Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Aluminum Alloy Microstructure Properties · Solidification and crystal growth phenomena · Microstructure and mechanical properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (65)

Show source-provided references
1. Simulation of grain refinement of Al-8Si-0.2 Mg alloy inoculated with Al-Nb-B via an improved cellular automaton model10.1016/j.matdes.2024.113561 ↗
2. Alloy development and process innovations for light metals casting10.1016/j.jmatprotec.2022.117606 ↗
3. Unified casting (UniCast) aluminum alloy—a sustainable and low-carbon materials solution for vehicle lightweighting10.1016/j.jmst.2023.02.003 ↗
4. Ultra-large aluminum shape casting: opportunities and challenges10.1007/s41230-024-4111-9 ↗
5. A formation map of iron-containing intermetallic phases in recycled cast aluminum alloys10.1007/s11661-019-05469-6 ↗
6. A new recycled Al–Si–Mg alloy for sustainable structural die casting applications10.1007/s11661-022-06711-4 ↗
7. Design of non-heat treatable high pressure die casting Al alloys: a review10.1007/s11665-024-09477-5 ↗
8. Effects of Fe content on the 3D morphology of Fe-rich phases and mechanical properties of cast Al-Mg-Si alloy10.1016/j.jallcom.2024.174501 ↗
9. Study of the evolution mechanisms of Fe-rich phases in Al-Si-Fe alloys with Mn modification using synchrotron X-ray imaging10.1016/j.jallcom.2022.165378 ↗
10. Secondary Al-Si-Mg high-pressure die casting alloys with enhanced ductility10.1007/s11661-014-2700-8 ↗
11. The effects of Mn additions on the microstructure and mechanical properties of Al–Si–Cu casting alloys10.1016/j.msea.2007.12.026 ↗
12. Fracture behavior of intermetallic clusters in HVDC AlSiMgMn alloys: a finite element study based on actual morphologies10.1016/j.engfracmech.2025.111358 ↗
13. Intermetallic sludge formation in Fe containing secondary Al–Si alloys influenced by Cr and Mn as preparative tool for metal melt filtration10.1002/adem.201700161 ↗
14. Precipitation of α-Al(Fe,Mn)Si from the melt10.1023/A:1004815621313 ↗
15. Understanding crystal structure and morphology evolution of Fe, Mn, Cr-containing phases in Al-Si cast alloy10.1016/j.intermet.2021.107103 ↗
16. Morphology, thermal stability, electronic structure and mechanical properties of α-AlFeMnSi phases with varying Mn/Fe atomic ratios: experimental studies and DFT calculations10.1016/j.jallcom.2021.163523 ↗
17. The influence of Cr content on the microstructure and mechanical properties of AlSi9Cu3(Fe) die-casting alloys10.1016/j.msea.2010.08.079 ↗
18. Uncovering the effects of neutralizing elements (Co, Mn and Cr) on the Fe-rich intermetallic formation in Al–Si–Cu alloys10.1016/j.msea.2022.144090 ↗
19. Controlling the Fe-intermetallic phases and mechanical properties of secondary Al-9Si-1Fe alloy with Cr and Mn additions10.1016/j.jmst.2024.04.014 ↗
20. CALPHAD-guided suppression of detrimental Fe-containing phases in secondary aluminum alloys10.1016/j.calphad.2025.102830 ↗
21. Precipitation of Fe rich intermetallics in Cr- and Co-modified A413 alloy10.1179/136404605225022928 ↗
22. Influence of sludge particles on the tensile properties of die-cast secondary aluminum alloys10.1007/s11663-014-0260-3 ↗
23. Effect of cooling rate and Co content on the formation of Fe-rich intermetallics in hypoeutectic Al7Si0.3Mg alloy with 0.5%Fe10.1016/j.matchar.2018.02.029 ↗
24. Effects of cobalt and solidification cooling rate on intermetallic phases and tensile properties of a -Cu, -Zn, -Fe containing Al-Si alloy10.1007/s00170-020-05077-4 ↗
25. Evolution of Fe-rich intermetallics in Al-Si-Cu 319 cast alloy with various Fe, Mo, and Mn contents10.1007/s11663-019-01584-2 ↗
26. Investigating the influences of Fe, Mn and Mo additions on the evolution of microstructure and mechanical performances of Al–Si–Mg cast alloys10.1016/j.jmrt.2023.05.234 ↗
27. Effect of Mn and Mo on microstructure and mechanical properties of Al-Si-Cu-Mg-0.6Fe alloy10.1007/s41230-023-3084-4 ↗
28. Effect of vanadium on Fe-rich phase, mechanical properties and thermal conductivity of hypoeutectic Al–Si alloy10.1088/2053-1591/abe5f0 ↗
29. Microstructure and mechanical properties of non-heat-treated Al–8Si-0.2Mg-0.5Mn alloy inoculated by Al–Nb–B refiner10.1016/j.jmrt.2024.06.144 ↗
30. Microstructural evolution and high-temperature performance of high-pressure die-cast Al-Si-Mg alloys through Mn and Zr alloying10.1007/s11837-025-07413-z ↗
31. 365.0 (Silafont®-36) and A365.0 (Aural®-2/-3)[1]: low-iron premium die-casting alloys
32. Revealing the effect of iron content on the microstructure evolution, mechanical properties and corrosion resistance of the A356-T6 aluminum alloys10.1016/j.jmrt.2024.09.233 ↗
33. Dilatant shear bands in solidifying metals10.1038/nature05426 ↗
34. Defect band characteristics in Mg-Al and Al-Si high-pressure die castings10.1007/s11661-007-9243-1 ↗
35. Accelerating the design of highly separable Fe-containing intermetallics in Al–Si alloys via DFT calculations and experimental validation
36. β- and δ-Al-Fe-Si intermetallic phase, their intergrowth and polytype formation10.1016/j.jallcom.2018.11.396 ↗
37. The crystal structure of the ternary alloy {$\alpha$}(AlFeSi)10.1107/S0365110X67004372 ↗
38. Intermetallic phases in high purity Al-10Si-0.3Fe cast alloys with and without Sr modification studied by FIB tomography and TEM10.1016/j.intermet.2016.02.003 ↗
39. Effect of Mn and cooling rates on α-, β-and δ-Al–Fe–Si intermetallic phase formation in a secondary Al–Si alloy10.1016/j.mtla.2018.100198 ↗
40. Strontium effects on the formation of iron-intermetallic phases in secondary Al–9Si–0.6Fe alloys10.1007/s11661-023-07267-7 ↗
41. Formation of intermetallic δ phase in Al-10Si-0.3 Fe alloy investigated by in-situ 4D X-ray synchrotron tomography10.1016/j.actamat.2017.02.048 ↗
42. Effects of Sr on Fe-rich intermetallics in recycled Al–Si–Cu alloys10.1007/s10853-024-09854-4 ↗
43. Morphological evolution and growth mechanism of primary Mg2Si phase in Al-Mg2Si alloys10.1016/j.actamat.2010.10.036 ↗
44. In situ study of nucleation and growth of the irregular α-Al/β-Al5FeSi eutectic by 3-D synchrotron X-ray microtomography10.1016/j.actamat.2010.06.012 ↗
45. Effect of melt conditioning on removal of Fe from secondary Al-Si alloys containing Mg, Mn, and Cr10.1007/s11661-018-4930-7 ↗
46. On the formation of sludge intermetallic particles in secondary aluminum alloys10.1007/s11661-015-2942-0 ↗
47. Thermodynamics-guided design of sustainable secondary Al-Si alloys for enhanced Fe-impurity tolerance and optimized Mn doping10.1016/j.actamat.2025.120932 ↗
48. Formation of the Fe-containing intermetallic compounds during solidification of Al-5Mg-2Si-0.7Mn-1.1Fe alloy10.1007/s11661-018-4591-6 ↗
49. Grain refinement and morphological control of intermetallic compounds: a comprehensive review10.1016/j.cossms.2024.101200 ↗
50. Que
51. Multi-scale simulation of grain evolution during indirect squeeze casting with considering solute suppressed nucleation and externally solidified crystals
52. The characterization of Fe-rich phases in a high-pressure die cast hypoeutectic aluminum-silicon alloy10.1016/j.jmst.2020.02.040 ↗
53. The role of grain refiner in the nucleation of AlFeSi intermetallic phases during solidification of a 6xxx aluminum alloy10.1007/s11661-019-05447-y ↗
54. Feeding mechanisms in high-pressure die castings10.1007/s11661-010-0222-6 ↗
55. Understanding Fe-containing intermetallic compounds in Al alloys: an overview of recent advances from the LiME research hub10.3390/met12101677 ↗
56. Unveiling the growth mechanism of Fe-containing intermetallics in Al–Si alloy in the perspective of surface stability and atom adsorption10.1016/j.jmrt.2025.01.159 ↗
57. Damage by eutectic particle cracking in aluminum casting alloys A356/35710.1007/s11661-003-0190-1 ↗
58. Microstructural effects on the tensile and fracture behavior of Aluminum casting alloys A356/35710.1007/s11661-003-0189-7 ↗
59. Mechanical properties of intermetallic phases in multi-component Al–Si alloys using nanoindentation10.1016/j.intermet.2009.02.003 ↗
60. In-situ study of morphology and growth of primary α-Al(FeMnCr)Si intermetallics in an Al-Si alloy10.1016/j.actamat.2017.03.026 ↗
61. Plastic deformation and damage modeling of AA7075 synthetic 3D microstructure created using generative AI10.1016/j.actamat.2024.120431 ↗
62. Tensile damage and fracture of high vacuum die-cast AlSiMgMn alloys with in-situ X-ray microtomography10.1016/j.msea.2025.147869 ↗
63. Evolution of sludge particles in secondary die-cast aluminum alloys as function of Fe, Mn and Cr contents10.1016/j.matchemphys.2014.12.050 ↗
64. Precipitation of primary Fe-rich compounds in secondary AlSi9Cu3(Fe) alloys10.1007/s10973-015-4952-y ↗
65. Achievement of high strength and ductility in Al–Si–Cu–Mg alloys by intermediate phase optimization in as-cast and heat treatment conditions10.3390/ma13030647 ↗