards high-temperature applications of aluminium alloys enabled by additive manufacturing10.1080/09506608.2021.1951580 ↗
27. Microstructure, tensile properties and thermal stability of AlMgSiScZr alloy printed by laser powder bed fusion10.1016/j.jmst.2020.08.033 ↗
28. Temporal evolution of the nanostructure of Al(Sc,Zr) alloys: part I – chemical compositions of Al(ScZr) precipitates10.1016/j.actamat.2005.08.016 ↗
29. Microstructure and properties of a high temperature al–ce–mn alloy produced by additive manufacturing10.1016/j.actamat.2020.07.014 ↗
30. An Al-5Fe-6Cr alloy with outstanding high temperature mechanical behavior by laser powder bed fusion
31. High-temperature tensile behaviors of an ultra-strong aluminum alloy fabricated by additive manufacturing
32. High-temperature tensile properties of an aluminum quasicrystal-forming alloy manufactured by laser powder bed fusion10.1016/j.msea.2023.145670 ↗
33. Laser powder bed fusion of an ultrafine microstructural in-situ TiB2/Al composite with excellent mechanical properties and thermal stability at elevated temperatures10.1016/j.msea.2023.145969 ↗
34. Elevated temperature mechanical properties of TiCN reinforced AlSi10Mg fabricated by laser powder bed fusion additive manufacturing10.1016/j.msea.2021.141025 ↗
35. Laser powder bed fusion of nano-titania modified 2219 aluminium alloy with superior mechanical properties at both room and elevated temperatures: the significant impact of solute
36. Role of TiC on the microstructure, tensile property and thermal stability of laser powder bed fusion fabricated AlSi10Mg alloy10.1016/j.msea.2024.147182 ↗
37. Additive manufacturing of metal matrix nanocomposites: novel approach for nanoparticles dispersion by electromagnetic three-dimensional vibration10.1016/j.matlet.2023.134399 ↗
38. The dispersion-strengthening effect of TiN evoked by in situ nitridation of NiCu-based alloy 400 during gas atomization for laser powder bed fusion10.1016/j.msea.2024.146129 ↗
39. A profile refinement method for nuclear and magnetic structures10.1107/S0021889869006558 ↗
40. Microstructural investigation and mechanical behavior of a two-material component fabricated through selective laser melting of AlSi10Mg on an al-cu-ni-fe-mg cast alloy substrate
41. Microstructure, precipitates and hardness of selectively laser melted AlSi10Mg alloy before and after heat treatment10.1016/j.matchar.2018.04.022 ↗
42. Three-dimensional analysis of grain structure and texture of additively manufactured 316L austenitic stainless steel
43. Some statistics associated with the random disorientation of cubes10.1093/biomet/44.1-2.205 ↗
44. Laser powder bed fusion of TiB2-modified Cu15Ni8Sn alloy: processability, microstructure and mechanical performance10.1016/j.msea.2022.143879 ↗
45. Absorbance study of powder conditions for laser additive manufacturing10.1016/j.matdes.2022.110591 ↗
46. Numerical modeling of the heating phase of the selective laser sintering process10.1016/j.ijthermalsci.2017.05.017 ↗
47. Laser absorption behavior of randomly packed powder-bed during selective laser melting of SiC and TiB2 reinforced Al matrix composites10.1016/j.optlastec.2019.105600 ↗
48. Effect of process parameters on melt pool geometry in laser powder bed fusion of metals: a numerical investigation10.1016/j.procir.2022.09.187 ↗
49. Mechanical and optical properties of thin film titanium nitride (TiN) resulting from deposition DC sputtering10.14421/icse.v2.47 ↗
50. Boron carbide: structure, properties, and stability under stress10.1111/j.1551-2916.2011.04865.x ↗
51. Influence of thermal properties on residual stresses in SLM of aerospace alloys10.1108/RPJ-03-2019-0065 ↗
52. Recent research on the optimization of interfacial structure and interfacial interaction mechanisms of metal matrix composites: a review10.1002/adem.202401392 ↗
53. Orientation independent heat transport characteristics of diamond/copper interface with ion beam bombardment10.1016/j.actamat.2021.117283 ↗
54. Role of electron–phonon coupling in thermal conductance of metal–nonmetal interfaces10.1063/1.1758301 ↗
55. Effects of graphene nano particles on interfacial microstructure and mechanical properties of Al7150/B4C hybrid nanocomposite fabricated by novel double ultrasonic two stage stir casting technique10.1016/j.jallcom.2024.176686 ↗
56. Microstructures and mechanical properties of Al nanocomposites hybrid-reinforced with B4C, carbon nanotubes and graphene nanoplatelets10.1016/j.mseb.2023.116457 ↗
57. Influence of B4C particle size on the microstructure and mechanical properties of B4C/Al composites fabricated by pressureless infiltration10.3390/met13081358 ↗
58. Rapid preparation of B4Cp/Al composites with homogeneous interface via ultrasound assisted casting method10.1016/j.jallcom.2020.157659 ↗
59. On the effects of particle size and preform porosity on the mechanical properties of reaction-bonded boron carbide infiltrated with Al-Si alloy at 950 °C10.1016/j.ceramint.2020.04.227 ↗
60. Interfacial reaction mechanism between matrix and reinforcement in B4C/6061Al composites10.1016/j.matchemphys.2015.01.052 ↗
61. Microstructure evolution of B4C/Al interface: a first-principle Study10.1007/s11665-021-06079-3 ↗
62. On the selective laser melting based additive manufacturing of AlSi10Mg: the process parameter investigation through multiphysics simulation and experimental validation10.1016/j.jallcom.2021.161873 ↗
63. J. Zeman, A. Herman, J. Šerák, The boron solubility in Al-Mg-B alloys, Arch. Foundry Eng. https://doi.org/10.24425/afe.2024.151305.10.24425/afe.2024.151305 ↗
64. Synthesis and characterization of mechanically alloyed Al/AlxMg1-xB2 composites10.1515/SECM.2009.16.4.267 ↗
65. A novel method to 3D-print fine-grained AlSi10Mg alloy with isotropic properties via inoculation with LaB6 nanoparticles
66. Towards understanding grain nucleation under Additive Manufacturing solidification conditions10.1016/j.actamat.2020.05.012 ↗
67. Nucleation catalysis10.1021/ie50510a031 ↗
68. The effect of carbide and nitride additions on the heterogeneous nucleation behavior of liquid iron10.1007/BF03037838 ↗
69. Influence of LaB6 inoculant on the thermodynamics within the molten pool and subsequent microstructure development and cracking behavior of laser powder bed fused TiAl-based alloys10.1016/j.jmrt.2023.10.062 ↗
70. Steady state columnar and equiaxed growth of dendrites and eutectic10.1016/0025-5416(84)90201-5 ↗
71. Additive manufacturing of metallic components – process, structure and properties10.1016/j.pmatsci.2017.10.001 ↗
72. Selective laser melting of in-situ Al4SiC4 + SiC hybrid reinforced Al matrix composites: influence of starting SiC particle size10.1016/j.surfcoat.2015.04.029 ↗
73. Particulate migration behavior and its mechanism during selective laser melting of TiC reinforced Al matrix nanocomposites10.1016/j.matdes.2015.05.041 ↗
74. Simultaneous enhancement of elevated temperature strength and ductility in additive-manufactured nickel-based superalloy via doping Y2O3 nanoparticles10.1016/j.jmst.2024.04.085 ↗
75. Microstructure evolution and properties of nanoparticulate SiC modified AlSi10Mg alloys10.1016/j.msea.2021.140864 ↗
76. Enhancement of grain refinement and heat resistance in TiB2-reinforced al-cu-mg-fe-ni matrix composite additive manufactured by electron beam melting10.1016/j.jallcom.2022.166395 ↗
77. An analytical model for the interaction between an insoluble particle and an advancing solid/liquid interface10.1007/BF02801184 ↗
78. Mechanical performance of particulate-reinforced Al metal-matrix composites (MMCs) and Al metal-matrix nano-composites (MMNCs)10.1007/s10853-017-1378-x ↗
79. Microstructure and mechanical properties of nanostructured Al-4Cu alloy produced by mechanical alloying and vacuum hot pressing10.1007/s11661-009-0005-0 ↗
80. The tensile response and fracture behavior of 2009 aluminum alloy metal matrix composite10.1016/S0921-5093(02)00481-1 ↗
81. Microstructure evolution and mechanical properties at high temperature of selective laser melted AlSi10Mg10.1016/j.jmst.2020.04.066 ↗
82. Elevated temperature ductility dip in an additively manufactured al-cu-ce alloy10.1016/j.actamat.2021.117285 ↗
83. The effect of deformation on grain growth in Zener pinned systems10.1016/S1359-6454(01)00033-7 ↗
84. Effect of Cu content on the mechanical properties of an al–cu–mg–ag alloy10.1016/S0925-8388(02)00076-2 ↗
85. Microstructural development and aging behavior of al–cr–zr heat-resistant alloy fabricated using laser powder bed fusion10.1016/j.jmrt.2021.10.027 ↗
86. Microstructures and mechanical properties of aluminum-transition metal binary alloys (Al-Fe, Al-Mn, and Al-Cr) processed by laser powder bed fusion10.1016/j.jallcom.2021.159680 ↗
87. Additively manufactured scalmalloy via laser powder bed fusion (L‐PBF): temperature-dependent tensile and fatigue behaviors10.1111/ffe.14549 ↗