Influence of ageing on the high-temperature mechanical strength of the Al-4Mn-3Ni-2Cu-1Zr alloy produced by laser powder bed fusion
Source abstract
Abstract
The mechanical properties of additively manufactured aluminium alloys at room temperature are often optimized through post-fabrication heat treatment (peak ageing). However, at high temperatures, peak-ageing does not necessarily result in the best mechanical properties. This raises the question of whether there is an optimal microstructure depending on the operating temperature. Herein, we examine the influence of ageing in an Al-4Mn-3Ni-2Cu-1Zr (wt.%) alloy processed by laser powder bed fusion on the tensile yield strength from room temperature to 300°C at 10 -2 and 10 -5 s -1 . In the stress-relieved conditions, the material shows a higher yield strength than in the peak-aged conditions at temperatures above 150°C at 10 -2 s -1 and as low as 100°C at 10 -5 s -1 . This evolution was not expected since nanoscale L1 2 -Al 3 Zr thermally stable precipitates form in the peak-aged conditions. The microstructure evolutions upon ageing are characterized across all scales and provide insights to rationalize the evolution of the alloy strength with temperature. The role of different microstructural features such as grain size, intermetallic morphology, nanoscale precipitates and solid solution composition is discussed. While the nanoscale Zr-rich precipitates contribute greatly to the room-temperature yield strength, their effect at elevated temperatures, typically >150°C, is minor. On the contrary, the supersaturation in Mn in the as-built material that is preserved after stress-relief is found to have a large impact on the tensile yield strength at elevated temperature. The globularisation of the elongated intermetallics observed in the stress-relieved microstructure is also identified to lower the elevated-temperature yield strength.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · High Entropy Alloys Studies · Aluminum Alloy Microstructure Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (43)
Show source-provided references
1. A creep-resistant additively manufactured Al-Ce-Ni-Mn alloy10.1016/j.actamat.2022.117699 ↗
2. An additively manufactured near-eutectic Al-Ce-Ni-Mn-Zr alloy with high creep resistance10.1016/j.actamat.2024.119787 ↗
3. Design of Al–Fe–Mn alloy for both high-temperature strength and sufficient processability of laser powder bed fusion
4. An Al-5Fe-6Cr alloy with outstanding high temperature mechanical behavior by laser powder bed fusion
5. Al-Cu-Ce(-Zr) alloys with an exceptional combination of additive processability and mechanical properties
6. An additively manufactured AlCuMnZr alloy microstructure and tensile mechanical properties10.1016/j.mtla.2020.100758 ↗
7. Microstructural development and aging behavior of Al–Cr–Zr heat-resistant alloy fabricated using laser powder bed fusion10.1016/j.jmrt.2021.10.027 ↗
8. Microstructure and strengthening of Al-6Ce-3Ni-0.7Fe (wt%) alloy manufactured by laser powder-bed fusion
9. Microstructures and high temperature tensile behaviours of laser powder bed fusion fabricated al-mn-sc alloy10.3390/met13040788 ↗
10. Multi-scale microstuctural investigation of a new Al-Mn-Ni-Cu-Zr aluminium alloy processed by laser powder bed fusion10.1016/j.mtla.2021.101160 ↗
11. Towards high-temperature applications of aluminium alloys enabled by additive manufacturing10.1080/09506608.2021.1951580 ↗
12. 3D printing of high-strength aluminium alloys10.1038/nature23894 ↗
13. Additive manufacturing of novel aluminium matrix composites with enhanced strength and processability via boron nitride functionalization
14. Revealing the precipitation behavior of crack-free TiB2/Al-Zn-Mg-Cu composites manufactured by laser Powder Bed fusion
15. Ageing response and strengthening mechanisms in a new Al-Mn-Ni-Cu-Zr alloy designed for laser powder bed fusion10.1016/j.actamat.2023.119271 ↗
16. Microstructure and mechanical properties of Al-Mg-Zr alloys processed by selective laser melting10.1016/j.actamat.2018.04.053 ↗
17. Microstructural evolution and strengthening mechanisms in a heat-treated additively manufactured Al–Cu–Mn–Zr alloy10.1016/j.msea.2022.142928 ↗
18. Direct ageing of LPBF Al-1Fe-1Zr for high conductivity and mechanical performance10.1016/j.actamat.2023.119199 ↗
19. Coarsening- and creep resistance of precipitation-strengthened Al–Mg–Zr alloys processed by selective laser melting10.1016/j.actamat.2020.02.008 ↗
20. Influence of microstructure heterogeneity on the tensile response of an aluminium alloy designed for laser powder bed fusion10.1016/j.actamat.2024.119786 ↗
21. Advancing novel Al-Mn-Cr-Zr based family of alloys tailored for powder bed fusion-laser beam process10.1016/j.jallcom.2023.171685 ↗
22. Effect of precipitation kinetics on microstructure and properties of novel Al-Mn-Cr-Zr based alloys developed for powder bed fusion – laser beam process10.1016/j.jallcom.2022.165870 ↗
23. Mechanical properties and microstructural characterisation including high-temperature performance of Al-Mn-Cr-Zr-based alloys tailored for additive manufacturing10.1016/j.matdes.2024.113160 ↗
24. Origin of non-uniform plasticity in a high-strength Al-Mn-Sc based alloy produced by laser powder bed fusion10.1016/j.jmst.2021.06.042 ↗
25. Selective laser melting of a high strength Al Mn Sc alloy: alloy design and strengthening mechanisms10.1016/j.actamat.2019.04.014 ↗
26. Tensile creep mechanisms of Al-Mn-Sc alloy fabricated by additive manufacturing
27. Automated crystal orientation and phase mapping in TEM10.1016/j.matchar.2014.08.010 ↗
28. Determination of matrix composition based on solute‐solute nearest‐neighbor distances in atom probe tomography10.1002/jemt.20899 ↗
29. Optimization of the strength vs. conductivity trade-off in an aluminium alloy designed for laser powder bed fusion10.1016/j.msea.2022.144139 ↗
30. Metrology of small particles and solute clusters by atom probe tomography10.1016/j.actamat.2020.02.023 ↗
31. Towards an alloy design strategy by tuning liquid local ordering: what solidification of an Al-alloy designed for laser powder bed fusion teaches Us
32. Criteria for developing castable, creep-resistant aluminum-based alloys – a review
33. Modeling of rapid solidification in laser powder Bed fusion processes10.1016/j.commatsci.2024.112918 ↗
34. Ultrahigh strength heat-resistant Al-Fe-V-Si-Sc alloy fabricated by laser powder bed fusion10.1016/j.jmst.2025.02.060 ↗
35. Influence of the microstructure on the high temperature ductility of the Al-4Mn-3Ni-2Cu-1Zr aluminium alloy designed for laser powder bed fusion10.1016/j.msea.2025.148559 ↗
36. Analysis of three-dimensional atom-probe data by the proximity histogram10.1007/S100050010051 ↗
37. Contribution of grain boundary sliding in low-temperature superplasticity of ultrafine-grained aluminum alloys10.1016/j.scriptamat.2009.10.010 ↗
38. Superplastic deformation mechanism of an ultrafine-grained aluminum alloy produced by friction stir processing10.1016/j.actamat.2010.05.003 ↗
39. Combining solution-, precipitation- and load-transfer strengthening in a cast Al-Ce-Mn-Sc-Zr alloy10.1016/j.actamat.2024.119683 ↗
40. Mechanical properties of Al(Sc,Zr) alloys at ambient and elevated temperatures10.1016/S1359-6454(03)00320-3 ↗
41. Solute-induced strengthening during creep of an aged-hardened Al-Mn-Zr alloy10.1016/j.actamat.2021.117268 ↗
42. First-principles study of solute-dislocation interaction in aluminum-rich alloys10.1103/PhysRevB.64.224203 ↗
43. Creep of metal matrix composites