Thermal shock damage of the self-reinforced α-SiAlON ceramic using barium aluminosilicate glass ceramic as the sintering additive
Source abstract
Abstract
Abstract Dy–α-SiAlON (Dy 1/3 Si 10 Al 2 ON 15 ) using 5 wt.% BaAl 2 Si 2 O 8 (BAS) glass ceramic as an additive was synthesized by hot-pressing. The thermal shock resistance of the material was investigated. The results indicated that this material has very good thermal shock resistance. The critical temperature difference could reach 1100 °C. The gradual growth of the pre-existent cracks and the significant interfacial debonding between the SiAlON grains and the intergranular BAS phase were the reasons for the flexure strength losses at the thermal shock temperature difference below and above 1100 °C, respectively. The slight oxidation introduced by the heating process marginally benefited the residual strength by surface damage healing.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Nuclear materials and radiation effects · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (29)
Show source-provided references
1. Chen · Nature · 1997 · 389 · 70110.1038/39542 ↗
2. Kim · J. Am. Ceram. Soc. · 2000 · 83 · 181910.1111/j.1151-2916.2000.tb01472.x ↗
3. Kurama · J. Eur. Ceram. Soc. · 2002 · 22 · 10910.1016/S0955-2219(01)00237-0 ↗
4. Jones · J. Am. Ceram. Soc. · 2004 · 87 · 71010.1111/j.1551-2916.2004.00710.x ↗
5. Peng · J. Mater. Res. · 2004 · 19 · 240210.1557/JMR.2004.0291 ↗
6. Zenotchkine · J. Am. Ceram. Soc. · 2004 · 87 · 104010.1111/j.1551-2916.2004.01040.x ↗
7. Hong · J. Mater. Res. · 2002 · 17 · 113610.1557/JMR.2002.0168 ↗
8. Yoshiki · J. Am. Ceram. Soc. · 1951 · 34 · 28310.1111/j.1151-2916.1951.tb09131.x ↗
9. Drummond · Ceram. Eng. Sci. Proc. · 1989 · 10 · 148510.1002/9780470310588.ch64 ↗
10. Ye · J. Mater. Res. · 2003 · 18 · 244610.1557/JMR.2003.0340 ↗
11. Ye · Mater. Sci. Eng. A · 2008 · 488 · 35210.1016/j.msea.2007.11.036 ↗
12. Hasselman · J. Am. Ceram. Soc. · 1963 · 46 · 53510.1111/j.1151-2916.1963.tb14605.x ↗
13. Hasselman · J. Am. Ceram. Soc. · 1969 · 52 · 60010.1111/j.1151-2916.1969.tb15848.x ↗
14. She · J. Am. Ceram. Soc. · 2003 · 86 · 73810.1111/j.1151-2916.2003.tb03367.x ↗
15. F. Ye, Postdoctoral Report (in Chinese), Northwestern Polytechnical University, China, 1997.
16. Becher · J. Am. Ceram. Soc. · 1998 · 81 · 282110.1111/j.1151-2916.1998.tb02702.x ↗
17. Zenotchkine · J. Am. Ceram. Soc. · 2001 · 84 · 88410.1111/j.1151-2916.2001.tb00760.x ↗
18. Ye · Int. J. Appl. Ceram. Technol. · 2010
19. Becher · Am. Ceram. Soc. Bull. · 1980 · 59 · 542
20. J.M. Zhou, Dissertation for the Master Degree in Engineering (in Chinese), Harbin Institute of Technology, China, 2007.
21. Ye · J. Alloy Compd. · 2010 · 493 · 27210.1016/j.jallcom.2009.12.078 ↗
22. Collin · Acta Mater. · 2000 · 48 · 165510.1016/S1359-6454(00)00011-2 ↗
23. Kim · J. Mater. Sci. · 1995 · 30 · 404310.1007/BF00360707 ↗
24. Swain · J. Am. Ceram. Soc. · 1989 · 73 · 62110.1111/j.1151-2916.1990.tb06562.x ↗
25. Wereszczak · J. Am. Ceram. Soc. · 1993 · 76 · 291910.1111/j.1151-2916.1993.tb04039.x ↗
26. Pan · J. Am. Ceram. Soc. · 2005 · 88 · 191410.1111/j.1551-2916.2005.00425.x ↗
27. Collin · J. Eur. Ceram. Soc. · 2002 · 22 · 43510.1016/S0955-2219(01)00319-3 ↗
28. Mecholskyjun · J. Mater. Sci · 1976 · 11 · 131010.1007/BF00545152 ↗
29. Swab · J. Am. Ceram. Soc. · 1998 · 81 · 226110.1111/j.1151-2916.1998.tb02620.x ↗