Abstract

The fitness of ageing cast iron pipe is a problem for both clean water and wastewater networks. Whilst considerable effort has been put into understanding the condition of cast iron mains that carry potable water, wastewater systems have received less attention. Compared with clean water mains, wastewater trunk sewers typically have thinner walls, are often of lesser casting quality, and typically are exposed to a harsher and more complex internal and external environment. It has been established that corrosion is a leading cause of deterioration in cast iron mains. Research has shown that when predicting residual load capacity in clean water main, a loss-of-section approach is not applicable when dealing with corrosion pitting, which is more discrete and notch-like. This research examines the use of both loss-of-section and fracture mechanics models to provide a failure envelope for a ring from a pipe under combined vertical loading and internal pressure. Internal corrosion, defect size, and morphology of this corrosion have a significant effect on the residual strength of the pipe. The failure envelope predicted is rather different to that previously reported for clean water mains, which is not unexpected given the differences in component geometry and operational conditions.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Concrete Corrosion and Durability · Structural Integrity and Reliability Analysis · Corrosion Behavior and Inhibition

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (23)

Show source-provided references
1. Thames water · 2017
2. London Olympic Park underpass leads to better understanding of cast iron10.1680/cien.12.00043 ↗
3. On the residual strength of aging cast iron trunk mains: physically-based models for asset failure10.1016/j.msea.2016.03.029 ↗
4. On the condition assessment of cast iron trunk main: the effect of microstructure and in-service graphitisation on mechanical properties in flexure10.1016/j.msea.2013.03.061 ↗
5. The fracture and fatigue properties of cast irons used for trunk mains in the water industry10.1016/j.msea.2010.05.071 ↗
6. Logan · 2014
7. Re-assessment of resistance of cast iron pipes subjected to vertical loads and internal pressure10.1016/j.engstruct.2012.06.019 ↗
8. Consideration of uncertainties to estimate structural capacity of ageing cast iron water mains- a Possibilistic approach10.1139/l06-042 ↗
9. Rajani · 2001 · 1259
10. Schlick · 1940
11. Rajani · 2000
12. Belmonte · Fatigue Fract. Eng. Mater. Struct. · 2008 · 31 · 37010.1111/j.1460-2695.2008.01233.x ↗
13. Estimating time to failure of ageing cast iron water mains under uncertainties
14. S A Adegbite, A Fahimi, T Evans, J Farrow, D A Jesson, M J Mulheron, and P A Smith: Trunk mains failures: the effect of corrosion on residual pipe strength, 4th International Conference on Integrity, Reliability and Failure, 2013-06-23 - 2013-06-27, (Funchal, Portugal).
15. Marshall · 2001
16. Talbot · 1926
17. Stress-intensity factors for internal and external surface cracks in cylindrical vessels
18. An empirical stress-intensity factor equation for the surface crack
19. Risk based service life prediction of underground cast iron pipes subjected to corrosion10.1016/j.ress.2013.05.013 ↗
20. Ashby · 2005
21. Finite element evaluation of the remaining mechanical strength of deteriorated cast iron pipes10.1115/1.1631027 ↗
22. Walton · 1958
23. Young · 1984