Source abstract
Abstract
Abstract Magnetically impelled arc butt (MIAB) welding has been the focus of several industries to weld metals in tubular form. 4 mm thick AISI 409 ferritic stainless steel tubes were joined effectively using MIAB welding. The arc duration was varied (4s–8s with an increment of 1s) during welding and all other process parameters such as arc rotation current, upset current, upset time, upset pressure and initial gap were maintained at a constant value. Several microscopic techniques were used to study the microstructure evolution in the joint region. The increase in arc duration pumped more heat energy during joining and increased the size of the weld zone and the axial shortening. The weld zone exhibited a typical forged structure which was affected by heat and mechanical force and is known as TMAZ. The grain size was continuously refined from base metal towards the weld center. The changes in grain size allowed dividing TMAZ into three regions. The welding cycle did not cause any grain growth to produce a heat affected zone (HAZ) similar to fusion welding processes. The increase in arc duration increased the grain size at the weld center. The ferritic structure did not transform into other structures during welding. There was a remarkable increase in the hardness of TMAZ compared to base metal. The strengthening was ascribed to the formation of strain fields in large quantities due to upsetting. Variation in arc duration remarkably influenced the tensile strength and the fracture location. The choice of the arc duration is important to produce sound joints.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Railway Systems and Materials Science · Welding Techniques and Residual Stresses · Hydrogen embrittlement and corrosion behaviors in metals
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (28)
Show source-provided references
1. Ultra-pure ferritic stainless steels—grade, refining operation, and application10.1016/S1006-706X(07)60053-3 ↗
2. Some considerations on the toughness properties of ferritic stainless steels—a brief review10.1016/0308-0161(93)90114-9 ↗
3. Recent developments in stainless steels10.1016/j.mser.2009.03.001 ↗
4. On the shear resistance of ferritic stainless steel composite slabs10.1016/j.conbuildmat.2018.09.003 ↗
5. Microstructural characterization of the HAZ in AISI 444 ferritic stainless steel welds10.1016/j.matchar.2007.03.011 ↗
6. Evaluation of microstructure and mechanical properties of laser beam welded AISI 409M grade ferritic stainless steel10.1016/S1006-706X(12)60050-8 ↗
7. Comparative studies on the weldability, microstructure and tensile properties of autogeneous TIG welded AISI 430 ferritic stainless steel with and without flux10.1016/j.jmapro.2015.09.008 ↗
8. Microstructure and mechanical properties of electron beam-welded AISI 409M-grade ferritic stainless steel10.1007/s00170-010-3044-1 ↗
9. Some experimental investigations on friction welded stainless steel joints10.1016/j.matdes.2007.06.006 ↗
10. The effect of tool rotational and traverse speed on friction stir weldability of AISI 430 ferritic stainless steels10.1016/j.matdes.2011.04.013 ↗
11. Analysis of arc rotation velocity in magnetically impelled arc butt welding10.1080/09507118709452125 ↗
12. Magnetically impelled arc butt welding of aluminium pipes
13. Magnetically impelled arc butt welding of hollow and solid parts10.1007/BF03263390 ↗
14. A study on the numerical analysis of magnetic flux density by a solenoid for magnetically impelled arc butt welding10.1243/095440503322617171 ↗
15. Recent developments in high productivity pipeline welding10.1590/S1678-58782004000100015 ↗
16. Technological windows for MIAB welding of tubes featuring original longitudinal magnetization system with peripheral solenoids10.1016/j.jmatprotec.2010.02.007 ↗
17. Magnetically Impelled Arc Butt Welding of alloy steel tubes in boilers – establishment of parameter window10.1016/j.mechatronics.2010.08.001 ↗
18. Feasibility of magnetically impelled arc butt (MIAB) welding of high-thickness tubes for pressure parts10.1080/10426914.2011.585488 ↗
19. MIAB welding of alloy steel tubes in pressure parts: metallurgical characterization and nondestructive testing10.1016/j.jmapro.2011.09.006 ↗
20. Effect of upset current in magnetically impelled arc butt (MIAB) welding of carbon steel tubes10.4028/www.scientific.net/AMM.592-594.240 ↗
21. Characterization of magnetically impelled arc butt welded T11 tubes for high pressure applications10.1016/j.dt.2015.03.005 ↗
22. Experimental investigations on magnetically impelled arc butt welded T91 steel tubes10.1007/s12666-017-1086-x ↗
23. Dynamic control of welding current and welding time to investigate ultimate tensile strength of MIAB welded T11 tubes10.1016/j.jmapro.2018.03.031 ↗
24. Numerical and experimental investigation of residual stresses in magnetically impelled arc butt welded joints in low alloy steels10.1007/s00170-018-1865-5 ↗
25. The Detectability of welding defects in MIAB welded thin-walled tubular components by immersion ultrasonic technique10.1007/s10921-020-00684-3 ↗
26. Light band zone formation and its influence on properties of magnetically impelled arc butt (MIAB) welded carbon steel tubes10.1007/s12666-017-1185-8 ↗
27. A new ferritic-martensitic stainless steel constitution diagram
28. Effect of cooling rate and vanadium content on the microstructure and hardness of medium carbon forging steel10.1016/j.jmst.2016.01.006 ↗