Anomalous precipitation hardening in Al-(1 wt%)Cu thin films
Source abstract
Abstract
This paper concentrates on the precipitation hardening of Al-(1 wt%)Cu thin films. It is shown that in contrast to bulk, the well-known approach of precipitation hardening in confined systems like thin layers and thin films does not operate in the conventional way. This work analyses and discusses the precipitate hardening and its relation to the precipitation mechanism of Al-(1 wt%)Cu thin films which are subjected to precipitation hardening, nano-indentation hardness measurements. Microfabricated Al-(1 wt%)Cu thin films were solution treated at 550 °C for 15 min, quenched and aged at 190 °C for various durations up to 48 h. Nano-indentation hardness measurements revealed for the first time an unexpected decrease in hardness at just ∼8 hours of aging, followed by a saturating increase. Microstructural analysis employing electron microscopy (high-resolution transmission, scanning, backscatter diffraction, energy dispersive spectroscopy) and x-ray diffraction revealed GP zones and θ precipitates but no θ’ in as-received films, and only θ precipitates for aging durations longer than 6 h in the precipitate hardened films. Through-thickness analyses of aged specimens highlighted that θ precipitates nucleate and grow essentially at grain boundary grooves and at the specimen surface as preferential nucleation sites, while depleting Cu from the grain interior. It is shown that the growing precipitation at the surface and grain boundary grooves depletes the Cu in the thin film interior explaining the weakening-hardening sequence observed in the hardness measurements. Hence, the work shows that precipitation kinetics, and not thermodynamics, determine the precipitation state in thin films.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metal and Thin Film Mechanics · Aluminum Alloys Composites Properties · Microstructure and mechanical properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (37)
Show source-provided references
1. Hundred years of precipitation hardening10.1016/S1471-5317(01)00006-2 ↗
2. Precipitation hardening in the first aerospace aluminum alloy: the Wright flyer crankcase10.1126/science.266.5187.1015 ↗
3. The effect of copper additions on electromigration in aluminum thin films10.1007/BF02662722 ↗
4. Mechanical properties and microstructural characterization of Al-0.5%Cu thin films10.1007/BF02673337 ↗
5. J.M.J. Den Toonder, A.R. Van Dijken, Optimization of mechanical properties of thin free-standing metal films for RF-MEMS, in: J. L. et al. (Ed.), Mater. Res. Soc. Symp. Proceedings, vol. 820 of Nanoengineered Assemblies and Advanced Micro/Nanosystems, 2004, pp. 177–182.10.1557/PROC-820-O8.3 ↗
6. Dislocation dynamics in aluminium and in aluminium-copper alloys: a nuclear magnetic resonance and transmission electron microscopic study10.1016/0001-6160(82)90173-0 ↗
7. Characterization of time-dependent anelastic microbeam bending mechanics10.1088/0022-3727/47/35/355306 ↗
8. On the underlying micromechanisms in time-dependent anelasticity in al-(1 wt%)10.1016/j.actamat.2016.10.058 ↗
9. Gradient crystal plasticity modelling of anelastic effects in particle strengthened metallic thin films10.1007/s11012-014-9907-z ↗
10. Haassen · 1996
11. Porter · 2009
12. Aluminum-copper system
13. Creep-resistant aluminum alloys for use in MEMS10.1088/0960-1317/15/7/023 ↗
14. The evolution of microstructure in Al-2%Cu thin films: precipitation, dissolution, and reprecipitation10.1007/BF02646989 ↗
15. The role of Cu distribution and Al2Cu precipitation on the electromigration reliability of submicrometer Al(Cu) lines10.1063/1.356102 ↗
16. Mechanical properties and microstructures of Al-Cu thin films with various heat treatments10.1007/BF03025973 ↗
17. Stress relaxation in Al-Cu and Al-Si-Cu thin films10.1557/JMR.1999.0170 ↗
18. Phase transformations in Al-Cu thin films: precipitation and copper redistribution10.1016/S1359-6454(01)00048-9 ↗
19. Formation of second phase particles in aluminum-copper alloy films10.1016/0040-6090(72)90209-X ↗
20. A. Jourdain, K. Vaesen, J.M. Scheer, J.W. Weekamp, J.T.M. van Beek, H.A.C. Tilmans, From zero- to second-level packaging of RF-MEMS devices, in: Proceedings of the 18th IEEE International Conference on Micro Electro Mechanical Systems, MEMS, 2005, pp. 36–39. 〈http://dx.doi.org/10.1109/MEMSYS.2005.1453861〉.10.1109/MEMSYS.2005.1453861 ↗
21. On-wafer time-dependent high reproducibility nano-force tensile testing10.1088/0022-3727/47/49/495306 ↗
22. The kinetics of the oxidation of aluminum-copper alloys in oxygen at high temperature10.1016/0010-938X(73)90015-2 ↗
23. Mechanical properties of Al-Cu films with various heat treatments10.1557/PROC-473-409 ↗
24. The correlation of the indentation size effect measured with indenters of various shapes10.1016/S0022-5096(01)00103-X ↗
25. Effects of the substrate on the determination of thin film mechanical properties by nanoindentation10.1016/S1359-6454(01)00328-7 ↗
26. Determining hardness of thin films in elastically mismatched film-on-substrate systems using nanoindentation10.1016/j.actamat.2005.11.026 ↗
27. Rate-dependent indentation hardness of a power-law creep solder alloy10.1063/1.1537513 ↗
28. Dislocation arrangement in copper single crystals as a function of strain10.1098/rspa.1966.0139 ↗
29. Precipitation of Al2Cu in blanket Al-Cu films10.1063/1.365745 ↗
30. θ- Al2Cu formation at room temperature in metastable Al-Cu alloy films10.1016/0001-6160(89)90260-5 ↗
31. The precipitation of θ′ at high-angle boundaries in an Al-Cu alloy10.1016/0001-6160(70)90082-9 ↗
32. Theory of thermal grooving10.1063/1.1722742 ↗
33. Physical origins of intrinsic stresses in Volmer-Weber thin films10.1557/mrs2002.15 ↗
34. Precipitate effects on the mechanical behavior of aluminum copper alloys: part i. experiments10.1007/s11661-005-1006-2 ↗
35. Lattice parameter determinations with an X-ray spectrogoniometer by the Debye-Scherrer method and the effect of specimen condition10.1063/1.1728392 ↗
36. Refinement of the crystal structure of tetragonal Al2Cu10.1016/0022-4596(89)90188-6 ↗
37. The θ’ structure in aluminium-copper alloys10.1107/S0365110X56001820 ↗