journal article·2025-10Open access

Activating the highly desirable transformation-induced plasticity effect in cold-drawn Ti-6Al-4V wires through two-step annealing

Xuefeng Zhou, Zhengwei He, Jiaju Wu, Zilin Liu, Yiyou Tu, Feng Fang, Jianqing Jiang

Abstract

Stress-induced martensite transformation (SIMT) and the consequent transformation-induced plasticity (TRIP), established as effective strategies for enhancing strain hardening ability and ductility in metallic materials, are seldom observed and utilized to mitigate the issue of restricted cold deformability in Ti-6Al-4V alloy. This study investigates potential factors influencing SIMT in Ti-6Al-4V, employing one- and two-step annealing approaches on cold-drawn wires within the enigmatic lower α+β regime (500–800 °C). In the one-step annealing scenario, SIMT is solely activated at 750 °C and absent at either lower or higher temperatures. Conversely, two-step annealing, which entails an initial annealing at 800 °C followed by a subsequent annealing at 600–750 °C, facilitates the reactivation of SIMT across a broader temperature spectrum. The onset of SIMT is found to be influenced by several β phase characteristics, including adequate β stabilizer concentrations, diminished dislocation densities, and micron-sized grains. For the deformed Ti-6Al-4V, these factors, which are contradictory in one-step annealing, can be adeptly harmonized through two-step annealing. The first annealing enables dislocation annihilation, while the second annealing engenders reverted β phases with appropriate sizes and compositions. Notably, the two-step annealed 800 + 700WQ achieves an extremely high strain hardening rate exceeding 6.5 GPa and a substantial total elongation of around 22 %, exemplifying the highly desired TRIP effect in the cold-drawn Ti-6Al-4V wires.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Titanium Alloys Microstructure and Properties · Metal and Thin Film Mechanics · Welding Techniques and Residual Stresses

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (24)

Show source-provided references
1. On the strain hardening abilities of α+ β titanium alloys: the roles of strain partitioning and interface length density10.1016/j.jallcom.2019.152040 ↗
2. Influence of alloy element partitioning on strength of primary α phase in Ti-6Al-4V alloy10.1016/j.jmst.2017.07.016 ↗
3. Effects of heating rate on the alloy element partitioning and mechanical properties in equiaxed α+β Ti-6Al-4V alloy10.1016/j.jmst.2021.02.061 ↗
4. A strategy to improve the work-hardening behavior of Ti-6Al-4V parts produced by additive manufacturing10.1080/21663831.2016.1245681 ↗
5. Strength and ductility-related mechanical properties of ultrafine grained two-phase titanium alloy produced by warm multiaxial forging10.1016/j.msea.2011.12.102 ↗
6. Achieving superior ductility for laser solid formed extra low interstitial Ti-6Al-4V titanium alloy through equiaxial alpha microstructure10.1016/j.scriptamat.2017.11.021 ↗
7. Dislocation hardening and phase transformation-induced high ductility in Ti-6Al-4V with a heterogeneous martensitic microstructure under tensile load10.1016/j.jallcom.2021.159155 ↗
8. Realizing superior ductility of selective laser melted Ti-6Al-4V through a multi-step heat treatment10.1016/j.msea.2020.140367 ↗
9. Micromechanical behavior and thermal stability of a dual-phase α+α’ titanium alloy produced by additive manufacturing10.1016/j.actamat.2018.09.050 ↗
10. Room-temperature ductility of Ti-6Al-4V alloy with α′ martensite microstructure10.1016/j.msea.2010.10.070 ↗
11. On the design of new β-metastable titanium alloys with improved work hardening rate thanks to simultaneous TRIP and TWIP effects10.1016/j.scriptamat.2012.01.049 ↗
12. Deformation-induced martensitic transformation in a new metastable β titanium alloy10.1016/j.jallcom.2015.07.263 ↗
13. Stress-introduced α″ martensite and twinning in a multifunctional titanium alloy10.1016/j.scriptamat.2007.09.010 ↗
14. Unusual stress-induced martensite transformation in Ti-6Al-4V alloy enabled by solution treatment in the lower α+β regime10.1016/j.jallcom.2023.170330 ↗
15. Thermal and mechanical stability of retained austenite surrounded by martensite with different degrees of tempering10.1016/j.msea.2017.03.017 ↗
16. Increase of martensite start temperature after small deformation of austenite10.1016/j.msea.2014.04.108 ↗
17. Mechanical stabilisation of austenite10.1179/174328406X86128 ↗
18. Effect of cold rolling and solution treatment on β stability and mechanical properties of a metastable β-Ti alloy
19. The origin of striation in the metastable β phase of titanium alloys observed by transmission electron microscopy10.1107/S1600576717004150 ↗
20. Metastable dual-phase ti-nb-sn-zr and ti-nb-sn-fe alloys with high strength-to-modulus ratio
21. A review of metastable beta titanium alloys10.3390/met8070506 ↗
22. The concern of elasticity in stress-induced martensitic transformation in NiTi10.1016/S0921-5093(98)00959-9 ↗
23. Thermoelastic behavior in martensitic transformations10.1016/0036-9748(75)90418-4 ↗
24. Factors influencing the austenite stability during tensile testing of quenching and partitioning steel determined via in-situ electron backscatter diffraction10.1016/j.msea.2015.04.075 ↗