Investigation of novel post-thermal treatments of alloy 718 fabricated by modulated laser powder bed fusion

Konstantinos Georgilas, Alessandro Sergi, Raja H.U. Khan, Mehmet E. Kartal

Abstract

The aim of this work is to determine the impact of post-thermal treatments on the mechanical properties and microstructure of alloy 718 superalloy manufactured through modulated laser powder bed fusion. Three post-thermal treatments at 980 °C and 1200 °C with and without hot isostatic pressing are utilised, followed by standard ageing procedure. The tensile mechanical properties, microstructure, crystallography, morphology, fracture impact and hardness after each heat treatment are determined. It has been found that the heat treatment procedure at 980 °C significantly affects the tensile properties while leading to no change in grain size or orientation, and formation of twined grains. A temperature of 1200 °C with and without pressure causes considerable grain growth in comparison with the as-built and 980 conditions and significant formation of twinned grains. Hot isostatic pressing was found to produce the tensile mechanical properties close to those of wrought alloy 718.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · High Entropy Alloys Studies · Additive Manufacturing and 3D Printing Technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (36)

Show source-provided references
1. On the time-temperature-transformation behavior of a new dual-superlattice nickel-based superalloy10.1007/s11661-017-4355-8 ↗
2. Georgilas · 2021
3. Influence of double aging heat treatment on phase transformation and dimensional accuracy of inconel 718 alloy made through laser-based additive manufacturing10.1007/s12666-021-02374-8 ↗
4. Effect of solutionizing temperature on the microstructural evolution during double aging of powder bed fusion-additive manufactured IN718 alloy10.1016/j.matchar.2020.110868 ↗
5. Effect of different heat treatments on the microstructure and mechanical properties in selective laser melted INCONEL 718 alloy10.1080/10426914.2016.1257805 ↗
6. Role of heat treatment and build orientation in the microstructure sensitive deformation characteristics of IN718 produced via SLM additive manufacturing
7. Improved plasticity of Inconel 718 superalloy fabricated by selective laser melting through a novel heat treatment process10.1016/j.matdes.2019.107915 ↗
8. Heat treatment of Inconel 718 produced by selective laser melting: microstructure and mechanical properties10.1016/j.msea.2019.02.046 ↗
9. Mitigation of scan strategy effects and material anisotropy through supersolvus annealing in LPBF IN718
10. On the microstructural and mechanical properties of post-treated additively manufactured Inconel 718 superalloy under quasi-static and cyclic loading10.1016/j.msea.2016.05.089 ↗
11. Impact of heat treatment on mechanical behaviour of Inconel 718 processed with tailored microstructure by selective laser melting10.1016/j.matdes.2017.05.065 ↗
12. Structure, texture and phases in 3D printed IN718 alloy subjected to homogenization and HIP treatments10.3390/met7060196 ↗
13. The influence of pulsed laser powder bed fusion process parameters on Inconel 718 material properties10.1016/j.msea.2019.138527 ↗
14. Donachie · 2002
15. Delta phase in INCONEL 718: mechanical properties and forging process requirements
16. 2016
17. SAE International · 2018
18. Reed · 2006
19. The physical metallurgy of cast and wrought alloy 718
20. Fatigue crack growth in IN718/316L multi-materials layered structures fabricated by laser powder bed fusion10.1016/j.ijfatigue.2021.106454 ↗
21. A. Oradei-Basile and J. F. Radavich, “A Current T-T-T Diagram for Wrought Alloy 718.” .
22. S. Azadian, L.-Y. Wei, F. Niklasson, and R. Warren, “PRECIPITATION IN SPRAY-FORMED IN 718.” .
23. Effect of standard heat treatment on the microstructure and mechanical properties of selective laser melting manufactured Inconel 718 superalloy10.1016/j.msea.2015.06.021 ↗
24. Effect of heat treatment on the microstructural evolution of a precipitation-hardened superalloy produced by selective laser melting10.1016/j.msea.2019.01.109 ↗
25. Effect of δ phase on high temperature mechanical performances of Inconel 718 fabricated with SLM process10.1016/j.msea.2019.138327 ↗
26. T. Antonsson and H. Fredriksson, “The Effect of Cooling Rate on the Solidification of INCONEL 718.” .
27. Functionally graded Inconel 718 processed by additive manufacturing: crystallographic texture, anisotropy of microstructure and mechanical properties10.1016/j.matdes.2016.10.075 ↗
28. Mechanical and microstructural investigation of nickel-based superalloy IN718 manufactured by selective laser melting (SLM)10.1002/adem.201500158 ↗
29. Effect of standard heat treatment on the microstructure and mechanical properties of selective laser melting manufactured Inconel 718 superalloy10.1016/j.msea.2015.06.021 ↗
30. Effect of heat treatment on the microstructure and mechanical properties of Inconel 718 processed by selective laser melting10.1016/j.msea.2015.05.035 ↗
31. Effect of the solution temperature on the precipitates and grain evolution of IN718 fabricated by laser additive manufacturing10.3390/ma13020340 ↗
32. The microstructure and mechanical properties of deposited-IN718 by selective laser melting10.1016/j.jallcom.2011.10.107 ↗
33. Porosity, cracks, and mechanical properties of additively manufactured tooling alloys: a review10.1007/s40436-021-00365-y ↗
34. Study on the microstructure and creep behavior of Inconel 718 superalloy fabricated by selective laser melting10.1016/j.msea.2019.138282 ↗
35. Microstructure and Charpy impact properties of 12–14Cr oxide dispersion-strengthened ferritic steels10.1016/j.jnucmat.2007.08.004 ↗
36. On the rejuvenation of crept Ni-Base single crystal superalloys (SX) by hot isostatic pressing (HIP)10.1016/j.msea.2019.04.078 ↗