Microstructural changes and mechanical property response to aging heat treatment in hypereutectoid Ti–Au–Mo biomedical alloys
Source abstract
Abstract
β (bcc) Ti–Au-based biomedical alloys are attractive due to their excellent biocompatibility, X-ray radiographic imaging properties, and shape memory effects. Furthermore, it was recently revealed that increasing the Au content beyond the eutectoid composition to 6 mol% Au exhibits a single β phase without the intermetallic compound Ti3Au and good superelasticity in hypereutectoid compositions. It has also been shown that specific heat treatment can produce Ti3Au with favorable mechanical properties. This study verified the feasibility of developing hypereutectoid Ti–Au–Mo ternary alloys from the viewpoint of aging heat treatment. By controlling the aging temperature and time, the precipitate could be controlled as ω, α, and/or Ti3Au. At aging temperatures higher than 773 K, aging products formed on the β grain boundaries, embrittling the alloy. Aging at 573 K resulted in a decrease in ductility and an increase in hardness with increasing aging time. These changes were more drastic at lower Au concentrations, with the smallest changes observed at 6 mol% Au. This study highlights the Mo equivalent as a measure of β phase stability, with values calculated based on empirical calculations or the binary phase diagram slope. Comparison with other Ti–Mo binary alloys with similar Mo equivalents suggests that Au causes less ω growth. These findings provide a solid foundation for the development of functional low-karat titanium-gold alloys for use in advanced medical devices.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Titanium Alloys Microstructure and Properties · Orthopaedic implants and arthroplasty · Bone Tissue Engineering Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (52)
Show source-provided references
1. Yamauchi · 2011
2. Effect of cyclic deformation on the pseudoelasticity characteristics of Ti-Ni alloys10.1007/BF02644447 ↗
3. Nickel hypersensitivity: a clinical review and call to action10.1111/j.1365-4632.2009.04307.x ↗
4. A review on alloy design, biological response, and strengthening of β-titanium alloys as biomaterials10.1016/j.msec.2020.111661 ↗
5. Gold nanoparticles: a new X-ray contrast agent10.1259/bjr/13169882 ↗
6. Study of corrosion in biocompatible metals for implants: a review10.1016/j.jallcom.2017.01.196 ↗
7. Characterization of passive layers formed on Ti–10 wt% (Ag, Au, Pd, or Pt) binary alloys and their effects on galvanic corrosion10.1016/j.corsci.2015.04.007 ↗
8. Metallic implant biomaterials10.1016/j.mser.2014.10.001 ↗
9. Exploration of hypereutectoid compositions for achieving and enhancing superelasticity in biomedical Ti–Au–Mo alloys
10. Change in microstructures and mechanical properties of biomedical Ti-Nb-Ta-Zr system alloy through cross-rolling10.2320/matertrans.MRA2008040 ↗
11. Microstructure evolution and deformation mechanism of α+β dual-phase Ti-xNb-yTa-2Zr alloys with high performance10.1016/j.jmst.2022.04.052 ↗
12. Tensile and superelastic behaviors of Ti-35Nb-2Ta-3Zr with gradient structure10.1016/j.matdes.2020.108961 ↗
13. The effect of ternary additions on the decompositon of metastable beta-phase titanium alloys10.1007/BF02663337 ↗
14. The precipitation of α-phase in metastable β-phase Ti alloys10.1007/BF03161837 ↗
15. The effect of omega phase on the mechanical properties of titanium alloys10.1007/BF02913423 ↗
16. Mechanical property optimization via microstructural control of new metastable beta titanium alloys10.1007/s11837-007-0010-y ↗
17. Influence of duplex ageing on secondary α precipitates and mechanical properties of the near β-Ti alloy Ti-5553110.1016/j.matchar.2018.06.025 ↗
18. Effect of annealing temperature on microstructure and superelastic properties of Ti-Au-Cr-Zr alloy10.2320/matertrans.M2014439 ↗
19. Improved trade-off between strength and plasticity in titanium based metastable beta type Ti-Zr-Fe-Sn alloys10.1016/j.msea.2019.138340 ↗
20. Morphological evolution of transformation products and eutectoid transformation(s) in a hyper-eutectoid Ti-12 at% Cu alloy10.1016/j.actamat.2019.01.044 ↗
21. Novel eutectoid Ti-5Ni alloy fabricated via direct energy deposition10.1016/j.scriptamat.2021.113918 ↗
22. Effect of Cu-induced eutectoid transformation on microstructure and mechanical properties of Ti–6Al–4V alloy by laser wire deposition10.1016/j.msea.2021.142316 ↗
23. Evaluations of mechanical properties and shape memory behaviors of the aging–treated Ti–Au–Mo alloys10.1016/j.matchemphys.2021.124775 ↗
24. Effect of 3d transition metal additions on the phase constituent, mechanical properties, and shape memory effect of near–eutectoid Ti–4Au biomedical alloys10.1016/j.jallcom.2020.157599 ↗
25. The Au-Ti (Gold-Titanium) system10.1007/BF02868667 ↗
26. The Mo−Ti (Molybdenum-Titanium) system10.1007/BF02881476 ↗
27. Effect of Cr additions on the phase constituent, mechanical properties, and shape memory effect of near–eutectoid Ti–4Au towards the biomaterial applications10.1016/j.jallcom.2021.159037 ↗
28. Superelasticity and tensile strength of Ti-Zr-Nb-Sn alloys with high Zr content for biomedical applications10.1016/j.intermet.2019.106545 ↗
29. Effect of aging on isothermal ω/α″ growth and resulting mechanical behaviors of the Ti–Mo–Al high temperature shape memory alloys10.1016/j.matchar.2023.112850 ↗
30. Effect of precipitation on mechanical properties in the β-Ti alloy Ti–24Nb–4Zr–8Sn10.1016/j.msea.2015.12.024 ↗
31. Effect of α phase precipitation on martensitic transformation and mechanical properties of metastable β Ti–6Cr–3Sn biomedical alloy10.1016/j.jallcom.2012.01.008 ↗
32. Improvements in the superelasticity and change in deformation mode of β-type TiNb24Zr2 alloys caused by aging treatments10.1007/s11661-011-0713-0 ↗
33. The effects of α″ and ω phases on the superelasticity and shape memory effect of binary Ti-Mo alloys10.1016/j.jallcom.2017.05.299 ↗
34. Effect of low temperature aging on superelastic behavior in biocompatible β TiNbSn alloy10.2320/matertrans.MER2007182 ↗
35. The crystallographic orientation of A15 V3Ga and Nb3Al precipitates in BCC matrices10.1063/1.92539 ↗
36. Shape memory effect and aging behavior of Bi-added Ti–Cr alloys for biomedical applications10.1016/j.jmbbm.2023.105800 ↗
37. Promoted mechanical properties and functionalities via Ta–tailored Ti–Au–Cr shape memory alloys towards biomedical applications10.1016/j.jmbbm.2022.105358 ↗
38. General approach to phase stability and elastic properties of β-type Ti-alloys using electronic parameters10.1016/j.scriptamat.2006.04.022 ↗
39. A β-titanium alloy with extra high strain-hardening rate: design and mechanical properties10.1016/j.scriptamat.2015.11.020 ↗
40. The role of stress induced martensite in ductile metastable beta Ti-alloys showing combined TRIP/TWIP effects10.1016/j.matpr.2015.07.336 ↗
41. Change in the deformation mode resulting from beta-omega compositional partitioning in a TiMo alloy: room versus elevated temperature10.1016/j.scriptamat.2016.11.013 ↗
42. Cryogenic tensile properties and deformation behavior of a superhigh strength metastable beta titanium alloy Ti–15Mo–2Al10.1016/j.msea.2021.141344 ↗
43. Using electron/atom ratio in titanium alloy design10.1007/BF00541408 ↗
44. Development of a novel Ti-Nb-Au superelastic alloy with exceptionally low elastic modulus10.1080/21663831.2023.2287072 ↗
45. Schaeffler-type phase diagram of Ti-based alloys10.1007/s11661-017-4218-3 ↗
46. Structural stabilities of β-Ti alloys studied using a new Mo equivalent derived from [β/(α + β)] phase-boundary slopes10.1007/s11661-015-2923-3 ↗
47. Isothermal transformation of Ti-Mo binary alloy10.2320/jinstmet1952.35.2_92 ↗
48. Effect of omega phase on mechanical properties of Ti-Mo alloys for biomedical applications
49. Effect of Sn and Zr content on superelastic properties of Ti-Mo-Sn-Zr biomedical alloys10.1016/j.msea.2017.07.097 ↗
50. Superelastic metastable Ti-Mo-Sn alloys with high elastic admissible strain for potential bio-implant applications10.1016/j.jmst.2023.01.061 ↗
51. Effect of heat treatment on shape memory effect and superelasticity in Ti–Mo–Sn alloys10.1016/j.msea.2006.05.092 ↗
52. Achievement of room temperature superelasticity in Ti-Mo-Al alloy system via manipulation of ω phase stability10.3390/ma15030861 ↗