journal article·2022-09Open access

Tailoring the microstructure to enhance the cryogenic mechanical properties of a Fe–34.5Mn–0.04C steel

Jianchao Xiong, Yuhui Wang, Yubin Zhang, Tiansheng Wang, Yan Peng, Andrew Godfrey, Niels Hansen, Xiaoxu Huang

Abstract

Samples of a Fe–34.5Mn–0.04C (wt. %) austenitic steel with average grain size in the range from 0.45 to 21.0 μm were produced by cold rolling and subsequent annealing. The effects of microstructure on room–temperature (RT) and cryogenic tensile properties, and on the related fracture modes, were investigated. It is found that for fully recrystallized samples (those with average grain size in the range from 2.3 to 21 μm), both the yield strength and uniform elongation increase with decreasing grain size at both RT and −180 °C, while for smaller grain sizes (corresponding to partly recrystallized samples) the strength increases at the expense of uniform elongation. In general, samples with an average grain size of 2.3 μm show a better combination of strength and ductility than samples with larger grain sizes. A detailed characterization of the microstructure and fracture surfaces after failure reveals that grain refinement results in elimination of grain boundary martensite, thereby leading to a transition from transgranular and intergranular fracture modes to a ductile fracture mode, characterized by dimpled fracture surfaces. The results are discussed with respect to stacking fault energy and to the Mn and C content. The study provides important inputs for the design of advanced Fe–Mn–C steels for cryogenic applications.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Microstructure and Mechanical Properties of Steels · Metal Alloys Wear and Properties · Metallurgy and Material Forming

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (42)

Show source-provided references
1. Very strong low temperature bainite10.1179/026708301225000725 ↗
2. Development of 9% nickel steel for LNG applications10.1002/srin.200705879 ↗
3. Effects of microstructural change on fracture characteristics in coarse-grained heat-affected zones of QLT-processed 9% Ni steel10.1016/S0921-5093(02)00190-9 ↗
4. Physical and mechanical properties of high manganese non-magnetic steel and its application to various products for commercial use10.2355/isijinternational1966.22.1010 ↗
5. Cryogenic structural materials for superconducting magnets
6. Composition and temperature dependence of tensile properties of austenitic Fe-Mn-Al-C alloys10.1016/0921-5093(89)90844-7 ↗
7. The effects of deformation twins and strain-induced ε-martensite on mechanical properties of an Fe-32Mn-12Cr-0.4C cryogenic alloy10.1016/0956-716X(95)00193-Y ↗
8. Temperature dependence of the flow stress of Fe-18Mn-0.6C-xAl twinning-induced plasticity steel10.1016/j.actamat.2013.07.042 ↗
9. Effects of Mn and Al contents on cryogenic-temperature tensile and Charpy impact properties in four austenitic high-Mn steels10.1016/j.actamat.2015.08.027 ↗
10. Effects of Mn addition on tensile and charpy impact properties in austenitic Fe-Mn-C-Al-based steels for cryogenic applications10.1007/s11661-014-2513-9 ↗
11. High strength Fe-Mn-(Al, Si) TRIP/TWIP steels development—properties—application10.1016/S0749-6419(00)00015-2 ↗
12. Effects of deformation induced phase transformation and twinning on the mechanical properties of austenitic Fe-Mn-Al alloys10.2355/isijinternational.29.868 ↗
13. High manganese austenitic twinning induced plasticity steels: a review of the microstructure properties relationships10.1016/j.cossms.2011.04.002 ↗
14. Cryogenic toughness in a low-cost austenitic steel10.1038/s43246-021-00149-8 ↗
15. Driving force for γ→ε martensitic transformation and stacking fault energy of γ in Fe-Mn binary system10.1007/s11661-000-0271-3 ↗
16. A general mechanism of martensitic nucleation: Part I. General concepts and the FCC→HCP transformation
17. The effects of grain size on yielding, strain hardening, and mechanical twinning in Fe-18Mn-0.6C-1.5Al twinning-induced plasticity steel10.1016/j.msea.2015.11.096 ↗
18. Grain refinement effect on cryogenic tensile ductility in a Fe-Mn-C twinning-induced plasticity steel10.1016/j.matdes.2013.01.061 ↗
19. Tensile properties and twinning behavior of high manganese austenitic steel with fine-grained structure10.1016/j.scriptamat.2008.06.050 ↗
20. A novel ultrafine-grained Fe-22Mn-0.6C TWIP steel with superior strength and ductility10.1016/j.matchar.2016.12.026 ↗
21. Choi · Proc. Int. Offshore Polar Eng. Conf. · 2012 · 29
22. Austenite stabilization through manganese enrichment10.1016/j.scriptamat.2010.09.040 ↗
23. Microstructural evolution and mechanical behaviour of Fe-30Mn-C steels with various carbon contents10.1080/02670836.2016.1268662 ↗
24. Microstructural features controlling the deformation and recrystallization behaviour Fe-30%Mn and Fe-30%Mn-0.5%C10.1016/j.msea.2010.03.014 ↗
25. Hall-Petch strengthening in Fe-34.5Mn-0.04C steel cold-rolled, partially recrystallized and fully recrystallized10.1016/j.scriptamat.2018.06.019 ↗
26. Laminated Fe-34.5 Mn-0.04C composite with high strength and ductility10.1016/j.jmst.2018.05.013 ↗
27. Tailoring dislocation structures and mechanical properties of nanostructured metals produced by plastic deformation10.1016/j.scriptamat.2009.02.018 ↗
28. Hardening by annealing and softening by deformation in nanostructured metals10.1126/science.1124268 ↗
29. Microstructure and mechanical strength of near- and sub-micrometre grain size copper prepared by spark plasma sintering10.1016/j.matdes.2016.12.042 ↗
30. Two-stage Hall-Petch relationship in Cu with recrystallized structure10.1016/j.jmst.2019.12.023 ↗
31. High strength-toughness combination of a low carbon medium-manganese steel plate with laminated microstructure and retained austenite10.1016/j.msea.2017.09.059 ↗
32. Transformation-induced plasticity (TRIP) in advanced steels: a review10.1016/j.msea.2020.140023 ↗
33. Effect of low-temperature on mechanical behavior for an AISI 304 austenitic stainless steel10.1016/j.msea.2017.11.003 ↗
34. The relationship between toughness and microstructure in Fe-high Mn binary alloys10.1007/BF02668556 ↗
35. On the grain boundary embrittlement in an aged 12Ni–6Mn–Fe martensite10.2320/matertrans1960.20.365 ↗
36. Effects of the thermodynamic parameters of the hcp phase on the stacking fault energy calculations in the Fe-Mn and Fe-Mn-C systems10.1016/j.calphad.2010.02.001 ↗
37. The effect of grain size and grain orientation on deformation twinning in a Fe-22wt.% Mn-0.6wt.% C TWIP steel10.1016/j.msea.2010.02.041 ↗
38. Microstructural dependence of Fe-high Mn tensile behavior10.1007/BF02643961 ↗
39. Effect of chemical composition on work hardening of Fe-Mn-C TRIP steels10.1179/026708309X12535382371852 ↗
40. Microstructural evolution and strain hardening of Fe-24Mn and Fe-30Mn alloys during tensile deformation10.1016/j.actamat.2009.05.003 ↗
41. Effect of Si and Al additions on the low temperature toughness and fracture mode of Fe-27Mn alloys10.2355/isijinternational.30.632 ↗
42. Unique transition of yielding mechanism and unexpected activation of deformation twinning in ultrafine grained Fe-31Mn-3Al-3Si alloy10.1038/s41598-021-94800-6 ↗