Investigation of the effect of electrolytic hydrogen charging on tensile-ductility loss in different Al-added low density steels
Source abstract
Abstract
Abstract The presentation investigated the hydrogen embrittlement of a Fe-8.3Mn- (9.5, 12) Al–1C (wt.%) low density steel, focusing on the influence of electrolytic hydrogen charging on tensile-ductility loss. We performed a tensile test after hydrogen charging at a low strain rate (9.5 × 10−6 s−1) to observe hydrogen-assisted cracking. The concentration of hydrogen was measured by thermal desorption spectroscopy and the fracture surface was evaluated by scanning electron microscope. Tensile test results have shown that the strength and elongation of the two kinds of steel after hydrogen charging both reduced, especially the elongation loss was more significant. For 12Al steel, the maximum tensile strength and elongation loss values were 74.22%, 67.73%, respectively. While for 9.5Al steel, the strength loss value was relatively small, the maximum loss value was 8.36%, and it reduced the maximum elongation loss of 26.02%. For the existence of κappa carbides and annealing twins in the tested steel, hydrogen preferentially concentrated on the grain boundaries and twins, leading to intergranular cracking, and the fracture mode changed from ductile fracture to quasi-cleavage fracture.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Microstructure and Mechanical Properties of Steels
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (38)
Show source-provided references
1. Driving force and logic of development of advanced high strength steels for automotive applications10.1002/srin.201200288 ↗
2. Novel ultra-high-strength (ferrite + austenite) duplex lightweight steels achieved by fine dislocation substructures (Taylor lattices), grain refinement, and partial recrystallization10.1016/j.actamat.2015.06.024 ↗
3. Twinning-induced plasticity (TWIP) steels10.1016/j.actamat.2017.06.046 ↗
4. Scott · 2006 · 293
5. Hydrogen delayed fracture properties and internal hydrogen behavior of a Fe-18Mn-1.5Al-0.6C TWIP steel10.2355/isijinternational.49.1952 ↗
6. Hydrogen influence on some advanced high-strength steels10.1016/j.corsci.2017.06.012 ↗
7. Low-density steels10.1016/j.scriptamat.2012.11.037 ↗
8. Low-density steels: the effect of Al addition on microstructure and properties, TMS
9. Alloy design, combinatorial synthesis, and microstructure - property relations for low-density Fe-Mn-Al-C austenitic steels10.1007/s11837-014-1032-x ↗
10. Effects of static and dynamic strain aging on hydrogen embrittlement in TWIP steels containing Al10.2355/isijinternational.53.1268 ↗
11. The mechanism of enhanced resistance to the hydrogen delayed fracture in Al-added Fe-18Mn-0.6C twinning-induced plasticity steels10.1016/j.ijhydene.2012.03.100 ↗
12. Hydrogen embrittlement associated with strain localization in a precipitation-hardened Fe-Mn-Al-C light weight austenitic steel10.1016/j.ijhydene.2013.12.171 ↗
13. Role of cold rolled followed by annealing on improvement of hydrogen induced cracking resistance in pipeline steel10.1016/j.engfailanal.2018.04.044 ↗
14. Hydrogen embrittlement of automotive advanced high-strength steels
15. Hydrogen embrittlement in different materials: a review10.1016/j.ijhydene.2018.09.201 ↗
16. Effect of hydrogen content on the embrittlement in a Fe-Mn-C twinning-induced plasticity steel10.1016/j.corsci.2012.03.009 ↗
17. Hydrogen embrittlement in Al-added twinning-induced plasticity steels evaluated by tensile tests during hydrogen charging10.2355/isijinternational.52.2283 ↗
18. Effect of strain rate on hydrogen embrittlement susceptibility of twinning-induced plasticity steel pre-charged with high-pressure hydrogen gas10.1016/j.ijhydene.2016.06.259 ↗
19. Hydrogen embrittlement in a Fe-Mn-C ternary twinning-induced plasticity steel10.1016/j.corsci.2011.09.022 ↗
20. The effect of Si on hydrogen embrittlement of Fe-18Mn-0.6C-xSi twinning-induced plasticity steels10.1016/j.actamat.2015.10.015 ↗
21. Molodov. On the deformation behavior of κ-carbide-free and κ-carbide-containing high-Mn light-weight steel10.1016/j.actamat.2016.10.006 ↗
22. k-phase formation in Fe-Mn-Al-C austenitic steels10.1002/srin.201400587 ↗
23. The predominant role of strain-induced vacancies in hydrogen embrittlement of steels Overview10.1016/j.actamat.2018.12.013 ↗
24. Hydrogen delayed fracture properties and internal hydrogen behavior of a Fe-18Mn-1.5Al-0.6C TWIP steel10.2355/isijinternational.49.1952 ↗
25. Equivalent hydrogen fugacity during electrochemical charging of some martensitic advanced high-strength steels10.1016/j.corsci.2017.08.011 ↗
26. Permeability, solubility and diffusivity of hydrogen isotopes in stainless steels at high gas pressures10.1016/j.ijhydene.2006.05.008 ↗
27. The diffusion and trapping of hydrogen in steel10.1016/0001-6160(70)90078-7 ↗
28. Hydrogen transport to fracture sites in metals and alloys multiphysics modelling10.1016/j.prostr.2017.07.112 ↗
29. Hydrogen trapping in ferritic steel weld metal10.1179/095066002225006548 ↗
30. Overview of hydrogen embrittlement in high-Mn steels10.1016/j.ijhydene.2017.02.214 ↗
31. Thermal analysis of trapped hydrogen in pure iron10.1007/BF02642424 ↗
32. Enumeration of the hydrogen-enhanced localized plasticity mechanism for hydrogen embrittlement in structural materials10.1016/j.actamat.2018.12.014 ↗
33. Diffusion coefficient of hydrogen interstitial atom in α-Fe, γ-Fe and ε-Fe crystals by first-principle calculations10.1016/j.ijhydene.2017.08.212 ↗
34. The role of κ-carbides as hydrogen traps in high-Mn steels
35. Effect of grain refinement on hydrogen embrittlement behaviors of high-Mn TWIP steel10.1016/j.msea.2015.11.017 ↗
36. Trap-governed hydrogen diffusivity and uptake capacity in ultrahigh-strength AERMET 100 steel10.1007/s11661-002-0032-6 ↗
37. Hydrogen-assisted failure in a twinning-induced plasticity steel studied under in situ hydrogen charging by electron channeling contrast imaging10.1016/j.actamat.2013.04.030 ↗
38. Hydrogen-induced cracking at grain and twin boundaries in an Fe-Mn-C austenitic steel10.1016/j.scriptamat.2011.12.015 ↗