Effect of arc pulsing in gas tungsten arc welding on microstructure and mechanical properties of Ti–6Al–4V-2.5Cu
Source abstract
Abstract
Abstract In the present study, a copper modified titanium alloy (Ti–6Al–4V–2.5Cu) was prepared by using vacuum arc re-melting and processed successfully by hot forging and rolling. The alloy was subjected to solution treatment (ST) at two temperatures, viz. 900 °C and 1010 °C followed by low temperature ageing at 500 °C. The weldments were fabricated from the alloy by using gas tungsten arc welding (GTAW) in continuous current (CC) and pulsed current (PC) modes. The effect of heat treatment and welding mode with and without post weld heat treatment (PWHT) on microstructure, hardness and tensile properties has been studied and compared. Pulsing of current during GTAW prompted in refinement of grains. While CC weldments showed coarser columnar grains, PC weldments reveal finer equiaxed β grains. Ageing and PWHT caused the formation of Ti2Cu intermetallic precipitates in the base alloy as well as in weldments. While the grain refinement in PC weldments manifested in higher strength and percent elongation relative to that of CC weldments, the higher improvement of strength in PWHT condition is due to the combination of both grain refinement and presence of Ti2Cu precipitates. However, the base metal evidenced the better strength properties in both heat treatment conditions than the weldments.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Titanium Alloys Microstructure and Properties · Welding Techniques and Residual Stresses · Advanced Welding Techniques Analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (16)
Show source-provided references
1. Effect of Ti2Cu precipitates on mechanical behavior of Ti–2.5Cu alloy subjected to different heat treatments10.1016/j.jallcom.2009.04.095 ↗
2. Mechanical behavior and deformation mechanism of Ti-2.5Cu alloy reinforced by nano scale precipitates at 293 and 77 K10.1016/j.msea.2003.08.015 ↗
3. Microstructure and mechanical properties of a copper containing three phase titanium alloy10.1016/j.msea.2011.05.080 ↗
4. Influence of welding processes on microstructure, tensile and impact properties of Ti-6Al-4V alloy joints10.1016/S1003-6326(11)60850-9 ↗
5. Effect of current pulsing on tensile properties of titanium alloy10.1016/j.matdes.2007.07.007 ↗
6. Weld microstructure refinement in a 1441 grade aluminium–lithium alloy10.1023/A:1018662126268 ↗
7. Effect of pulsed current on temperature distribution, weld bead profiles and characteristics of gas tungsten arc welded aluminum alloy joints10.1016/S1003-6326(11)60710-3 ↗
8. Effect of pulsed current and post weld aging treatment on tensile properties of argon arc welded high strength aluminium alloy10.1016/j.msea.2006.12.125 ↗
9. Effect of arc vibration and current pulses on microstructure and mechanical properties of TIG tantalum welds10.1179/mt.1978.5.1.190 ↗
10. Microstructural refinement of weld fusion zones in α-β titanium alloys using pulsed current welding10.1016/S0921-5093(98)01010-7 ↗
11. Microstructure evolution and fracture behaviour for electron beam welding of Ti–6Al–4V10.1007/BF02704777 ↗
12. Formation of α Widmanstatten structure: effects of grain size and cooling rate on the Widmanstatten morphologies and on the mechanical properties in Ti6Al4V alloy10.1016/S0925-8388(01)01571-7 ↗
13. A novel Ti-6Al-4V alloy microstructure with very high strength and good ductility10.1016/j.scriptamat.2015.05.008 ↗
14. A comparative evaluation of laser and gas tungsten arc weldments in high-temperature titanium alloys
15. Advances in titanium alloy welding metallurgy
16. Welding of Ti-6Al-4V alloy using dynamically controlled plasma arc welding process10.1016/S1003-6326(11)60888-1 ↗