Abstract To enhance the mechanical reliability without sacrificing the electrical conductivity of the flexible electronics, in this work submicron-thick Cu/Au/PI (CAP) and graphene/Cu/Au/PI (GCAP) films were fabricated successfully by using a series of assembly methods through introducing a graphene passivation layer onto the polyimide (PI)-supported Cu film surface, and a nanoscale gold (Au) interlayer between the Cu/PI interface. Tensile testing results reveal that the yield strength, the fracture strain and the electrical properties of the GCAP film were improved simultaneously. Furthermore, the GCAP film also exhibited a higher fatigue strength than the CAP film. The basic mechanism is mainly attributed to the effective suppression of the Cu/graphene interface on the fatigue extrusion formation through constraining dislocation motion.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced Sensor and Energy Harvesting Materials · Nanomaterials and Printing Technologies · Graphene research and applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (61)

Show source-provided references
1. Fatigue of metals at nanoscale: metal thin films and conductive interconnects for flexible device application10.1016/j.nanoms.2019.02.003 ↗
2. Flexible electronics: stretchable electrodes and their future10.1002/adfm.201805924 ↗
3. Flexible electrodes for sodium-ion batteries: recent progress and perspectives10.1002/adma.201703012 ↗
4. Deformation-mechanism dependent stretchability of nanocrystalline gold films on flexible substrates10.1557/jmr.2017.349 ↗
5. Ductility of thin metal films on polymer substrates modulated by interfacial adhesion10.1016/j.ijsolstr.2006.07.022 ↗
6. Strengthening materials by engineering coherent internal boundaries at the nanoscale10.1126/science.1159610 ↗
7. High ductility of a metal film adherent on a polymer substrate10.1063/1.2108110 ↗
8. Microstructural parameters from X-ray diffraction peak broadening10.1016/j.scriptamat.2004.05.007 ↗
9. Impact of deposition conditions on the crystallization kinetics of amorphous GeTe films10.1007/s10853-015-9493-z ↗
10. On the microstructure of nanoporous gold: an X-ray diffraction study10.1021/nl803799q ↗
11. Quantitative microstructural imaging by scanning Laue x-ray micro- and nanodiffraction10.1557/mrs.2016.97 ↗
12. Probing phase transformations and microstructural evolutions at the small scales: synchrotron X-ray microdiffraction for advanced applications in 3D IC (integrated circuits) and solar PV (photovoltaic) devices10.1007/s11664-016-5012-5 ↗
13. Progress of in situ synchrotron X-ray diffraction studies on the mechanical behavior of materials at small scales10.1016/j.pmatsci.2018.01.004 ↗
14. Synchrotron X-ray micro-diffraction – probing stress state in encapsulated thin silicon solar cells10.1016/j.proeng.2015.09.241 ↗
15. Probing stress states in silicon nanowires during electrochemical lithiation using in situ synchrotron X-ray microdiffraction10.3389/fenrg.2018.00019 ↗
16. Plasticity evolution in nanoscale Cu/Nb single-crystal multilayers as revealed by synchrotron X-ray microdiffraction10.1016/j.msea.2015.03.067 ↗
17. Nano-structuration effect on the mechanical behavior of gold thin films studied by 2D synchrotron x-ray diffraction10.1016/j.surfcoat.2016.08.097 ↗
18. In situ monitoring of X-ray strain pole figures of a biaxially deformed ultra-thin film on a flexible substrate10.1107/S1600576713030720 ↗
19. Metal films on polymer substrates stretched beyond 50%10.1063/1.2817234 ↗
20. Effect of film thickness and grain size on fatigue-induced dislocation structures in Cu thin films10.1080/0950083031000151383 ↗
21. Damage behavior of 200-nm thin copper films under cyclic loading10.1557/JMR.2005.0019 ↗
22. Length-scale-controlled fatigue mechanisms in thin copper films10.1016/j.actamat.2006.03.013 ↗
23. Effect of length scale on fatigue life and damage formation in thin Cu films10.1016/j.msea.2007.06.092 ↗
24. Grain boundary instability dependent fatigue damage behavior in nanoscale gold films on flexible substrates10.1016/j.msea.2017.07.006 ↗
25. Nanotwin-assisted grain growth in nanocrystalline gold films under cyclic loading10.1038/ncomms4021 ↗
26. Tensile and fatigue strength of ultrathin copper films10.1016/j.msea.2007.02.132 ↗
27. Enhancing fatigue cracking resistance of nanocrystalline Cu films on a flexible substrate10.1016/j.msea.2014.12.098 ↗
28. Influences of Ta passivation layers on the fatigue behavior of thin Cu films10.1016/j.msea.2014.05.024 ↗
29. Transfer of large-area graphene films for high-performance transparent conductive electrodes10.1021/nl902623y ↗
30. Ultratransparent and stretchable graphene electrodes10.1126/sciadv.1700159 ↗
31. Characterization techniques for graphene-based materials in catalysis10.3934/matersci.2017.3.755 ↗
32. Mechanical and electrical properties of copper-graphene nanocomposite fabricated by high pressure torsion10.1016/j.jallcom.2018.10.139 ↗
33. Nanocarbon-reinforced metal-matrix composites for structural applications10.1557/mrs.2018.321 ↗
34. Ultrahigh electrical conductivity of graphene embedded in metals10.1002/adfm.201806792 ↗
35. Strengthening effect of single-atomic-layer graphene in metal-graphene nanolayered composites10.1038/ncomms3114 ↗
36. Graphene coating makes copper more resistant to plastic deformation10.1016/j.coco.2019.01.006 ↗
37. Role of graphene in reducing fatigue damage in Cu/gr nanolayered composite10.1021/acs.nanolett.7b01431 ↗
38. Bilayer graphene-covered Cu flexible electrode with excellent mechanical reliability and electrical performance10.1557/jmr.2019.290 ↗
39. Tensile and fatigue properties of free-standing Cu foils
40. Optimizing fatigue performance of nacre-mimetic PE/TiO2 nanolayered composites by tailoring thickness ratio10.1557/jmr.2018.134 ↗
41. A novel evaluation strategy for fatigue reliability of flexible nanoscale films10.1088/2053-1591/aab1c5 ↗
42. Gamburg · 2011
43. On the applicability of the x-ray diffraction line profile analysis in extracting grain size and microstrain in nanocrystalline materials10.1557/JMR.1999.0079 ↗
44. Optimized poly(methyl methacrylate)-mediated graphene-transfer process for fabrication of high-quality graphene layer10.1088/1361-6528/aad4d9 ↗
45. Conductivity and thermal studies of blend polymer electrolytes based on PVAc–PMMA10.1016/j.ssi.2006.04.013 ↗
46. Large-area synthesis of high-quality and uniform graphene films on copper foils10.1126/science.1171245 ↗
47. The effect of film thickness on the failure strain of polymer-supported metal films10.1016/j.actamat.2009.11.010 ↗
48. Metal-graphene interfaces in epitaxial and bulk systems: a review10.1016/j.pmatsci.2020.100652 ↗
49. Strengthening and deformation mechanisms in nanolaminated graphene-Al composite micro-pillars affected by graphene in-plane sizes10.1016/j.ijplas.2019.01.006 ↗
50. Mechanical properties of bilayer graphene with twist and grain boundaries10.1063/1.4789594 ↗
51. Strengthening and toughening mechanisms in graphene-Al nanolaminated composite micro-pillars10.1016/j.actamat.2016.11.043 ↗
52. Thermomechanical behavior of different texture components in Cu thin films10.1016/S1359-6454(01)00127-6 ↗
53. Achieving high strength and high ductility in metal matrix composites reinforced with a discontinuous three-dimensional graphene-like network10.1039/C6NR07335B ↗
54. Fatigue behavior of polycrystalline thin copper films10.3139/146.020392 ↗
55. Hirth · 1982
56. Cyclic deformation of polycrystalline Cu films10.1080/0141861021000056690 ↗
57. High cycle fatigue of thin silver films investigated by dynamic microbeam deflection10.1016/S1359-6462(99)00231-6 ↗
58. Size effects in the fatigue behavior of thin Ag films10.1016/S1359-6454(02)00391-9 ↗
59. Ab initio study of stability and migration of point defects in copper-graphene layered composite10.1016/j.jallcom.2016.08.311 ↗
60. Radiation resistant vanadium-graphene nanolayered composite
61. The influence of Cu–Nb interfaces on local vacancy concentrations in Cu10.1016/j.scriptamat.2013.03.019 ↗