Fatigue behavior of Zr-based metallic glass micropillars
Source abstract
Abstract
Abstract Metallic glass with thermoplastic properties in the supercooled liquid region is a potential type of material for fabricating micro molds. Fatigue behavior of metallic glass is the crucial property that enables it to serve as a mold material. Here, fatigue and fracture behaviors of the micro-sized Zr41·2Ti13·8Cu12·5Ni10Be22.5 (at.%, Vit1) metallic glass micropillars were investigated by uniaxial compression-compression fatigue tests. It was shown that the micropillars have fatigue–endurance limit of ~1000 MPa and a fatigue ratio of ~0.56. The effects of sample size and heat treatment on the fatigue limit were also studied. After annealing at 450 °C, the fatigue limit decreased to ~600 MPa and the fatigue ratio decreased to ~0.43. The fracture angles between the stress axis and the shear plane of unannealed metallic glass were found to be ~42°, while the annealed Vit1 micropillars failed in break or splitting modes. These findings provided the experimental evidence for the inhomogeneous structure and the size effect in metallic glass failure modes at the micro-scale size. Our results can serve as a guideline for further studies to investigate the mechanical behavior and deformation mechanisms of the metallic glass.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metallic Glasses and Amorphous Alloys · Glass properties and applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (54)
Show source-provided references
1. The elastic properties, elastic models and elastic perspectives of metallic glasses10.1016/j.pmatsci.2011.07.001 ↗
2. Mechanical behavior of amorphous alloys10.1016/j.actamat.2007.01.052 ↗
3. Bulk metallic glass: the smaller the better10.1002/adma.201002148 ↗
4. Thermoplastic extrusion of bulk metallic glass10.1016/j.scriptamat.2009.02.052 ↗
5. The superplastic forming of bulk metallic glasses
6. Nanomoulding with amorphous metals10.1038/nature07718 ↗
7. Superplastic micro-forming of Zr65Cu17.5Ni10Al7.5 bulk metallic glass with silicon mold using hot embossing technology10.1016/j.jallcom.2009.04.092 ↗
8. Polymer micro molding with bulk metallic glass mold10.1007/s00542-014-2221-9 ↗
9. An experimental investigation and modeling of micro array replication with Zr-based bulk metallic glass using a hot embossing process10.1016/j.ijmachtools.2017.02.003 ↗
10. Fatigue-induced damage in Zr-based bulk metallic glasses10.1038/srep02578 ↗
11. Fatigue behaviour of Fe-Cr-Si-B metallic glass wires10.1016/S0142-1123(02)00014-2 ↗
12. Fatigue behavior of Zr-based bulk-metallic glasses
13. Progress in studying the fatigue behavior of Zr-based bulk-metallic glasses and their composites10.1016/j.intermet.2009.01.017 ↗
14. Compression-compression fatigue study on model metallic glass nanowires by molecular dynamics simulations10.1063/1.3610443 ↗
15. Fatigue and fracture behavior of bulk metallic glasses and their composites10.1016/j.pmatsci.2018.07.002 ↗
16. The fatigue endurance limit of a Zr-based bulk metallic glass10.1016/j.scriptamat.2006.06.015 ↗
17. Fracture toughness and fatigue-crack propagation in a Zr–Ti–Ni–Cu–Be bulk metallic glass10.1063/1.119610 ↗
18. Fatigue of a Zr-Ti-Cu-Ni-Be bulk amorphous metal: stress/life and crack-growth behavior10.1016/S1359-6462(97)00522-8 ↗
19. Mechanisms for fracture and fatigue-crack propagation in a bulk metallic glass10.1007/s11661-999-0173-y ↗
20. Fatigue-strength enhancement of cast Zr50Cu40Al10 glassy alloys10.2320/matertrans.47.1286 ↗
21. Fatigue crack initiation and small-crack propagation in Zr-based bulk metallic glass10.2320/matertrans.MJ200758 ↗
22. Fatigue of Zr-based bulk metallic glass under compression-compression stress10.1002/adem.200800141 ↗
23. Fatigue deformation of microsized metallic glasses10.1016/j.scriptamat.2012.12.011 ↗
24. Size effect in Pd77.5Cu6Si16.5 metallic glass micro-wires: more scattered strength with decreasing diameter10.1063/1.4991849 ↗
25. Size effects on tensile and compressive strengths in metallic glass nanowires10.1016/j.jmps.2015.07.018 ↗
26. Atomistic origin of size effects in fatigue behavior of metallic glasses10.1016/j.jmps.2017.04.005 ↗
27. Effects of size on the strength and deformation mechanism in Zr-based metallic glasses10.1016/j.ijplas.2010.09.010 ↗
28. Real-time, high-resolution study of nanocrystallization and fatigue cracking in a cyclically strained metallic glass10.1073/pnas.1320235110 ↗
29. Shear band-mediated fatigue cracking mechanism of metallic glass at high stress level10.1016/j.msea.2015.01.008 ↗
30. Compression-compression fatigue behavior of CuZr-based bulk metallic glass composite containing B2 phase10.1016/j.intermet.2017.02.001 ↗
31. Probabilistic measurements of the fatigue limit data from a small sampling up-and-down test method10.1016/j.ijfatigue.2008.06.004 ↗
32. Metallic Materials and Elements for Aerospace Vehicle Structures (MIL-HDBK-5J), DoD2004.
33. Nanocrystallization of Zr41.2Ti13.8Cu12.5Ni10.0Be22.5 metallic glass10.1016/j.actamat.2004.05.038 ↗
34. Relaxation and crystallization of Zr41.2Ti13.8Cu12.5Ni10Be22.5 bulk amorphous alloys10.1016/j.msea.2003.08.007 ↗
35. Characterization of multiple crystallization steps in Zr41.2Ti13.8Cu12.5Ni10Be22.5 bulk metallic glass10.1016/j.msea.2006.02.425 ↗
36. Fracture and fatigue behavior of a Zr–Ti–Nb ductile phase reinforced bulk metallic glass matrix composite10.1016/j.scriptamat.2003.08.020 ↗
37. Corrosion–fatigue studies of the Zr-based Vitreloy 105 bulk metallic glass10.1016/j.msea.2007.03.106 ↗
38. Fatigue and fracture behavior of (Zr58Ni13.6Cu18Al10.4)99Nb1 bulk-amorphous alloy10.1016/j.intermet.2006.01.044 ↗
39. Fatigue endurance limit and crack growth behavior of a high-toughness Zr 61 Ti 2 Cu 25 Al 12 bulk metallic glass10.1016/j.actamat.2015.07.071 ↗
40. Fatigue behavior of a Zr-based bulk metallic glass under uniaxial tension–tension and three-point bending loading mode10.1016/j.intermet.2015.02.005 ↗
41. Fatigue behavior of Zr52.5Al10Ti5Cu17.9Ni14.6 bulk metallic glass10.1016/S0966-9795(02)00152-8 ↗
42. Fatigue behavior of Zr–Ti–Ni–Cu–Be bulk-metallic glasses10.1016/j.intermet.2004.07.037 ↗
43. Comparison of fatigue behavior of a bulk metallic glass and its composite10.1016/j.intermet.2006.01.045 ↗
44. The influence of Pd on tension–tension fatigue behavior of Zr-based bulk-metallic glasses10.1016/j.ijfatigue.2009.04.009 ↗
45. Difference in compressive and tensile fracture mechanisms of Zr59Cu20Al10Ni8Ti3 bulk metallic glass10.1016/S1359-6454(02)00521-9 ↗
46. Stress-temperature scaling for steady-state flow in metallic glasses10.1103/PhysRevLett.104.205701 ↗
47. Cavitation in amorphous solids10.1103/PhysRevLett.110.185502 ↗
48. Evaluation of flow units and free volumes in metallic glasses10.1063/1.4895586 ↗
49. Decoding flow unit evolution upon annealing from fracture morphology in metallic glasses10.1016/j.msea.2016.12.130 ↗
50. The Mohr-Coulomb criterion from unit shear processes in metallic glass10.1016/j.intermet.2004.07.001 ↗
51. Cyclic deformation in metallic glasses10.1021/acs.nanolett.5b03045 ↗
52. Homogeneous flow of metallic glasses: a free volume perspective10.1016/j.scriptamat.2005.09.046 ↗
53. Fatigue damage and fracture behavior of metallic glass under cyclic compression10.1016/j.msea.2018.01.056 ↗
54. Fatigue behavior of an Fe48Cr15Mo14Er2C15B6 amorphous steel10.1557/jmr.2007.0047 ↗