Comparative study of heat treatment effects on the mechanical properties of laser directed energy deposited Ti6Al4V alloy with and without ultrasonic impact treatment
Bibliographic record
Abstract
No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.
Source: Not provided · Quality: missing
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · High Entropy Alloys Studies · Surface Treatment and Residual Stress
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (49)
Show source-provided references
1. High-strength titanium alloys for aerospace engineering applications: a review on melting-forging process10.1016/j.msea.2022.143260 ↗
2. Solidification microstructure variations in additively manufactured Ti-6Al-4V using laser powder bed fusion10.1016/j.scriptamat.2023.115430 ↗
3. Preliminary study on machining of additively manufactured Ti-6Al-4V
4. A critical review on additive manufacturing of Ti-6Al-4V alloy: microstructure and mechanical properties10.1016/j.jmrt.2022.04.055 ↗
5. Microstructure, static properties, and fatigue crack growth mechanisms in Ti-6Al-4V fabricated by additive manufacturing: LENS and EBM10.1016/j.engfailanal.2016.05.036 ↗
6. Anisotropic tensile behavior of Ti–6Al–4V components fabricated with directed energy deposition additive manufacturing10.1016/j.actamat.2014.12.054 ↗
7. Residual stress and texture control in Ti-6Al-4V wire + arc additively manufactured intersections by stress relief and rolling10.1016/j.matdes.2018.03.065 ↗
8. Combining manufacturing of titanium alloy through direct energy deposition and laser shock peening processes10.1016/j.matdes.2021.109626 ↗
9. Experimental optimization for fatigue life maximization of additively manufactured Ti-6Al-4V alloy employing ultrasonic impact treatment10.1007/s11665-021-05576-9 ↗
10. Effects of combining ultrasonic micro-forging treatment with laser metal wire deposition on microstructural and mechanical properties in Ti–6Al–4V alloy10.1016/j.matchar.2020.110187 ↗
11. Interpass rolling of Ti-6Al-4V wire + arc additively manufactured features for microstructural refinement
12. Laser shock peening of laser based directed energy deposition and powder bed fusion additively manufactured parts: a review10.1007/s12540-022-01334-1 ↗
13. Laser shock peening of laser additive manufactured Ti6Al4V titanium alloy10.1016/j.surfcoat.2018.06.020 ↗
14. Reducing the anisotropy of the mechanical properties of directed energy deposited Ti6Al4V alloy with inter-layer ultrasonic impact peening and heat treatment10.1016/j.msea.2022.144123 ↗
15. Strengthening effect in laser metal deposited Ti6Al4V alloy via layer-by-layer ultrasonic impact treatment10.1016/j.msea.2023.145693 ↗
16. Effect of electropulsing treatment on the microstructure and mechanical properties of Ti6Al4V alloy processed by a hybrid method of directed energy deposition and layer-by-layer ultrasonic impact peening10.1016/j.msea.2024.146774 ↗
17. Heat treatment for metal additive manufacturing10.1016/j.pmatsci.2022.101051 ↗
18. Heat treatment of Ti6Al4V produced by selective laser melting: microstructure and mechanical properties10.1016/j.jallcom.2012.07.022 ↗
19. Effect of heat treatment on the microstructure and mechanical properties of selective laser-melted Ti64 and Ti-5Al-5Mo-5V-1Cr-1Fe10.3390/met11040534 ↗
20. Globularization mechanism and mear isotropic properties in subcritical heat-treated Ti6Al4V fabricated by directed energy deposition10.1007/s40195-022-01516-1 ↗
21. Experimental and numerical simulation to study the reduction of welding residual stress by ultrasonic impact treatment10.3390/ma13040837 ↗
22. Effects of ultrasonic impact treatment on the stress-controlled fatigue performance of additively manufactured DMLS Ti-6Al-4V Alloy10.3390/app9224787 ↗
23. Residual stress, mechanical properties, and grain morphology of Ti-6Al-4V alloy produced by ultrasonic impact treatment assisted wire and arc additive manufacturing10.3390/met8110934 ↗
24. Effect of subtransus heat treatment on the microstructure and mechanical properties of additively manufactured Ti-6Al-4V alloy10.1016/j.jallcom.2017.11.263 ↗
25. Microstructural evolution and tensile property enhancement of remanufactured Ti6Al4V using hybrid manufacturing of laser directed energy deposition with laser shock peening
26. Microstructure and mechanical properties of laser metal deposited Ti6Al4V alloy with near equiaxed β grain structure10.1016/j.jmrt.2022.12.068 ↗
27. Role of changes in heat input on additively manufactured Ti–6Al–4V fabricated by directed energy deposition10.1016/j.msea.2021.141541 ↗
28. Comparison of direct energy deposition and powder bed fusion technology in the preparation of Ti–6Al–4V alloy10.1016/j.jmrt.2025.01.231 ↗
29. Microstructure evolution, tensile properties, and fatigue damage mechanisms in Ti-6Al-4V alloys fabricated by two additive manufacturing techniques10.1016/j.proeng.2015.08.007 ↗
30. Effect of solution temperature on microstructure and properties of Ti6Al4V by laser-directed energy deposition10.1007/s11665-022-07244-y ↗
31. Post-annealing effect on the tensile deformation mechanism of a Ti–6Al–4V alloy manufactured via directed energy deposition10.1016/j.msea.2022.142729 ↗
32. Additive manufacturing of Ti-6Al-4V alloy by hybrid plasma-arc deposition and microrolling: grain morphology, microstructure, and tensile properties10.1007/s11431-021-1991-7 ↗
33. Influence of in situ micro-rolling on the improved strength and ductility of hybrid additively manufactured metals10.1016/j.engfracmech.2021.107868 ↗
34. Isotropic and improved tensile properties of Ti-6Al-4V achieved by in-situ rolling in direct energy deposition
35. Research on microstructure and mechanical properties of Ti–6Al–4V ELI fabricated by hybrid directed energy deposition with in-situ rolling and annealing10.1016/j.matchar.2024.113914 ↗
36. Effect of low-temperature annealing on microstructure and mechanical properties of Ti6Al4V produced by laser shock peening10.1016/j.msea.2023.145317 ↗
37. Effects of heat treatments on microstructure and properties of Ti-6Al-4V ELI alloy fabricated by electron beam melting (EBM)10.1016/j.msea.2017.01.019 ↗
38. Effects of synchronized magnetic arc oscillation on microstructure, texture, grain boundary and mechanical properties of wire arc additively manufactured Ti6Al4V alloy
39. Formation mechanism and characterization of nanostructured Ti6Al4V alloy prepared by mechanical alloying10.1016/j.matdes.2011.12.044 ↗
40. Evaluation of dislocation densities in various microstructures of additively manufactured Ti6Al4V (Eli) by the method of X-ray diffraction10.3390/ma13235355 ↗
41. A modified Hall–Petch relationship in ultrafine-grained titanium recycled from chips by equal channel angular pressing10.1016/j.scriptamat.2012.02.008 ↗
42. Gradient microstructure evolution in laser shock peened Ti6Al4V titanium alloy10.1016/j.surfcoat.2022.128378 ↗
43. Overcoming the strength-ductility trade-off and anisotropy of mechanical properties of Ti6Al4V with electron beam powder bed fusion10.1016/j.msea.2023.145301 ↗
44. Simultaneously enhancing the hot workability and room-temperature strength of Ti-6Al-4V alloy via adding Mo and Fe10.1016/j.jmst.2023.04.054 ↗
45. Microstructure evolution and mechanical properties of multi-layer deposition of Ti-6Al-4V-5Ni alloy developed by μ-plasma-based metal additive manufacturing process10.1007/s00170-023-11491-1 ↗
46. A study of Cu modified Ti–6Al–4V deposits fabricated by wire-arc directed energy deposition: alloy design, microstructure, and mechanical properties10.1016/j.msea.2023.145750 ↗
47. Modelling strengthening mechanisms in beta-type Ti alloys10.1016/j.msea.2019.04.027 ↗
48. Quantitatively analyzing strength contribution vs grain boundary scale relation in pure titanium subjected to severe plastic deformation10.1007/s11661-016-3391-0 ↗
49. Polygonization: theory and comparison with experiments10.1016/j.ijengsci.2012.03.005 ↗