journal article·2018-05

Role of Sc on the glass forming ability and mechanical properties of Al-Y-Ni-Sc bulk metallic glass produced with different cooling rates

Chih-Yuan Chen, Wei-Sheng Hsu, Shih-Fan Chen

Publisher page

Abstract

Abstract In the present study, the role of Sc in the glass forming ability (GFA) and mechanical properties of (Al87Y8Ni5)99Sc1 alloy ribbon produced by single roller melt-spinning with various rotation speeds has been investigated in an attempt to understand the influence of cooling rate in the transition element of the Al-TM-RE (TM: transition metal, RE: rare earth metal) alloy system. The crystallinities of the two alloy ribbons formed at various cooling rates were evaluated by X-ray diffraction (XRD) in order to examine whether the amorphous structure, α-Al particles and precipitation compounds could be formed at any cooling rate. Results revealed α-Al in the Al87Y8Ni5 alloy, but both phases (i.e., α-Al and Al3Sc) were indexed for (Al87Y8Ni5)99Sc1 alloy at a low cooling rate (1000–2000 rpm). Moreover, larger full width at half maximum (FWHM) of characteristic peaks (corresponding to α-Al) were observed for both alloy ribbons, indicating a lower degree of structural relaxation as the cooling rate was increased. Therefore, better short-range ordering of the atomic configuration can be achieved when the alloy ribbons are synthesized at a lower cooling rate, which allows sufficient time for the atoms to reach their local ordered equilibrium positions. On the other hand, the maximum hardness was obtained for both non-scandium and scandium-doped alloys produced at the intermediate cooling rate (2000 rpm) due to the random and homogeneous distribution of numerous tiny precipitates in the amorphous matrix. In addition, compared to Al87Y8Ni5 alloy ribbon, the occurrence of glass transition temperature (Tg), higher crystallization temperature (Tx, Tp1, Tp2), and smaller amount of crystallization fraction in the (Al87Y8Ni5)99Sc1 during continuous heating proves the advantageous effects, namely higher glass forming ability and better thermal stability, of the scandium addition. The mechanism underlying this advantage should be associated with the enhancement of the viscosity of the alloy melt, which results from the increased packing density of the alloy melt when scandium is added. The shear-banded structures that characteristically appear around the indents were observed to be completely absent around indents made at a low cooling rate, revealing that inhomogeneous deformation is not mediated by shear bands below a certain cooling rate. In addition, observation of the fracture surfaces revealed that the fracture surfaces of both alloy ribbons produced at high and low cooling rates transformed from vein patterns to isotropic dimple structures, revealing a change in fracture mode from brittle to ductile as the cooling rate decreased.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Metallic Glasses and Amorphous Alloys · Cultural Heritage Materials Analysis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (51)

Show source-provided references
1. On nanovoids formation in shear bands of an amorphous Al-based alloy10.1016/j.mechmat.2017.07.007 ↗
2. Structure and dynamics of shear bands in amorphous–crystalline nanolaminates10.1016/j.scriptamat.2015.07.038 ↗
3. Ductile fracture in notched bulk metallic glasses10.1016/j.actamat.2017.06.048 ↗
4. Cooling rate effect on Young's modulus and hardness of a Zr-based metallic glass10.1016/j.jallcom.2010.12.095 ↗
5. Effect of Ga substitution on the crystallization behavior and glass forming ability of Zr-Al-Cu-Ni alloys10.1016/j.msea.2009.10.020 ↗
6. Glass forming ability of Al–Ni–La alloys with Si addition10.1016/j.jallcom.2015.08.037 ↗
7. Amorphous, nanoquasicrystalline and nanocrystalline alloys in Al-based systems10.1016/S0079-6425(98)00005-X ↗
8. Investigation of glass formability in Al-based multinary alloys10.1016/S1359-6462(00)00540-6 ↗
9. Insight on the glass-forming ability of Al–Y–Ni–Ce bulk metallic glass10.1016/j.jallcom.2015.02.217 ↗
10. Role of atomic size on glass formability and thermal stability of Al-based amorphous alloys10.2320/matertrans1989.41.1406 ↗
11. Nano-crystal development and thermal stability of amorphous Al–Ni–Y–Ce alloy10.1016/j.jnoncrysol.2013.04.059 ↗
12. High entropy state of orientationally-disordered clusters in Zr-based bulk metallic glass10.1016/S1002-0071(12)60012-4 ↗
13. New amorphous alloys in Al-Si-Fe-Ni and Al-Si-Fe-Co systems and their crystallization behaviour10.2320/matertrans1989.38.595 ↗
14. The effect of Fe on the crystallization behavior of Al–Mm–Ni–Fe amorphous alloys10.1023/A:1017567924939 ↗
15. Effect of Si and Co on the crystallization of Al–Ni–RE amorphous alloys10.1016/j.jallcom.2006.11.056 ↗
16. Effects of B upon glass forming ability of Al87Y8Ni5 amorphous alloy10.1016/j.jallcom.2013.02.135 ↗
17. Thermal stability, crystallization kinetics and mechanical properties of Al81.8Ni9.2Co4.8Y3.1Zr1.1 amorphous alloy consolidated to a fully dense nanocrystalline matrix with some remaining amorphous phase10.1016/j.jallcom.2014.03.075 ↗
18. Nanocrystalline or amorphous matrix Al60Fe15Ti15(Co/Mg/Zr)5–5%B composites produced by consolidation of mechanically alloyed powders – lightweight materials with high hardness10.1016/j.intermet.2012.04.011 ↗
19. A model of the ductile–brittle transition of partially crystallized amorphous Al–Ni–Y alloys10.1016/S1359-6454(99)00088-9 ↗
20. Formation of bulk metallic glass in situ nanocomposite in (Cu50Zr43Al7)99Si1 alloy10.1016/j.msea.2012.05.066 ↗
21. Cooling rate-dependent yield behavior of metallic glass wires10.1016/j.msea.2016.12.022 ↗
22. Processing effects on fracture toughness of metallic glasses10.1016/j.scriptamat.2016.11.011 ↗
23. Influence of the preparation cooling rate on crystallization kinetics of Fe74Mo6P13C7 amorphous alloys10.1016/j.jnoncrysol.2017.09.012 ↗
24. Effect of cooling rate on microstructure and mechanical properties of rapidly solidified Al-based bulk alloys10.1016/j.jallcom.2010.03.211 ↗
25. The effect of cooling rate on the plasticity of amorphous metal10.1016/j.jallcom.2015.06.212 ↗
26. Effect of quenching rate on the microstructure and mechanical behavior of Ce75Al21Ga4 glassy alloy10.1016/j.matchar.2017.09.037 ↗
27. The Al-rich region in the Y–Ni–Al system: microstructures and phase equilibria10.1016/S0966-9795(99)00100-4 ↗
28. Microstructure of Al3Sc with ternary transition-metal additions10.1016/S0921-5093(01)01608-2 ↗
29. The effect of scandium on the microstructure, mechanical properties and weldability of a cast Al–Mg alloy10.1016/S1359-6454(02)00259-8 ↗
30. The solidification behavior of dilute aluminium–scandium alloys10.1016/S1359-6454(98)00257-2 ↗
31. Non-isothermal crystallization kinetics and mechanical properties of Al86Ni6Y4.5Co2La1.5 metallic glass powder10.1016/j.jallcom.2012.03.083 ↗
32. Thermal stability and hardness of Mg–Cu–Au–Y amorphous alloys10.1016/j.jallcom.2006.08.110 ↗
33. Partially or fully devitrified alloys for mechanical properties10.1016/S0921-5093(00)01449-0 ↗
34. Microstructure and mechanical properties of a partially crystallized La-based bulk metallic glass10.1080/0141861861031000104163 ↗
35. Effect of thermal annealing on the local structure in ZrCuAl bulk metallic glass10.1016/j.jallcom.2010.02.072 ↗
36. Defect generation and analysis in mechanically alloyed stoichiometric Fe–Ni alloys10.1016/j.jallcom.2015.02.038 ↗
37. Stability of medium range order in Al-based metallic glass compacted by severe plastic deformation10.1016/j.jallcom.2013.02.010 ↗
38. Quenched-in quasicrystal medium-range order and pair distribution function study on Zr55Cu35Al10 bulk metallic glass10.1016/j.intermet.2006.01.005 ↗
39. Discrepancy of structural stability against temperature between metallic liquids and their glasses10.1016/j.jnoncrysol.2010.08.033 ↗
40. Supercooling investigation and critical cooling rate for glass formation in Pd–Cu–Ni–P alloy10.1016/S1359-6454(99)00030-0 ↗
41. Superplastic nanoforming of Pd-based amorphous alloy10.1016/S1359-6462(01)00837-5 ↗
42. Effect of minor alloying additions on glass formation in bulk metallic glasses10.1016/j.intermet.2004.07.034 ↗
43. In-situ precipitated nanocrystal beneficial to enhanced plasticity of Cu-Zr based bulk metallic glasses10.1002/adem.200800123 ↗
44. High-strength Zr-based bulk amorphous alloys containing nanocrystalline and nanoquasicrystalline particles10.1016/S1468-6996(00)00009-7 ↗
45. Atomic packing in multicomponent aluminum-based metallic glasses10.1016/j.actamat.2008.08.049 ↗
46. Iron-based bulk metallic glasses10.1179/1743280412Y.0000000007 ↗
47. Mechanical behavior of amorphous alloys10.1016/j.actamat.2007.01.052 ↗
48. The fracture topography of metallic glasses10.1007/BF00761791 ↗
49. Evolution of shear bands into cracks in metallic glasses10.1016/j.jallcom.2014.09.205 ↗
50. Fracture of brittle metallic glasses: brittleness or plasticity10.1103/PhysRevLett.94.125510 ↗
51. The mechanism of fracture in glassy materials capable of some inelastic deformation10.1016/0025-5416(76)90198-1 ↗