journal article·2025-07Open access

Toughening nitride hard coatings by deflecting cracks along grain boundaries

Yinxia Zhang, Matthias Bartosik, Steffen Brinckmann, Subin Lee, Christoph Kirchlechner

Abstract

Grain boundaries (GBs) in hard coatings are often considered as the weakest link, acting as preferred pathways for crack propagation and thereby limiting the coating's fracture toughness. In this study, we investigate whether continuous crack deflection along GBs can mitigate this limitation and enhance the fracture resistance of hard coatings. Three model systems were examined: CrN, AlN and their multilayered structure coatings, all characterized by columnar GB structures. Fracture toughness was quantitatively assessed using an in situ SEM micro-cantilever fracture testing. The key approach of this study is the use of two different loading geometries, with notches aligned either parallel or perpendicular to the coating's growth direction, allowing us to compare the influence of the crack propagation direction and deflection. Across all three systems, the perpendicular notch configuration—aligned across the columnar microstructure—resulted in approximately 8 % higher fracture toughness. This enhancement is attributed to continuous crack deflection along GBs during deformation. Additionally, the extent of crack deflection was found to depend on the local GB arrangement, with transgranular fracture observed when no well-aligned GBs were present along the crack path. These findings provide quantitative insights into the toughening mechanisms enabled by GB-mediated crack deflection and offer design strategies for mechanically robust hard coatings.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Metal and Thin Film Mechanics · Diamond and Carbon-based Materials Research · Boron and Carbon Nanomaterials Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (38)

Show source-provided references
1. Aerospace coatings
2. The contribution of surface engineering to the product performance in the automotive industry10.1016/S0257-8972(03)00371-2 ↗
3. High-performance coatings for cutting tools10.1016/j.cirpj.2016.11.004 ↗
4. Microstructural design of hard coatings10.1016/j.pmatsci.2006.02.002 ↗
5. Hard coatings for cutting applications: physical vs. chemical vapor deposition and future challenges for the coatings community10.1016/j.surfcoat.2021.127949 ↗
6. Functional and smart coatings for corrosion protection: a review of recent advances10.1016/j.surfcoat.2014.06.031 ↗
7. Bilayer period and ratio dependent structure and mechanical properties of TiN/MoN superlattices10.1016/j.actamat.2024.120313 ↗
8. Anderson · 2005
9. 1997
10. A review of experimental approaches to fracture toughness evaluation at the micro-scale10.1016/j.matdes.2019.107762 ↗
11. Analysis of stresses and strains near the end of a crack traversing a plate10.1115/1.4011547 ↗
12. In situ mechanical testing of hard yet tough high entropy nitride coatings deposited on compliant steel substrates10.1016/j.tsf.2023.140137 ↗
13. Phase-field simulations of microstructure evolution during physical vapor deposition of single-phase thin films10.1016/j.commatsci.2017.01.034 ↗
14. High rate thick film growth10.1146/annurev.ms.07.080177.001323 ↗
15. Growth defects in PVD hard coatings10.1016/j.vacuum.2009.05.018 ↗
16. Annealing activated substrate element diffusion and its influence on the microstructure and mechanical properties of CVD TiN/TiCN coatings10.1016/j.surfcoat.2024.131079 ↗
17. Measuring fracture toughness of coatings using focused-ion-beam-machined microbeams10.1557/JMR.2005.0048 ↗
18. A comparative micro-cantilever study of the mechanical behavior of silicon based passivation films10.1016/j.tsf.2009.07.143 ↗
19. From quantum to continuum mechanics: studying the fracture toughness of transition metal nitrides and oxynitrides10.1080/21663831.2017.1414081 ↗
20. Grain boundary design of thin films: using tilted brittle interfaces for multiple crack deflection toughening10.1016/j.actamat.2016.09.027 ↗
21. On the interplay between microstructure, residual stress and fracture toughness of (Hf-Nb-Ta-Zr) C multi-metal carbide hard coatings10.1016/j.matdes.2022.111323 ↗
22. On the fracture behavior of Cr2AlC coatings10.1016/j.matdes.2021.109757 ↗
23. Segregation-enhanced grain boundary embrittlement of recrystallised tungsten evidenced by site-specific microcantilever fracture10.1016/j.actamat.2023.119256 ↗
24. The influence of microstructural orientation on fracture toughness in (V, Al)N and (V, Al)(O, N) coatings as measured by microcantilever bending10.1557/s43578-023-01111-9 ↗
25. Anisotropy of fracture toughness in nanostructured ceramics controlled by grain boundary design10.1016/j.matdes.2018.11.028 ↗
26. The importance of fracture toughness in ultrafine and nanocrystalline bulk materials10.1080/21663831.2016.1166403 ↗
27. Nanostructured NbMoTaW high entropy alloy thin films: high strength and enhanced fracture toughness10.1016/j.scriptamat.2019.04.011 ↗
28. Direct observation of crack arrest after bridge notch failure: a strategy to increase statistics and reduce FIB-Artifacts in micro-cantilever testing10.1016/j.matdes.2023.112188 ↗
29. Becker · 2022
30. Thermal expansion of Ti-Al-N and Cr-Al-N coatings10.1016/j.scriptamat.2016.09.022 ↗
31. An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments10.1557/JMR.1992.1564 ↗
32. Fracture in small-scale structures and confined volumes10.1557/s43577-022-00382-7 ↗
33. Can microscale fracture tests provide reliable fracture toughness values? A case study in silicon10.1557/jmr.2015.2 ↗
34. Columnar grain boundaries are the weakest link in hard coatings: insights from micro-cantilever testing with bridge notches
35. Designing superhard, self-toughening CrAlN coatings through grain boundary engineering10.1016/j.actamat.2012.06.049 ↗
36. Tuning mechanical properties of ultrafine-grained tungsten by manipulating grain boundary chemistry10.1016/j.actamat.2022.117939 ↗
37. Delamination toughening assisted by phosphorus in medium-carbon low-alloy steels with ultrafine elongated grain structures10.1016/j.msea.2015.09.102 ↗
38. Hard and tough CrN coatings strengthened by high-density distorted coherent grain boundaries10.1016/j.jallcom.2021.162139 ↗