Laser powder bed fusion of a Co–Al–W-based composite: Effects of Y2O3 nanoparticles on crack elimination, microstructure and mechanical properties
Source abstract
Abstract
In order to meet the aerospace industry's growing demand for higher-temperature and more-efficient materials, Co–Al–W-based superalloy was invented in 2006 and is expected to become the next generation of potential superalloys for aero engines. Laser powder bed fusion, as a type of additive manufacturing technology, is considered to be an advanced method for manufacturing aerospace components. However, for Co–Al–W-based superalloy, cracking commonly occurs during this process. To solve the cracking in the non-weldable Co–Al–W-based superalloy during laser powder bed fusion, 0.5 wt% Y2O3 nanoparticles were added to this alloy, forming a Co–Al–W-based composite. The results show that the cracks that formed in the Co–Al–W-based superalloy were attributed to the solidification cracking owing to the formation of the Laves phase in the inter-dendritic region. The added Y2O3 nanoparticles presented a stable chemical state without extra reactions with other elements during the laser powder bed fusion process. They played a heterogeneous nucleation role to induce columnar to equiaxed transition, where the microstructure was refined, and the cracks were eliminated. As a result, the tensile performance was dramatically improved.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · High Entropy Alloys Studies · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (52)
Show source-provided references
1. Cobalt-Base high-temperature alloys10.1126/science.1121738 ↗
2. High-temperature oxidation behaviour of a Co-based superalloy fabricated through laser powder bed fusion10.1016/j.corsci.2023.111703 ↗
3. On the atomic solute diffusional mechanisms during compressive creep deformation of a Co-Al-W-Ta single crystal superalloy10.1016/j.actamat.2019.11.035 ↗
4. Sub/micro-structural evolution of a Co–Al–W–Ta–Ti single crystal superalloy during creep at 900 °C and 420 MPa10.1016/j.msea.2019.138791 ↗
5. In situ oxidation analysis on Co-Al-W-Ti-Ta single-crystal alloy in an environmental TEM10.1016/j.corsci.2020.108725 ↗
6. Understanding the significant effect of boron content on the printability of IN738LC superalloy fabricated using laser powder bed fusion10.1016/j.optlastec.2022.108954 ↗
7. Review on fatigue of additive manufactured metallic alloys: microstructure, performance, enhancement, and assessment methods
8. Additive manufacturing of Ni-based superalloys: residual stress, mechanisms of crack formation and strategies for crack inhibition10.1016/j.nanoms.2022.08.001 ↗
9. Y2O3 nanoparticles decorated IN738LC superalloy manufactured by laser powder bed fusion: cracking inhibition, microstructures and mechanical properties10.1016/j.compositesb.2021.109555 ↗
10. Effects of TiB2 content on the processability and mechanical performance of Hastelloy-X based composites fabricated by selective laser melting10.1016/j.optlastec.2022.108441 ↗
11. Heterogeneous structures in a Ni-based superalloy with tailoring mechanical properties produced by a twin laser powder bed fusion system10.1016/j.jallcom.2022.166983 ↗
12. Effect of processing parameters on surface roughness, porosity and cracking of as-built IN738LC parts fabricated by laser powder bed fusion10.1016/j.jmatprotec.2020.116788 ↗
13. Influence of the temperature gradient and the pulling velocity on solidification cracking susceptibility during welding: a phase field study10.1016/j.matdes.2023.112424 ↗
14. Solidification cracking nature and sequence of different stainless steels10.1016/j.jmrt.2023.06.017 ↗
15. Effect of local carbide formation behavior on repair weld liquation cracking susceptibility for long-term-serviced 247LC superalloy10.1016/j.jmrt.2023.12.003 ↗
16. Thermal faceting on the ductility-dip cracking fracture surfaces of nickel-based alloys – occurrence, characterization, and implications for the cracking mechanism10.1016/j.msea.2023.145994 ↗
17. Study on the ductility-dip cracking and its formation mechanism of additive manufactured NiCrFe-7A alloy: effect of the carbon content10.1016/j.matlet.2022.131761 ↗
18. Effect of Nd:YAG pulsed laser welding process on the liquation and strain-age cracking in GTD-111 superalloy10.1016/j.jmapro.2020.01.049 ↗
19. Laser additive manufacturing of nano-TiC reinforced Ni-based nanocomposites with tailored microstructure and performance10.1016/j.compositesb.2018.12.146 ↗
20. Microstructure and mechanical properties of Inconel 625/nano-TiB2 composite fabricated by LAAM10.1016/j.matdes.2016.08.078 ↗
21. Enhancement of tensile properties due to microstructure optimization in ODS steels by zirconium addition10.1016/j.fusengdes.2017.03.170 ↗
22. Effects of Y2O3 nanoparticles on the high-temperature oxidation behavior of IN738LC manufactured by laser powder bed fusion10.1016/j.corsci.2020.108715 ↗
23. Additive manufacturing of nano-oxide decorated AlSi10Mg composites: a comparative study on Gd2O3 and Er2O3 additions10.1016/j.matchar.2022.112206 ↗
24. In-situ alloying of stainless steel 316L by co-inoculation of Ti and Mn using LPBF additive manufacturing: microstructural evolution and mechanical properties10.1016/j.msea.2022.144114 ↗
25. In situ alloying of AlSi10Mg-5 wt% Ni through laser powder bed fusion and subsequent heat treatment10.1016/j.jallcom.2022.164081 ↗
26. Effect of carbon content on the microstructure, tensile properties and cracking susceptibility of IN738 superalloy processed by laser powder bed fusion
27. Unique strength-ductility balance of AlCoCrFeNi2.1 eutectic high entropy alloy with ultra-fine duplex microstructure prepared by selective laser melting10.1016/j.jmst.2021.10.013 ↗
28. Role of porosity defects in metal 3D printing: formation mechanisms, impacts on properties and mitigation strategies10.1016/j.mattod.2022.08.014 ↗
29. Prediction of microstructure in laser powder bed fusion process10.1016/j.actamat.2016.11.018 ↗
30. Reduction of micro-cracking in nickel superalloys processed by Selective Laser Melting: a fundamental alloy design approach10.1016/j.actamat.2015.04.035 ↗
31. Influence of thermal post treatments on microstructure and oxidation behavior of EB-PBF manufactured Alloy 71810.1016/j.matchar.2019.02.016 ↗
32. Hierarchical microstructure and enhanced mechanical properties of SLM-fabricated GH5188 Co-superalloy10.1016/j.msea.2021.142276 ↗
33. Investigations of γ′, γ″ and δ precipitates in heat-treated Inconel 718 alloy fabricated by selective laser melting10.1016/j.matchar.2018.01.006 ↗
34. Origins of the mechanical property heterogeneity in a hybrid additive manufactured Hastelloy X10.1016/j.msea.2021.141716 ↗
35. Facile and cost-effective approach to additively manufacture crack-free 7075 aluminum alloy by laser powder bed fusion10.1016/j.jallcom.2022.167097 ↗
36. Predicting solidification cracking in directed energy deposition of Hastelloy X alloys based on thermal-mechanical model10.1016/j.jmapro.2023.06.033 ↗
37. A review of existing solidification crack tests and analysis of their transferability to additive manufacturing10.1016/j.jmatprotec.2023.118090 ↗
38. Effects of cooling rates on the solidification behavior, microstructural evolution and mechanical properties of Al–Zn–Mg–Cu alloys10.1016/j.jmrt.2022.12.082 ↗
39. Weldability study of 304HCu stainless steel using varestraint and “Gleeble” based hot ductility tests
40. Selective laser melting of Hastelloy X nanocomposite: effects of TiC reinforcement on crack elimination and strength improvement10.1016/j.compositesb.2020.108442 ↗
41. Cracking behaviour and its suppression mechanisms with TiB2 additions in the laser additive manufacturing of solid-solution-strengthened Ni-based alloys10.1016/j.compositesb.2023.111023 ↗
42. Evolution of Y2O3 dispersoids during laser powder bed fusion of oxide dispersion strengthened Ni-Cr-Al-Ti γ/γ’ superalloy
43. Simultaneously enhanced strength and ductility in heterogeneous grain structured Ni26Co26Fe25Cu17Ti6 high entropy alloy by introducing an appropriate amount of Y2O3 nanoparticles10.1016/j.msea.2022.144192 ↗
44. Mechanical properties and lattice misfit of γ/γ′ strengthened Co-base superalloys in the Co–W–Al–Ti quaternary system10.1016/j.intermet.2014.07.006 ↗
45. Microstructure and room temperature hardening of ultra-fine-grained oxide-dispersion strengthened copper prepared by cryomilling10.1016/j.msea.2004.05.049 ↗
46. A novel method to 3D-print fine-grained AlSi10Mg alloy with isotropic properties via inoculation with LaB6 nanoparticles
47. Cracking inhibition behavior and the strengthening effect of TiC particles on the CM247LC superalloy prepared by selective laser melting10.1016/j.msea.2022.144119 ↗
48. High wear resistance and strength of Hastelloy X reinforced with TiC fabricated by laser powder bed fusion additive manufacturing10.1016/j.apsusc.2023.159004 ↗
49. Microstructure and grain growth direction of SRR99 single-crystal superalloy by selective laser melting10.1016/j.jallcom.2019.151740 ↗
50. Laser powder bed fusion of nano-titania modified 2219 aluminium alloy with superior mechanical properties at both room and elevated temperatures: the significant impact of solute
51. Fatigue strength of additive manufactured Mar-M-509 superalloy10.1016/j.msea.2022.142913 ↗
52. Effect of standard heat treatment on the microstructure and mechanical properties of selective laser melting manufactured Inconel 718 superalloy10.1016/j.msea.2015.06.021 ↗