An analysis of the influence of heat treatments and surface finishing conditions on the high cycle fatigue behaviour of W360 hot work tool steel produced by Powder Bed Fusion – Laser Beam
Source abstract
Abstract
High-cycle fatigue behaviour of W360 steel produced by Powder Bed Fusion – Laser Beam (PBF-LB) is explored by comparing post-processing of industrial interest, involving both heat treatments (conventional quenching and multiple tempering (CHT), or innovative high-pressure heat treatment (HPHT)) and surface finishing (sandblasting, machining, shot peening). The combination of HPHT and machining returns the highest fatigue strength (767 ± 10 MPa) by reason of: i) reduced number and size of process-related defects compared to CHT and machining (457 ± 19 MPa); ii) reduced surface roughness compared to HPHT and sandblasting (243 ± 23 MPa) and HPHT and shot-peening (403 ± 19 MPa). The latter combination, however, shows an improved fatigue strength than the sandblasted one, thanks to compressive residual stress in the superficial region. The correlation between killer defect and fatigue performance is also discussed based on the Kitagawa-Takahashi diagram and the El-Haddad model, and compared to the conventionally manufactured steel. • High-pressure heat treatment (HPHT) on PBF-LB W360 steel reduces defect content and size. • HPHT leads to higher fatigue strength then quenching and multiple tempering. • Machining post-HPHT represents the best surface finishing solution to improve fatigue. • Shot peening improves fatigue strength over sandblasting by compressive residual stress. • A unique curve can represent the relationship between defect size and fatigue strength.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · High Entropy Alloys Studies · Welding Techniques and Residual Stresses
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (63)
Show source-provided references
1. Replacement of nitrided 33CrMoV steel with ESR hot work tool steels for motorsport applications: microstructural and fatigue characterization10.1007/s11665-018-3481-9 ↗
2. Heat treating of hot-work tool steels
3. Laser powder bed fusion of potential superalloys: a review10.3390/met11010058 ↗
4. Additive manufacturing of tool steels
5. Properties and applications of additively manufactured metallic cellular materials: a review10.1016/j.pmatsci.2021.100918 ↗
6. On the current research progress of metallic materials fabricated by laser powder bed fusion process: a review10.1016/j.jmrt.2022.07.085 ↗
7. Additive manufacturing of metallic components – process, structure and properties10.1016/j.pmatsci.2017.10.001 ↗
8. Effect of heat treatment and defects on the tensile behavior of a hot work tool steel manufactured by laser powder bed fusion10.1111/ffe.14025 ↗
9. Advanced manufacturing of high-speed steels: a critical review of the process design, microstructural evolution, and engineering performance10.1016/j.jmrt.2023.04.269 ↗
10. Hot work tool steel processed by laser powder bed fusion: a review on most relevant influencing factors10.1002/adem.202170027 ↗
11. Defects in a laser powder bed fused tool steel10.1002/adem.202000833 ↗
12. Influence of solidification cell structure on the martensitic transformation in additively manufactured steels
13. Impact of in situ heat treatment effects during laser‐based powder bed fusion of 1.3343 high‐speed steel with preheating temperatures up to 700 °C10.1002/srin.202200775 ↗
14. Deep cryogenic treatment of AISI M2 high-speed steel
15. Effects of pressure on microstructure and residual stresses during hot isostatic pressing post treatment of AISI M50 produced by laser powder-bed fusion10.3390/met11040596 ↗
16. Improving the fatigue strength of laser powder bed‐fused AISI M3:2 by hot isostatic pressing10.1002/srin.202200435 ↗
17. Laser beam melting and heat-treatment of 1.2343 (AISI H11) tool steel – microstructure and mechanical properties10.1016/j.msea.2018.11.001 ↗
18. A short review on selective laser melting of H13 steel10.1007/s00170-020-05584-4 ↗
19. A study of microstructure and cracking behavior of H13 tool steel produced by laser powder bed fusion using single-tracks, multi-track pads, and 3D cubes10.1016/j.jmatprotec.2020.116802 ↗
20. Tool steels
21. Impact of in situ heat treatment effects during laser‐based powder bed fusion of 1.3343 high‐speed steel with preheating temperatures up to 700 °C10.1002/srin.202200775 ↗
22. Influence of preheating temperatures on material properties of PBF-LB manufactured hot-work tool steel X37CrMoV5-110.1016/j.procir.2022.08.143 ↗
23. General investigations on processing tool steel X40CrMoV5-1 with selective laser melting10.1016/j.jmatprotec.2018.01.012 ↗
24. Microstructural effects on the tensile and fracture behavior of selective laser melted H13 tool steel under varying conditions10.1016/j.matchar.2019.109817 ↗
25. Selective laser melting of H13: microstructure and residual stress10.1007/s10853-017-1380-3 ↗
26. Influence of solidification cell structure on the martensitic transformation in additively manufactured steels
27. Heat treatment and properties of a hot work tool steel fabricated by additive manufacturing10.1016/j.msea.2019.03.027 ↗
28. Effect of heat treatment on microstructure evolution of X38CrMoV5-1 hot-work tool steel produced by L-PBF10.1007/s11661-021-06248-y ↗
29. Tensile behaviour of a hot work tool steel manufactured via Laser Powder Bed Fusion: effect of an innovative high pressure heat treatment10.1016/j.prostr.2023.07.087 ↗
30. Effect of different heat treatments on tensile properties and unnotched and notched fatigue strength of cold work tool steel produced by powder Metallurgy10.3390/met12060900 ↗
31. Murakami · 2019
32. Material defects as cause for the fatigue failure of metallic components10.1016/j.ijfatigue.2019.06.024 ↗
33. Subsurface crack initiation and propagation mechanism in high-strength steel in a very high cycle fatigue regime10.1016/j.ijfatigue.2005.08.015 ↗
34. Influence of non-metallic inclusions on fatigue life in the very high cycle fatigue regime10.1016/j.ijfatigue.2015.11.001 ↗
35. Influence of carbide and inclusion contents on the fatigue properties of high speed steels and tool steels10.1016/S0142-1123(00)00087-6 ↗
36. Defects as a root cause of fatigue failure of metallic components. III: cavities, dents, corrosion pits, scratches10.1016/j.engfailanal.2019.01.034 ↗
37. Defects as a root cause of fatigue failure of metallic components. I: basic aspects10.1016/j.engfailanal.2019.01.055 ↗
38. A comprehensive review on laser powder bed fusion of steels: processing, microstructure, defects and control methods, mechanical properties, current challenges and future trends10.1016/j.jmapro.2021.12.033 ↗
39. Effect of hot isostatic pressing on porosity and mechanical properties of 316 L stainless steel prepared by the selective laser melting method10.3390/ma13194377 ↗
40. Influence of heat treatment under hot isostatic pressing (HIP) on microstructure of intermetallic-reinforced tool steel manufactured by laser powder bed fusion10.1016/j.msea.2019.138699 ↗
41. Defect analysis for additively manufactured materials in fatigue from the viewpoint of quality control and statistics of extremes10.1016/j.prostr.2019.12.014 ↗
42. High cycle fatigue behavior and life prediction for additively manufactured 17-4 PH stainless steel: effect of sub-surface porosity and surface roughness10.1016/j.tafmec.2020.102477 ↗
43. Effects of post-processing on the surface finish, porosity, residual stresses, and fatigue performance of additive manufactured metals: a review10.1007/s11665-021-06021-7 ↗
44. Comparison of the fatigue strength between additively and conventionally fabricated tool steel 1.2344
45. Effects of building direction and defect sensitivity on the fatigue behavior of additively manufactured H13 tool steel10.1016/j.tafmec.2020.102634 ↗
46. Numerical and experimental evaluation of a conformally cooled H13 steel injection mould manufactured with selective laser melting10.1007/s00170-017-0426-7 ↗
47. https://www.voestalpine.com/additive-manufacturing/en/centers-of-excellence/am-center-germany.
48. https://www.bohler.it/en/products/w360-ampo.
49. Hot isostatic pressing for metal additive manufacturing
50. ImageJ2: ImageJ for the next generation of scientific image data10.1186/s12859-017-1934-z ↗
51. Defects and anomalies in powder bed fusion metal additive manufacturing10.1016/j.cossms.2021.100974 ↗
52. High-temperature oxidation behavior of Fe–1Cr–0.2Si steel10.3390/ma13030509 ↗
53. High-temperature oxidation behaviour of AISI H11 tool steel10.3390/met11050758 ↗
54. Quintus Purus®
55. Properties of the fine granular area and postulated models for its formation during very high cycle fatigue—a review10.3390/app10238475 ↗
56. Solubility of argon in laser additive manufactured α-titanium under hot isostatic pressing condition10.1016/j.commatsci.2017.01.040 ↗
57. Effect of thermal history on the superplastic expansion of argonfilled pores in titanium: Part I kinetics and microstructure10.1016/j.actamat.2004.01.039 ↗
58. The effectiveness of hot isostatic pressing for closing porosity in titanium parts manufactured by selective electron beam melting10.1007/s11661-016-3429-3 ↗
59. Effect of heat treatments on pore morphology and microstructure of laser additive manufactured parts
60. A comparison of fatigue strength sensitivity to defects for materials manufactured by AM or traditional processes10.1016/j.ijfatigue.2016.06.020 ↗
61. About the fatigue crack propagation threshold of metals as a design criterion – a review10.1016/j.engfracmech.2015.12.002 ↗
62. Fatigue properties of AlSi10Mg obtained by additive manufacturing: defect-based modelling and prediction of fatigue strength10.1016/j.engfracmech.2017.11.002 ↗
63. Garwood · 1951