Slow crack growth behavior of 3Y-TZP in cryogenic environment using dynamic fatigue and indentation technique
Source abstract
Abstract
Abstract The dynamic fatigue of 3 mol% Y 2 O 3 stabilized tetragonal zirconia ceramic (3Y-TZP) was assessed at 293 K and 77 K by testing the same batch of specimens in four-point flexure at various stress rates. The crack propagation velocities were also measured using Vickers indentation specimens under dynamic-loading conditions in ambient and cryogenic environment. The slow crack growth (SCG) parameter n at 77 K was larger than that at 293 K. Also, the crack propagation velocity under cryogenic circumstance is much slower than that under ambient circumstance. The experimental results suggest that the 3Y-TZP exhibits a lesser degree of SCG behavior in cryogenic environment. It should be ascribed to two reasons. The negligible effect of stress corrosion and crack tip shielding mechanism induced by temperature. The high SCG resistance in cryogenic environment makes the 3Y-TZP a promising candidate material for long-term service in cryogenic structural applications.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Metal and Thin Film Mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (23)
Show source-provided references
1. ASTM C1368, West Conshohocken, PA, 2010
2. Yin · Acta Metall. Mater. · 1995 · 43 · 37110.1016/0956-7151(95)90293-7 ↗
3. Chevalier · J. Am. Ceram. Soc. · 1999 · 82 · 312910.1111/j.1151-2916.1999.tb02213.x ↗
4. Aza · J. Am. Ceram. Soc. · 2003 · 86 · 11510.1111/j.1151-2916.2003.tb03287.x ↗
5. Alcalá · J. Am. Ceram. Soc. · 1997 · 80 · 275910.1111/j.1151-2916.1997.tb03192.x ↗
6. Gremillard · Acta. Mater. · 2000 · 48 · 464710.1016/S1359-6454(00)00252-4 ↗
7. Marro · J. Eur. Ceram. Soc. · 2012 · 32 · 154110.1016/j.jeurceramsoc.2012.01.013 ↗
8. Xue · J. Am. Ceram. Soc. · 2011 · 94 · 277510.1111/j.1551-2916.2011.04711.x ↗
9. Xue · Scr.. Mater. · 2012 · 67 · 96310.1016/j.scriptamat.2012.08.030 ↗
10. Lawn · 1993
11. Chantikul · J. Am. Ceram. Soc. · 1981 · 64 · 53910.1111/j.1151-2916.1981.tb10321.x ↗
12. Lawn · J. Am. Ceram. Soc. · 1980 · 63 · 57410.1111/j.1151-2916.1980.tb10768.x ↗
13. Newman · Eng. Fract. Mech. · 1981 · 15 · 18510.1016/0013-7944(81)90116-8 ↗
14. Hannink · J. Am. Ceram. Soc. · 2000 · 83 · 46110.1111/j.1151-2916.2000.tb01221.x ↗
15. Shetty · J. Am. Ceram. Soc. · 1984 · 67 · 20110.1111/j.1151-2916.1984.tb19663.x ↗
16. Scott · Fatigue Fract. Eng. Mater. Struct. · 1981 · 4 · 29110.1111/j.1460-2695.1981.tb01127.x ↗
17. Lawn · J. Mater. Sci. · 1981 · 16 · 284610.1007/BF02402849 ↗
18. Chevalier · Compos. Part A: Appl. Sci. Manuf. · 1999 · 30 · 52510.1016/S1359-835X(98)00145-6 ↗
19. Mitov · Dent. Mater. · 2011 · 27 · 68410.1016/j.dental.2011.03.010 ↗
20. Teixeira · J. Mater. Sci.: Mater. Med. · 2007 · 18 · 1219
21. Wang · J. Mater. Sci. · 1989 · 24 · 342110.1007/BF02385721 ↗
22. Kruzic · J. Am. Ceram. Soc. · 2005 · 88 · 223610.1111/j.1551-2916.2005.00434.x ↗
23. Ramalingam · J. Am. Ceram. Soc. · 2011 · 94 · 57610.1111/j.1551-2916.2010.04086.x ↗