Abstract Ferrite-bainite microstructures and impact toughness of the X65 low-carbon microalloyed steel were investigated after helical rolling at 1000, 920, 850, and 810 °C followed by continuous cooling in air. After helical rolling at 1000 °C, granular bainite with large areas of the massive-shape martensite-austenite constituent (d = 1.5 μm) and a high fraction of twinned martensite (d > 2.0 μm) were observed in the steel. This caused a decrease in impact energy at low test temperatures (for example, 70 J at –70°С). Lowering the helical rolling temperature contributed to a reduction of dimensions of both ferrite-bainite and martensite-austenite constituent areas, as well as the replacement of the latter by a slender type one and an improvement in fracture toughness at the low temperatures. The highest impact energy level (210 J at –70 °C) was achieved after helical rolling at 850 °C due to the formation of a homogeneous microstructure, which included dispersed ferrite grains, granular bainite and small fractions of the slender type martensite-austenite constituent (d = 0.1–0.7 μm). In this case, areas of twinned martensite were absent.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Microstructure and Mechanical Properties of Steels · Metal Alloys Wear and Properties · Metallurgy and Material Forming

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (43)

Show source-provided references
1. Cold brittleness and fracture of metals with various crystal lattices: dislocation mechanisms10.1134/S1063784216070070 ↗
2. Significant influence of carbon and niobium on the precipitation behavior and microstructural evolution and their consequent impact on mechanical properties in microalloyed steels10.1016/j.msea.2016.11.102 ↗
3. Microstructural characteristics and impact fracture behaviors of low-carbon vanadium-microalloyed steel with different nitrogen contents10.1016/j.msea.2019.138501 ↗
4. Phase transformation, microstructure, and mechanical properties of X100 pipeline steels based on TMCP and HTP concepts10.1007/s10853-016-0459-6 ↗
5. Low-temperature toughening mechanism in thermomechanically processed high-strength low-alloy steels10.1007/s11661-010-0448-3 ↗
6. Effect of rolling process on impact toughness in high strength low carbon bainitic steel
7. Thermomechanical processing of low carbon Nb-Ti stabilized microalloyed steel: microstructure and mechanical properties10.1016/j.msea.2015.08.072 ↗
8. The effects of thermo-mechanical control process on microstructures and mechanical properties of a commercial pipeline steel10.1016/S0921-5093(01)01904-9 ↗
9. Effect of microstructural constituents on strength-toughness combination in a low carbon bainitic steel10.1016/j.msea.2014.05.084 ↗
10. Correlation of microstructure and mechanical properties of thermomechanically processed low-carbon steels containing boron and copper10.1007/s11661-009-0070-4 ↗
11. Microstructure and properties of 09MnNiDR steel for -70 °C ultra low temperature environment
12. Processing-structure-mechanical property relationship in Ti-Nb microalloyed steel: continuous cooling versus interrupted cooling10.1016/j.msea.2016.06.061 ↗
13. Effect of cooling rate and composition on microstructure and mechanical properties of ultrahigh-strength steels10.1007/s42243-019-00276-0 ↗
14. Effects of continuous cooling rate on morphology of granular bainite in pipeline steels10.1007/s42243-019-00346-3 ↗
15. Microstructural characteristics with various cooling paths and the mechanism of embrittlement and toughening in low-carbon high performance bridge steel10.1016/j.msea.2012.08.091 ↗
16. Effects of microstructure on CVN impact toughness in thermomechanically processed high strength microalloyed steel10.1007/s11661-016-3893-9 ↗
17. Quantitative analysis of microstructural and mechanical behavior for Fe-0.1C-(V, Nb) steels as a function of the final rolling temperature10.1016/j.msea.2007.11.145 ↗
18. Influence of prior austenite grain size on martensite-austenite constituent and toughness in the heat affected zone of 700MPa high strength linepipe steel10.1016/j.msea.2014.07.100 ↗
19. Influence of Martensite-Austenite constituents formed at different intercritical temperatures on toughness10.1016/j.matdes.2014.10.028 ↗
20. Mechanical and metallurgical investigation of martensite-austenite constituents in simulated welding conditions10.1016/j.jmatprotec.2004.04.021 ↗
21. Influence of martensite-austenite (MA) on impact toughness of X80 line pipe steels10.1016/j.msea.2016.03.095 ↗
22. Microstructure and mechanical properties of intercritical heat-affected zone of X80 pipeline steel in simulated in-service welding10.1007/s40195-015-0272-2 ↗
23. Elemental distribution in the martensite–austenite constituent in intercritically reheated coarse-grained heat-affected zone of a high-strength pipeline steel10.1016/j.scriptamat.2017.06.017 ↗
24. Metallographic investigation of M‐A constituent Deterioration and improvement of HAZ toughness in 780 and 980 MPa class HSLA steels welded with high heat inputs (2nd report)10.1080/09507119409548716 ↗
25. Innovative equipment for producing cost-effective hollow billets for mechanical-engineering parts of small diameter10.1007/s11015-017-0480-2 ↗
26. Putting into practice innovative potential in the universal radial-shear rolling process
27. Deformation action of screw rolling on a cast wheel billet10.1007/s11015-013-9653-9 ↗
28. Modification of the structure of low-carbon pipe steel by helical rolling, and the increase in its strength and cold resistance10.1134/S0031918X18010076 ↗
29. The role of nanoscale strain-induced defects in the sharp increase of low-temperature toughness in low-carbon and low-alloy steels10.1016/j.msea.2019.138491 ↗
30. Characterisation and quantification of complex bainitic microstructures in high and ultra-high strength linepipe steels10.4028/www.scientific.net/MSF.500-501.387 ↗
31. Transmission electron microscopy of martensite/austenite islands in pipeline steel X7010.1016/j.msea.2006.02.118 ↗
32. Substructures of martensite in Fe-1C-17Cr stainless steel10.1016/j.scriptamat.2010.01.022 ↗
33. Morphological aspects of martensite-austenite constituents in intercritical and coarse grain heat affected zones of structural steels10.1016/S0921-5093(04)00859-7 ↗
34. Materials perspective: classification and quantification of microstructures in steels10.1179/026708304225010325 ↗
35. Effect of applied thermal cycle conditions on chemistry and volume fraction of M-A constituent formed in a low alloy steel10.2355/tetsutohagane1955.84.4_297 ↗
36. Structure-property relationships in intercritical heat affected zone of low-carbon microalloyed steels10.1179/mst.1987.3.8.649 ↗
37. Classification of martensite-austenite constituents according to its internal morphology in high-strength low alloy steel10.1016/j.matlet.2020.128422 ↗
38. A study of the influence of thermomechanical controlled processing on the microstructure of bainite in high strength plate steel10.1007/s11661-014-2444-5 ↗
39. Effect of reheat temperature on continuous cooling bainite transformation behavior in low carbon microalloyed steel10.1007/s10853-013-7251-7 ↗
40. Enhancing the weldability of C-Mn pressure vessel steels — a tale of two elements
41. Transformation twins in the weld HAZ of a low-carbon high-strength microalloyed steel10.1016/j.msea.2006.07.055 ↗
42. Impact toughness of subzones in the intercritical heat-affected zone of low-carbon bainitic steel
43. Variations in DBTT and CTOD within weld heat-affected zone of API X65 pipeline steel10.1016/j.msea.2012.03.062 ↗