journal article·2025-09

Impact of hydrogen-assisted cracking on the mechanical properties of 316L stainless steel produced by selective laser melting using an in-situ small punch test

Van Hung Dao, Kee Bong Yoon, Hee Soo Yun, Hyusang Kwon, Kyung-Oh Bae, Seung Hoon Nahm

Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Hydrogen embrittlement and corrosion behaviors in metals · High Temperature Alloys and Creep

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (64)

Show source-provided references
1. Additively manufactured hierarchical stainless steels with high strength and ductility10.1038/nmat5021 ↗
2. Dislocation network in additive manufactured steel breaks strength–ductility trade-off10.1016/j.mattod.2017.11.004 ↗
3. Intragranular cellular segregation network structure strengthening 316L stainless steel prepared by selective laser melting10.1016/j.jnucmat.2015.12.034 ↗
4. Hardened austenite steel with columnar sub-grain structure formed by laser melting10.1016/j.msea.2014.12.018 ↗
5. Determining the necessity of post‐processing heat treatment for the 316L stainless steel manufactured by laser powder bed fusion through evaluation of mechanical and corrosion properties
6. Anisotropic creep behavior of stainless steel produced by selective laser melting10.1016/j.msea.2020.140040 ↗
7. Overview of hydrogen-resistant alloys for high-pressure hydrogen environment: on the hydrogen energy structural materials10.1093/ce/zkad009 ↗
8. Permeability, solubility and diffusivity of hydrogen isotopes in stainless steels at high gas pressures10.1016/j.ijhydene.2006.05.008 ↗
9. Analysis of martensitic transformation in 304 type stainless steels tensile tested in high pressure hydrogen atmosphere by means of XRD and magnetic induction10.1016/j.ijhydene.2011.11.080 ↗
10. Investigation of crystal growth mechanism during selective laser melting and mechanical property characterization of 316L stainless steel parts10.1016/j.matdes.2016.03.111 ↗
11. About metastable cellular structure in additively manufactured austenitic stainless steels
12. New insights on cellular structures strengthening mechanisms and thermal stability of an austenitic stainless steel fabricated by laser powder-bed-fusion10.1016/j.actamat.2020.11.018 ↗
13. Characterization technique of gases permeation properties in polymers: H2, he, N2 and Ar gas10.1038/s41598-022-07321-1 ↗
14. Hydrogen sorption and desorption properties in rubbery polymer10.1016/j.matchemphys.2022.125745 ↗
15. Analyses of permeation characteristics of hydrogen in nitrile butadiene rubber using gas chromatography10.1016/j.matchemphys.2021.124653 ↗
16. Determination of permeation properties of hydrogen gas in sealing rubbers using thermal desorption analysis gas chromatography10.1038/s41598-021-96266-y ↗
17. Ductility and fatigue properties of low nickel content type 316L austenitic stainless steel after gaseous thermal pre-charging with hydrogen10.1016/j.ijhydene.2019.08.233 ↗
18. Hydrogen environment embrittlement of stable austenitic steels10.1016/j.ijhydene.2012.08.071 ↗
19. Effects of alloy composition and strain hardening on tensile fracture of hydrogen-precharged type 316 stainless steels10.1016/j.ijhydene.2007.10.046 ↗
20. Effect of strain-induced martensite on hydrogen embrittlement of austenitic stainless steels investigated by combined tension and hydrogen release methods10.1016/j.ijhydene.2013.01.198 ↗
21. Hydrogen embrittlement of additively manufactured austenitic stainless steel 316 L10.1016/j.corsci.2021.109790 ↗
22. Superior resistance to hydrogen damage for selective laser melted 316L stainless steel in a proton exchange membrane fuel cell environment10.1016/j.corsci.2019.108425 ↗
23. Effect of additive manufacturing and subsequent heat And/Or surface treatment on the hydrogen embrittlement sensitivity of 316L austenitic stainless steel10.1016/j.ijhydene.2023.05.215 ↗
24. Strain-induced twins and martensite: effects on hydrogen embrittlement of selective laser melted (SLM) 316 L stainless steel10.1016/j.corsci.2022.110669 ↗
25. Hydrogen embrittlement of austenitic stainless steels revealed by deformation microstructures and strain-induced creation of vacancies10.1016/j.actamat.2013.12.039 ↗
26. The effect of pre-strain on the resistance to hydrogen embrittlement in 316L austenitic stainless steel10.2320/matertrans.M2014036 ↗
27. Hydrogen embrittlement of 3-D printing manufactured austenitic stainless steel part for hydrogen service10.1016/j.scriptamat.2016.11.020 ↗
28. Hydrogen-induced softening and embrittlement in 316L stainless steel fabricated using laser-powder bed fusion10.1016/j.actamat.2024.119959 ↗
29. Formation of strain-induced martensite in selective laser melting austenitic stainless steel10.1016/j.msea.2018.10.121 ↗
30. Dislocation network in additive manufactured steel breaks strength–ductility trade-off10.1016/j.mattod.2017.11.004 ↗
31. Effect of aluminium on deformation mode and mechanical properties of austenitic Fe Mn Cr Al C alloys10.1016/0921-5093(94)09751-8 ↗
32. Strain hardening behavior of a TRIP/TWIP steel with 18.8% Mn10.1016/j.msea.2010.10.040 ↗
33. The dependence of hydrogen embrittlement on hydrogen transport in selective laser melted 304L stainless steel10.1016/j.ijhydene.2021.02.035 ↗
34. Hydrogen trapping and micromechanical behavior in additively manufactured CoCrFeNi high-entropy alloy in as-built and pre-strained conditions10.1016/j.actamat.2024.119886 ↗
35. Hydrogen uptake and its influence in selective laser melted austenitic stainless steel: a nanoindentation study10.1016/j.scriptamat.2020.113718 ↗
36. Effect of molten pool boundaries on the mechanical properties of selective laser melting parts10.1016/j.jmatprotec.2014.06.002 ↗
37. Influence of scan strategy and molten pool configuration on microstructures and tensile properties of selective laser melting additive manufactured aluminum based parts10.1016/j.optlastec.2017.08.015 ↗
38. Significance of melt pool structure on the hydrogen embrittlement behavior of a selective laser-melted 316L austenitic stainless steel10.3390/ma16041741 ↗
39. Transformation of austenite to duplex austenite-ferrite assembly in annealed stainless steel 316L consolidated by laser melting10.1016/j.jallcom.2015.01.249 ↗
40. Effects of process parameters on the high temperature strength of 17-4PH stainless steel produced by selective laser melting10.1007/s12206-020-0718-y ↗
41. Effects of scanning speed on creep behaviour of 316L stainless steel produced using selective laser melting10.1111/ffe.13298 ↗
42. Investigation into the effect of process parameters on microstructural and physical properties of 316L stainless steel parts by selective laser melting10.1007/s00170-014-6297-2 ↗
43. Development of a methodology to study the hydrogen embrittlement of steels by means of the small punch test10.1016/j.msea.2014.12.083 ↗
44. Hydrogen compatibility evaluation of ferritic steels using a combined method of small punch test (SPT) and numerical simulation for notched specimens10.1016/j.ijhydene.2024.10.149 ↗
45. Effect of energy density and scanning strategy on densification, microstructure and mechanical properties of 316L stainless steel processed via selective laser melting10.1016/j.msea.2019.138455 ↗
46. Effects of wall thickness variation on hydrogen embrittlement susceptibility of additively manufactured 316L stainless steel with lattice auxetic structures10.3390/ma16062523 ↗
47. Effect of precharging methods on the hydrogen embrittlement of 304 stainless steel10.1016/j.ijhydene.2023.09.073 ↗
48. Environment hydrogen embrittlement of pipeline steel X70 under various gas mixture conditions with in situ small punch tests10.1016/j.msea.2020.139114 ↗
49. Study of the influence of current density and displacement rate on hydrogen embrittlement using small punch tests10.1016/j.tafmec.2023.103838 ↗
50. Hull · 2011 · vol. 37
51. Geometrically necessary dislocations, hardening, and a simple gradient theory of crystal plasticity10.1016/S1359-6462(02)00337-8 ↗
52. Christian · 2002
53. Dislocation-type evolution in quasi-statically compressed polycrystalline nickel10.1016/j.actamat.2018.05.022 ↗
54. Review on superior strength and enhanced ductility of metallic nanomaterials10.1016/j.pmatsci.2018.02.002 ↗
55. New discoveries in deformed metals10.1007/s11661-001-0167-x ↗
56. Hydrogen-enhanced localized Plasticity—A mechanism for hydrogen-related fracture10.1016/0921-5093(94)90975-X ↗
57. Hydrogen effects on the interaction between dislocations10.1016/S1359-6454(97)00349-2 ↗
58. Hydrogen permeation behavior and hydrogen-induced defects in 316L stainless steels manufactured by additive manufacturing10.1016/j.matchemphys.2020.123038 ↗
59. The dual role of coherent twin boundaries in hydrogen embrittlement10.1038/ncomms7164 ↗
60. Hydrogen-assisted twin boundary fracture of type 304 austenitic stainless steel at low temperature investigated by scanning probe microscopy
61. Hydrogen trapping in laser powder bed fusion 316l stainless steel10.3390/met12101748 ↗
62. Effect of processing parameters on microstructure and tensile properties of austenitic stainless steel 304L made by directed energy deposition additive manufacturing10.1016/j.actamat.2016.03.019 ↗
63. Trap theory of hydrogen embrittlement10.1016/0001-6160(80)90106-6 ↗
64. A kinetic trapping model for hydrogen-induced cracking10.1016/0001-6160(79)90059-2 ↗