Abstract

Abstract The use of alternating hydrogenated amorphous carbon (a-C:H) full coatings on all sides of a single-crystal silicon (SCS) based microstructure was proposed to explore the enhancement of the tensile strength and fracture toughness of a coating−substrate system. By tailoring the individual layer thickness (λ) from 25 to 150 nm, we synthesized a series of multilayer coatings deposited alternately by controlling bias voltage between −200 and −600 V with the total thickness maintained at 300 nm by plasma enhanced chemical vapor deposition (PECVD). The tensile strength and fracture toughness of coating−substrate system were investigated by a quasi-static tensile test and pillar splitting, respectively. A ∼37.8% increase in the tensile strength (maximum of 4.34 GPa) and ∼41.5% increase in the fracture toughness (maximum of 1.33 MPa m1/2) of coated samples were achieved as compared with a bare silicon microstructure. The highest tensile strength was found at a λ of 75 nm, whereas fracture toughness increased monotonically as λ dropped from 150 to 25 nm. We attributed this λ dependence to a combined effect of toughness enhancement and crack shielding. These new findings were useful for the design of alternating multilayer coated micro electro mechanical system (MEMS) devices with enhanced mechanical reliability.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Diamond and Carbon-based Materials Research · Metal and Thin Film Mechanics · Advanced ceramic materials synthesis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (43)

Show source-provided references
1. Fracture behavior of single crystal silicon with thermal oxide layer10.1016/j.engfracmech.2015.08.029 ↗
2. Specimen size effect on tensile strength of surface-micromachined polycrystalline silicon thin films10.1109/84.661392 ↗
3. Influence of ICP etching damage on the brittle-fracture strength of single-crystal silicon10.2472/jsms.56.920 ↗
4. Selective carbon material engineering for improved MEMS and NEMS10.3390/mi10080539 ↗
5. A perspective on the optimisation of hard carbon and related coatings for engineering applications10.1016/j.tsf.2007.02.011 ↗
6. Fracture behavior and deformation mechanisms in nanolaminated crystalline/amorphous micro-cantilevers10.1016/j.actamat.2019.09.002 ↗
7. 60 years of DLC coatings: historical highlights and technical review of cathodic arc processes to synthesize various DLC types, and their evolution for industrial applications10.1016/j.surfcoat.2014.08.017 ↗
8. Effects of indenter angle on micro‐scale fracture toughness measurement by pillar splitting10.1111/jace.15093 ↗
9. Tensile test of a silicon microstructure fully coated with submicrometer-thick diamond like carbon film using plasma enhanced chemical vapor deposition method10.7567/JJAP.56.06GN01 ↗
10. Effect of substrate bias voltage on tensile properties of single crystal silicon microstructure fully coated with plasma CVD diamond-like carbon film10.1016/j.apsusc.2018.02.179 ↗
11. Fracture behavior of single-crystal silicon microstructure coated with stepwise bias-graded aC: H film
12. Tensile testing of silicon thin films10.1111/j.1460-2695.2005.00910.x ↗
13. Indentation-based methods to assess fracture toughness for thin coatings10.1088/0022-3727/45/20/203001 ↗
14. Prediction of the fracture toughness of a ceramic multilayer composite-Modeling and experiments10.1016/j.actamat.2006.07.046 ↗
15. Superlattice effect for enhanced fracture toughness of hard coatings10.1016/j.scriptamat.2016.06.030 ↗
16. Model of superlattice yield stress and hardness enhancements10.1063/1.359467 ↗
17. Effect of microstructure and mechanical properties difference between sub-layers on the performance of alternate hard and soft diamond-like carbon multilayer films10.1016/j.surfcoat.2013.06.030 ↗
18. Enhanced tribological and corrosion properties of multilayer ta-C films via alternating sp3 content10.1016/j.surfcoat.2019.05.087 ↗
19. ECR sputtering and electron/ion alternative irradiation for multilayer carbon films fabrication with tunable layer thickness10.1016/j.surfcoat.2016.04.001 ↗
20. Improving the crack resistance and fracture toughness of Cu/Ru multilayer thin films via tailoring the individual layer thickness10.1016/j.jallcom.2018.01.282 ↗
21. A novel pillar indentation splitting test for measuring fracture toughness of thin ceramic coatings10.1080/14786435.2014.913110 ↗
22. High temperature fracture toughness of ceramic coatings evaluated using micro-pillar splitting10.1016/j.scriptamat.2018.11.013 ↗
23. Measurement of fracture toughness by nanoindentation methods: recent advances and future challenges10.1016/j.cossms.2015.04.003 ↗
24. Thin films stress extraction using micromachined structures and wafer curvature measurements10.1016/j.mee.2004.07.003 ↗
25. Statistical evaluation of the strength of wear-resistant hard coatings10.1016/j.surfcoat.2007.07.088 ↗
26. Measuring the fracture resistance of hard coatings10.1063/1.4803928 ↗
27. Amorphous carbon thin films10.1016/S0927-796X(02)00005-0 ↗
28. Pulsed PECVD deposition of diamond-like carbon films10.1016/S0925-9635(01)00612-4 ↗
29. Electrical properties of multilayer (DLC-TiC) films produced by pulsed laser deposition10.1016/j.apsusc.2017.08.058 ↗
30. Growth of single‐crystal TiN/VN strained‐layer superlattices with extremely high mechanical hardness10.1063/1.339770 ↗
31. Relationship between interfacial strain and the elastic response of multilayer metal films10.1103/PhysRevLett.61.2356 ↗
32. Continuum elasticity analysis of the enhanced modulus effect in metal-alloy superlattice films10.1103/PhysRevB.35.5413 ↗
33. Fracture toughness of diamondlike carbon coatings10.1557/JMR.1999.0293 ↗
34. Deformation and cracking mechanism in CrN/TiN multilayer coatings10.3390/coatings9060363 ↗
35. Length-scale-dependent deformation mechanism of Cu/X(X¼Ru,W) multilayer thin films10.1016/j.msea.2016.03.126 ↗
36. Indentation mechanics and fracture behavior of metal/ceramic nanolaminate composites10.1007/s10853-008-2450-3 ↗
37. Focused ion beam (FIB) tomography of nanoindentation damage in nanoscale metal/ceramic multilayers10.1016/j.matchar.2010.01.005 ↗
38. Fracture mechanisms of thin amorphous carbon films in nanoindentation10.1016/S1359-6454(97)00143-2 ↗
39. Determination of elastic modulus and Poisson's ratio of diamond-like carbon films10.1016/S0040-6090(98)01512-0 ↗
40. Cracking of thin bonded films in residual tension10.1016/0020-7683(92)90015-L ↗
41. Length-scale-dependent deformation and fracture behavior of Cu/X (X= Nb, Zr) multilayers: the constraining effects of the ductile phase on the brittle phase10.1016/j.actamat.2011.08.016 ↗
42. Retardation of dislocation generation and motion in thin-layered metal laminates10.1103/PhysRevLett.41.1814 ↗
43. Apparent fracture toughness of Si3N4-based laminates with residual compressive or tensile stresses in surface layers10.1016/j.actamat.2004.09.022 ↗