journal article·2022-01

Macrostructures and mechanical properties in laser melting deposited titanium alloy plate at different thickness positions

Kai Wang, Binchao Liu, Qiuyi Wang, Rui Bao

Publisher page

Abstract

Abstract Mechanical properties, including tensile properties and fatigue crack growth behaviors, and their relationships with macrostructures at different thickness positions in plates of laser melting deposited Ti–5Al–5Mo–5V–1Cr–1Fe, are experimentally investigated in this paper. It is observed that there display obvious differences in macrostructure features between overlap zones and non-overlap zones along thickness direction, which leads to anisotropies and heterogeneities of tensile properties including yield stress, tensile strength and total elongation. In fatigue crack growth tests with thin compact tension specimens at different thickness positions, crack paths are deviated from mode I with varying angles and fatigue crack growth rates display obvious fluctuations, which are mainly caused by the macrostructure features in overlap zone. In the end, evaluation methods are discussed for fatigue crack growth behaviors from the perspective of mechanics-materials interactive mechanisms, which helps strive for the future processing-material-structure-property-evaluation paradigm for additively manufactured metal structures.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · Welding Techniques and Residual Stresses

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (43)

Show source-provided references
1. Energy and emissions saving potential of additive manufacturing: the case of lightweight aircraft components10.1016/j.jclepro.2015.04.109 ↗
2. Understanding the effect of laser scan strategy on residual stress in selective laser melting through thermo-mechanical simulation
3. A strategy to improve the work-hardening behavior of Ti-6Al-4V parts produced by additive manufacturing10.1080/21663831.2016.1245681 ↗
4. An experimental study of wire EDM on Ti-6Al-4V alloy10.1016/j.mspro.2014.07.517 ↗
5. Inagaki · 2014 · 22
6. On the characteristics of titanium alloys for the aircraft applications10.1016/j.matpr.2017.07.249 ↗
7. Research progress in laser solid forming of high-performance metallic components at the state key laboratory of solidification processing of China10.1089/3dp.2014.0016 ↗
8. Tensile and fatigue crack growth behavior of commercially pure titanium produced by laser powder bed fusion additive manufacturing
9. Additive manufacturing of strong and ductile Ti-6Al-4V by selective laser melting via in situ martensite decomposition10.1016/j.actamat.2014.11.028 ↗
10. Effect of build geometry on the β-grain structure and texture in additive manufacture of Ti-6Al-4V by selective electron beam melting10.1016/j.matchar.2013.07.012 ↗
11. Graded microstructure and mechanical properties of additive manufactured Ti-6Al-4V via electron beam melting10.1016/j.actamat.2015.06.036 ↗
12. An overview of Direct Laser Deposition for additive manufacturing; Part II: mechanical behavior, process parameter optimization and control
13. Multi-scale microstructural development and mechanical properties of a selectively laser melted beta titanium alloy
14. Microstructure and tensile properties of laser melting deposited Ti-5Al-5Mo-5V-1Cr-1Fe near β titanium alloy10.1016/j.msea.2013.08.032 ↗
15. Comparison on mechanical anisotropies of selective laser melted Ti-6Al-4V alloy and 304 stainless steel10.1016/j.msea.2017.04.031 ↗
16. Microstructure and tensile properties of selectively laser-melted and of HIPed laser-melted Ti-6Al-4V10.1016/j.msea.2013.04.099 ↗
17. Interrupted fatigue testing with periodic tomography to monitor porosity defects in wire + arc additive manufactured Ti-6Al-4V
18. Assessment of the effect of isolated porosity defects on the fatigue performance of additive manufactured titanium alloy
19. The influence of the microtexture and orientation of columnar grains on the fatigue crack growth of directed energy deposited Ti-6.5Al-2Zr-Mo-V alloys
20. Characterization of fatigue crack growth behavior in LENS fabricated Ti-6Al-4V using high-energy synchrotron x-ray microtomography
21. Effect of primary α phase on the fatigue crack path of laser melting deposited Ti-5Al-5Mo-5V-1Cr-1Fe near β titanium alloy10.1016/j.ijfatigue.2018.06.041 ↗
22. Material-structure-performance integrated laser-metal additive manufacturing10.1126/science.abg1487 ↗
23. Fatigue in additive manufactured aircraft: the long way to make it fly
24. Texture and microstructure characterization in laser additive manufactured Ti-6Al-2Zr-2Sn-3Mo-1.5 Cr-2Nb titanium alloy10.1016/j.matdes.2015.09.053 ↗
25. Characterization of microstructure and mechanical properties of laser melting deposited Ti-6.5Al-3.5Mo-1.5Zr-0.3Si titanium alloy10.1016/j.matdes.2013.11.044 ↗
26. Effects of heat accumulation on microstructure and mechanical properties of Ti6Al4V alloy deposited by wire arc additive manufacturing
27. Additive manufacturing of fatigue resistant materials: challenges and opportunities10.1016/j.ijfatigue.2017.01.001 ↗
28. Progress towards metal additive manufacturing standardization to support qualification and certification
29. Mochache · 2021
30. Hrabe · 2019
31. Aviation Administration · 2016
32. Liu · 2018
33. Microstructural characterization of laser melting deposited Ti-5Al-5Mo-5V-1Cr-1Fe near β titanium alloy10.1016/j.jallcom.2013.03.243 ↗
34. Development of a pre-heat treatment for obtaining discontinuous grain boundary α in laser melting deposited Ti–5Al–5Mo–5V–1Cr–1Fe alloy
35. 2016
36. Plastic anisotropy of laser melting deposited Ti-5Al-5Mo-5V-1Cr-1Fe titanium alloy10.1016/j.msea.2019.01.031 ↗
37. 2015
38. Suresh · 1998
39. The effects of α/β phase interfaces on fatigue crack deflections in additively manufactured titanium alloy: a peridynamic study10.1016/j.ijfatigue.2020.105622 ↗
40. Fatigue crack growth behaviour and life prediction for 2324-T39 and 7050-T7451 aluminum alloys under truncated load spectra10.1016/j.ijfatigue.2009.12.010 ↗
41. Assessment of mixed mode loading on macroscopic fatigue crack paths in thick section Al-Cu-Li alloy plate10.1016/j.matdes.2015.12.116 ↗
42. Anisotropic fatigue crack growth in high-strength aluminium alloys
43. A specimen to evaluate susceptibility of aluminum alloys to L-S crack deviation