Mechanical behavior of the joints between carbon/carbon composites and Li2O–Al2O3–SiO2 glass ceramics with YAS interlayer at high temperature
Source abstract
Abstract
Abstract YAS (Y2O3–Al2O3–SiO2) glass ceramics were selected to join carbon/carbon (C/C) composites and Li2O–Al2O3–SiO2 (LAS) glass ceramics through vacuum hot-pressing sintering, due to the corresponding excellent compositional and structural stability at high temperature. Microstructures, mechanical properties and fracture features of the C/C-LAS joints were investigated. The joints with YAS interlayer exhibited more favorable results than the joints with MAS (MgO–Al2O3–SiO2) interlayer subsequently to shear testing at 300 and 600 °C. Strength retention of 70% for YAS joints was achieved at 600 °C, while for MAS joints the strength retention was only 28%. The joining properties amount decrease of YAS joints was due to degradation of the intrinsic properties of YAS and LAS glass ceramics. Regarding MAS joints, the poor structural stability of MAS interlayer at high temperature was the reason for the corresponding decrease. As a result, the mechanical behavior of joints at elevated temperatures was not only related to wettability and interfacial bonding, but it was also related to the intrinsic properties as well as to high-temperature stability of the interlayer and the joined substrates.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Bone Tissue Engineering Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (33)
Show source-provided references
1. Carbon nanotube/carbon composite fiber with improved strength and electrical conductivity via interface engineering10.1016/j.carbon.2018.12.091 ↗
2. Realizing the synergy of carbon nanotubes and matrix microstructure for improved flexural behavior of laminated carbon/carbon composites10.1016/j.jallcom.2017.12.111 ↗
3. Flexible SiC-nanowire membrane reinforced pyrocarbon profiled joints with significantly improved thermal shock resistance10.1016/j.ceramint.2018.10.137 ↗
4. Influence of cryogenic thermal cycling treatment on the thermophysical properties of carbon/carbon composites between room temperature and 1900 °C10.1016/j.jmst.2017.03.001 ↗
5. Application of mesophase pitchbased carbon fibers reinforced C/C composites in hypersonic vehicles
6. Pre-infiltration and brazing behaviors of Cf/C composites with high temperature Ti–Si eutectic alloy10.1016/j.carbon.2018.08.021 ↗
7. J. Feng. C/SiC composite-Ti6Al4V joints brazed with negative thermal expansion ZrP2WO12 nanoparticle reinforced AgCu alloy10.1016/j.jeurceramsoc.2018.12.028 ↗
8. Combustion joining of carbon–carbon composites to TiAl intermetallics using a Ti–Al–C powder composite interlayer10.1016/j.compscitech.2015.05.001 ↗
9. Joining of SiC nanowires-toughened SiC coated C/C composites and nickel based superalloy (GH3044) using Ni71CrSi interlayer10.1016/j.jallcom.2016.09.245 ↗
10. The preparation and mechanical properties of Carbon/Carbon Composite (C/C) and Carbon fiber reinforced silicon carbide Composite (Cf/SiC) joint by Transient Liquid Phase (TLP) diffusion bonding process with Ti/Ni/Ti multiple foils10.1016/j.vacuum.2018.09.045 ↗
11. Antimicrobial and bioactive phosphate-free glass–ceramics for bone tissue engineering applications10.1016/j.msec.2018.01.002 ↗
12. 45S5 bioglass-derived glass-ceramic scaffolds for bone tissue engineering10.1016/j.biomaterials.2005.11.025 ↗
13. Survival of dicor glass-ceramic dental restorations over 14 years: part i. survival of dicor complete coverage restorations and effect of internal surface acid etching, tooth position, gender, and age10.1016/S0022-3913(99)70231-3 ↗
14. SiO2-SnO2: Er3+ glass-ceramic monoliths10.3390/app8081335 ↗
15. Tb3+ -doped BaF2 -Al2O3 -B2O3, glass and glass-ceramic for radiation measurements10.1016/j.jnoncrysol.2018.02.013 ↗
16. Chalcogenide glass-ceramic with self-organized heterojunctions: application to photovoltaic solar cells
17. Mechanical milling assisted synthesis of novel LiTi2(PO4)3 -glass-ceramic nanocomposites10.1016/j.jnoncrysol.2018.01.016 ↗
18. Enhancement of C/C-LAS joint using aligned carbon nanotubes prepared by injection chemical vapor deposition10.1016/j.msea.2015.10.003 ↗
19. Construction of SiCnw/MAS nanocomposites to strengthen and toughen C/C-LAS joints10.1016/j.msea.2017.06.059 ↗
20. Enhancement of C/C-LAS joint using aligned carbon nanotubes prepared by injection chemical vapor deposition10.1016/j.msea.2015.10.003 ↗
21. Significant influence of Al2O3 on the flexural properties of C/C composites10.1016/j.vacuum.2018.02.036 ↗
22. Zhou · 2013
23. Influences of SiCf content and length on the strength, toughness and dielectric properties of SiCf/LAS glass-ceramic composites10.1016/j.ceramint.2012.09.094 ↗
24. The preparation and mechanical properties of carbon–carbon/lithium–aluminum–silicate composite joints10.1016/j.matdes.2012.07.060 ↗
25. Protective coatings for carbon bonded carbon fibre composites10.1016/j.ceramint.2007.03.012 ↗
26. A gradient LMAS interlayer joint of SiC coated C/C composites to LAS glass ceramics10.1016/j.ceramint.2013.08.021 ↗
27. Study on oxidation mechanism of two-dimensional carbon/carbon composites
28. Segregation behavior and evolution mechanism of iron-rich phases in molten magnesium alloys10.1016/j.jmst.2015.10.013 ↗
29. Effects of elements-doping on the crystal structure and thermal expansion coefficient of cordierite
30. Joining of SiC-based materials for nuclear energy applications10.1016/j.jnucmat.2010.12.160 ↗
31. Wide applicability10.1115/1.4010337 ↗
32. Ultrasonic non destructive evaluation of microstructural changes and degradation of ceramics at high temperature10.1557/PROC-142-263 ↗
33. Structural changes of B2O3 through the liquid-glass transition range: a Raman-scattering study10.1103/PhysRevB.45.12797 ↗