journal article·2022-01

Surface activation and brazing of SiC ceramic by ion bombardment

Z.B. Chen, X.G. Song, M. Dan, Y. Luo, B. Han

Publisher page

Abstract

Abstract Surface microstructural modification of SiC ceramic is induced by ion bombardment under different bias voltage, and the effect on related evolution of interfacial microstructure and shear property of brazed joints are studied in detail. Increasing the bias voltage from 30 keV to 60 keV, the thickness of the amorphous layer in the SiC surface increases from 80.8 nm to 130 nm, as well as for the amorphization degree. Moreover, dislocation generation, twin formation and complete amorphization transformation evolution processes occur below the amorphous layer. The surface roughness of SiC decreases while surface energy increases 14.9%. Obvious stratification is gradually disappeared and a TiC + Ti5Si3 mixed reaction layer is formed in SiC brazed joints when bias voltage reaches 40 keV. The thickness of the interfacial reaction layer decreases firstly and then increases slightly, while the shear strength of the brazed joints follows the opposite trend. The interfacial reaction layer and shear property of brazed joints can be regulated by optimizing ion bombardment parameters.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Nuclear materials and radiation effects

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (32)

Show source-provided references
1. Fabrication of SiC ceramic architectures using stereolithography combined with precursor infiltration and pyrolysis10.1016/j.ceramint.2019.04.100 ↗
2. Fabrication and characterization of SPS sintered SiC-based ceramic from Y3Si2C2-coated SiC powders10.1016/j.jeurceramsoc.2018.07.054 ↗
3. Microstructure and mechanical properties of SiC ceramic joints vacuum brazed with in-situ formed SiC particulate reinforced Si–24Ti alloy10.1016/j.vacuum.2019.109160 ↗
4. Microstructural evolution and mechanical properties of FeNi42 alloy and SiC ceramic joint vacuum brazed with Ag-based filler metals10.1016/j.ceramint.2020.02.049 ↗
5. Interfacial microstructure and mechanical properties of SiC joints achieved by reactive air brazing using Ag-V2O5 filler10.1016/j.jeurceramsoc.2019.03.013 ↗
6. Microstructure and mechanical strength of SiC joints brazed with Cr3C2 particulate reinforced Ag-Cu-Ti brazing alloy10.1016/j.ceramint.2018.04.002 ↗
7. Initial stages of wetting of alumina by reactive CuAgTi alloys10.1016/j.scriptamat.2011.03.026 ↗
8. Titanium-deposition assisted brazing of SiC ceramic using inactive AgCu filler10.1016/j.matchar.2018.05.054 ↗
9. Effect of Ti addition on the wetting and brazing of Sn0.3Ag0.7Cu filler on SiC ceramic10.1111/jace.16245 ↗
10. An analysis of deformation mechanism in the Si3N4–AgCuTi+SiCp–Si3N4 joints by digital image correlation10.1016/j.jeurceramsoc.2012.07.038 ↗
11. Brazing of CBN grains with Ag-Cu-Ti/TiX composite filler - the effect of TiX particles on microstructure and strength of bonding layer10.1016/j.matdes.2016.03.033 ↗
12. Effects of ion implantation on the brazing properties of high purity alumina10.1016/j.surfcoat.2011.09.034 ↗
13. Activation of electroplated-Cu surface via plasma pretreatment for low temperature Cu-Sn bonding in 3D interconnection10.1016/j.apsusc.2016.05.023 ↗
14. Plasma-activated direct bonding of diamond-on-insulator wafers to thermal oxide grown silicon wafers10.1016/j.diamond.2010.08.015 ↗
15. Improve the structure and optical surface properties of LDPE by ion bombardment technique10.1016/j.optmat.2021.110940 ↗
16. Surface modification and structure evolution of aluminum under argon ion bombardment10.1016/j.apsusc.2020.147819 ↗
17. Surface-activation assisted brazing of Al-Zn-Mg-Cu alloy: improvement in microstructure and mechanical properties10.1016/j.matlet.2018.01.153 ↗
18. Study of ion bombardment of SiC ceramic: surface and interfacial reaction modification10.1016/j.jeurceramsoc.2019.11.008 ↗
19. Wetting behavior of AgCu–Ti filler metal on SiC ceramic surface pre-treated by ion bombardment10.1016/j.ceramint.2019.12.154 ↗
20. Brazing of SiC ceramic pretreated by chromium coating using inactive AgCu filler metal10.1111/ijac.13605 ↗
21. Radiation tolerance of complex oxides10.1126/science.289.5480.748 ↗
22. Electron-irradiation-induced crystalline-to-amorphous transition in β-SiC single crystals10.1080/13642819208223042 ↗
23. Neutron irradiation induced amorphization of silicon carbide10.1016/S0022-3115(99)00023-9 ↗
24. Handbook of SiC properties for fuel performance modeling10.1016/j.jnucmat.2007.05.016 ↗
25. Twins induced by high-temperature ion irradiation in body-centered cubic V-4Cr-4Ti alloy10.1016/j.scriptamat.2018.11.033 ↗
26. Quantification of irradiation defects in beta-silicon carbide using Raman spectroscopy10.1016/j.scriptamat.2016.08.004 ↗
27. Amorphization of silicon carbide by carbon displacement10.1063/1.1739515 ↗
28. Ultrahigh strength and high electrical conductivity in copper10.1126/science.1092905 ↗
29. Interfacial microstructure and mechanical property of ZrC-SiC ceramic and Ti6Al4V joint brazed with AgCuTi alloy10.1016/j.jeurceramsoc.2017.02.056 ↗
30. Wettability and joining of SiC by Sn-Ti: microstructure and mechanical properties10.1016/j.jmst.2019.08.040 ↗
31. A comparative study of low energy radiation responses of SiC, TiC and ZrC10.1016/j.actamat.2016.03.011 ↗
32. Defect production, multiple ion–solid interactions and amorphization in SiC10.1016/S0168-583X(02)00598-0 ↗