journal article·2021-03

Competitive relationship during fatigue-crack initiation of friction-stir-welded Al alloy

Zepeng Liu, Hongxia Zhang, Zhenguo Hou, Zhifeng Yan, Peter K. Liaw, Peng Dong

Publisher page

Abstract

Abstract In the present work, uniaxial fatigue tests (R = 0.1) showed that for high-strength aluminum alloys, the crack origin also presented a tendency of transition from the outside to the inside with the stress decreasing. The interior crack-initiation mode has a characteristic of a fish-eye embracing fine granular area (FGA) originated from an inclusion. Moreover, the formation mechanism of FGA was discussed. The values of the stress intensity factor (SIF) range of a surface mode and an internal mode were calculated. The results showed that ΔKFGA keeps constant with an average value of 1.84 MPa•m1/2, which was close to the interior crack-growth threshold (ΔKth,i), 1.911 MPa•m1/2. Paris-Hertzberg law was used to predict the life of fatigue-crack initiation and propagation during internal fracture. The crack-growth rate within FGA and fish-eye was also estimated. Furthermore, the competitive relationship between the interior and surface cracks initiation of welded joints was discussed through the SIF range.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced Welding Techniques Analysis · Fatigue and fracture mechanics · Mechanical stress and fatigue analysis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (38)

Show source-provided references
1. Fatigue behavior of carburized steel with internal oxides and nonmartensitic microstructure near the surface10.1007/BF02648572 ↗
2. Effect of alumite surface treatments on long-life fatigue behavior of a cast aluminum in rotating bending10.1016/j.ijfatigue.2009.10.002 ↗
3. Effect of inclusion on subsurface crack initiation and gigacycle fatigue strength10.1016/S0142-1123(02)00037-3 ↗
4. Relationship among fatigue life, inclusion size and hydrogen concentration for high-strength steel in the VHCF regime10.1016/j.msea.2009.10.056 ↗
5. Mechanism of fatigue crack initiation and propagation in the very high cycle fatigue regime of high-strength steels10.1016/j.scriptamat.2012.07.049 ↗
6. On the formation mechanisms of fine granular area (FGA) on the fracture surface for high strength steels in the VHCF regime10.1016/j.ijfatigue.2015.08.021 ↗
7. Fatigue life and mechanistic modeling of interior micro-defect induced cracking in high cycle and very high cycle regimes10.1016/j.actamat.2018.07.036 ↗
8. Investigation of crack initiation mechanisms responsible for the fish eye formation in the very high cycle fatigue regime10.1016/j.ijfatigue.2018.06.016 ↗
9. The role of local plasticity during very high cycle fatigue crack initiation in high-strength steels10.1016/j.ijfatigue.2018.02.008 ↗
10. There is no infinite fatigue life in metallic materials10.1046/j.1460-2695.1999.00183.x ↗
11. Very high cycle fatigue – is there a fatigue limit?10.1016/j.ijfatigue.2010.05.009 ↗
12. The fatigue limit of bearing steels – Part I: a pragmatic approach to predict very high cycle fatigue strength10.1016/j.ijfatigue.2011.09.015 ↗
13. Fatigue and fracture behaviour of structural Al-alloys up to very long life regimes10.1016/j.ijfatigue.2005.09.017 ↗
14. Micro-crack initiation and propagation in a high strength aluminum alloy during very high cycle fatigue10.1016/j.msea.2018.01.008 ↗
15. Effect of microstructure inhomogeneity and crack initiation environment on the very high cycle fatigue behavior of a magnesium alloy10.1016/j.ijfatigue.2019.105376 ↗
16. Effects of inclusion size and location on very-high-cycle fatigue behavior for high strength steels
17. Effect of stress ratio on HCF and VHCF properties at temperatures of 20 °C and 700 °C for nickel-based wrought superalloy GH3617M10.1016/j.cja.2019.01.026 ↗
18. Mean stress dependence of fatigue strength and subsurface crack initiation in Ti–15Mo–5Zr–3Al alloy10.1016/S0921-5093(99)00710-8 ↗
19. Course of SN-curves especially in the high-cycle fatigue regime with regard to component design and safety10.1016/j.ijfatigue.2006.11.015 ↗
20. A model to predict S–N curves for surface and subsurface crack initiations in different environmental media10.1016/j.ijfatigue.2013.11.013 ↗
21. Transition of fatigue failure mode of Ni–Cr–Mo low-alloy steel in very high cycle regime10.1016/j.ijfatigue.2009.06.011 ↗
22. Incredible improvement in fatigue resistance of friction stir welded 7075-T651 aluminum alloy via surface mechanical rolling treatment10.1016/j.ijfatigue.2019.02.023 ↗
23. Characteristic S–N properties of high-carbon–chromium-bearing steel under axial loading in long-life fatigue10.1046/j.1460-2695.2002.00574.x ↗
24. Fish-eye shape prediction with gigacycle fatigue failure10.1111/j.1460-2695.2011.01576.x ↗
25. S–N curve characteristics and subsurface crack initiation behaviour in ultra-long life fatigue of a high carbon–chromium bearing steel10.1046/j.1460-2695.2001.00459.x ↗
26. Subsurface crack initiation and propagation mechanism in high-strength steel in a very high cycle fatigue regime10.1016/j.ijfatigue.2005.08.015 ↗
27. Factors influencing the mechanism of superlong fatigue failure in steels10.1046/j.1460-2695.1999.00187.x ↗
28. The formation mechanism of characteristic region at crack initiation for very-high-cycle fatigue of high-strength steels10.1016/j.ijfatigue.2015.11.029 ↗
29. Super-long life tension–compression fatigue properties of quenched and tempered 0.46% carbon steel10.1016/S0142-1123(98)00028-0 ↗
30. Gigacycle fatigue behavior and fracture morphology of high speed tool steel, JIS SKH 5110.1299/kikaia.69.662 ↗
31. Review and prospects for current studies on very high cycle fatigue of metallic materials for machine structural use10.1299/jmmp.3.425 ↗
32. Microscopic and nanoscopic observations of metallurgical structures around inclusions at interior crack initiation site for a bearing steel in very high-cycle fatigue10.1111/ffe.12344 ↗
33. Propensities of crack interior initiation and early growth for very-high-cycle fatigue of high strength steels10.1016/j.ijfatigue.2013.02.023 ↗
34. Prediction of threshold value for FGA formation
35. Near threshold fatigue crack propagation and internal cracks in steel
36. Investigation of high cycle and Very-High-Cycle Fatigue behaviors for a structural steel with smooth and notched specimens10.1016/j.engfailanal.2010.06.002 ↗
37. Quantitative evaluation of effects of nonmetallic inclusions on fatigue strength of high strength steels. I: basic fatigue mechanism and evaluation of correlation between the fatigue fracture stress and the size and location of non-metallic inclusions10.1016/0142-1123(89)90054-6 ↗
38. Fatigue crack growth from small to long cracks in very-high-cycle fatigue with surface and internal “fish-eye” failures for ferrite-perlitic low carbon steel SAE 862010.1016/j.msea.2006.08.131 ↗