Effects of artificial defect on the material residual strength of SiC ceramics after thermal-shock
Source abstract
Abstract
Abstract Thermal shock behaviors of SiC ceramic with artificial defects were studied. Artificial surface cracks were simulated by Vickers and Knoop indentations, and artificial inner cracks were obtained using novel method of introducing plastic fibers. The residual flexural strength and microstructure were analyzed. The flexural strength of artificial defect free SiC ceramic maintains minimum 87% of the original strength after thermal shock ΔT no more than 400 ℃, and the residual strength of those with artificial crack, no matter surface type or inner type, can still be improved by the joint effect of thermal treatment, thermal shock and the stress relaxation by artificial crack if ΔT no more than 400 ℃. It is believed that inner and surface artificial defects ease the crack propagation during the thermal shock process.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (24)
Show source-provided references
1. Analysis of the effective thermoelastic properties and stress fields in silicon nitride based on EBSD data10.1016/j.jeurceramsoc.2015.10.046 ↗
2. characterisation, significance and detection of manufacturing defects in reaction sintered silicon carbide armour materials10.1016/j.ceramint.2015.06.083 ↗
3. H. Knoch, D. Steinmann, Ceramic Bearings and Wearing Parts of Silicon-Nitride, Silicon-Carbide and Boron-Carbide. Metall, 1989. 43(3), pp. 250-254.
4. Effect of hexagonal-BN additions on the sliding-wear resistance of fine-grained α-SiC densified with Y3Al5O12 liquid phase by spark-plasma sintering10.1016/j.jeurceramsoc.2013.09.016 ↗
5. M. Ichinose, et al., Preliminary design of high temperature lithium-lead blanket with SiC cooling panel, in Proceedings of the 23rd IEEE/NPSS Symposium on Fusion Engineering. San Diego, California, USA, 2009.10.1109/FUSION.2009.5226508 ↗
6. Re-evaluation of SiC permeation coefficients at high temperatures10.1016/j.fusengdes.2015.12.041 ↗
7. Effect of Ar or N2 sintering atmosphere on the high-temperature oxidation behaviour of pressureless liquid-phase-sintered α-SiC in air10.1016/j.jeurceramsoc.2009.08.004 ↗
8. Numerical model for the cracking behavior of heterogeneous brittle solids subjected to thermal shock10.1016/j.ijsolstr.2015.10.012 ↗
9. Effect of thermal shock and rapid unloading on mechanical rock properties
10. Influence of thermal shock damage on the flexure strength of alumina ceramic at different temperatures10.1016/j.matlet.2016.03.026 ↗
11. The thermal shock resistance of Y2O3 ceramics10.1016/j.ceramint.2016.03.140 ↗
12. Transient thermal shock behavior simulation of porous silicon nitride ceramics10.1016/j.ceramint.2015.10.102 ↗
13. Thermal shock behavior of pressureless liquid phase sintered SiC ceramics10.1016/j.ceramint.2016.02.101 ↗
14. Fracture toughness, strength and thermal shock behaviour of bulk plasma sprayed alumina Ð eects of heat treatment10.1016/S0955-2219(00)00033-9 ↗
15. Thermal shock resistance of ultra-high temperature ceramics under active cooling condition including the effects of external constraints10.1016/j.applthermaleng.2016.09.004 ↗
16. Unified theory of thermal shock fracture initiation and crack propagation in Brittle Ceramics10.1111/j.1151-2916.1969.tb15848.x ↗
17. Elastic energy at fracture and surface energy as design criteria for thermal shock10.1111/j.1151-2916.1963.tb14605.x ↗
18. Thermal-stress fracture of a thermomechanically strengthened aluminosilicate ceramic10.1111/j.1151-2916.1972.tb11258.x ↗
19. R-curve analysis of solid-phase-sintered and liquid-phase-sintered silicon carbide ceramics by indentation fracture and indentation-strength-in-bending methods10.1016/j.ceramint.2015.11.070 ↗
20. Grain growth and fracture toughness of fine-grained silicon carbide ceramics10.1111/j.1151-2916.1995.tb09100.x ↗
21. Toughness properties of a silicon carbide with an in situ induced heterogeneous grain structure10.1111/j.1151-2916.1994.tb04637.x ↗
22. Dynamic Vickers indentation of brittle materials10.1016/S0043-1648(99)00364-6 ↗
23. Comparison of instrumented Knoop and Vickers hardness measurements on various soft materials and hard ceramics10.1016/j.jeurceramsoc.2006.06.011 ↗
24. Vickers indentation crack analysis of solid-phase-sintered silicon carbide ceramics10.1016/j.ceramint.2012.05.095 ↗