journal article·2018-07

Twin induced fracture toughness in SiCW/SiC composites processed by spark plasma sintering

Mangesh Lodhe, G. Logesh, M. Balasubramanian

Publisher page

Abstract

Abstract The twin boundaries (TBs) was responsible for 30% and 26% enhancement in the fracture toughness of 10% and 20% SiCW/SiC composites spark plasma sintered at 1800 °C, respectively. Crack deflection at TBs, and daughter crack formation at the twin zone were found to be the responsible mechanisms for twin toughening.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (16)

Show source-provided references
1. An extended hardness limit in bulk nanoceramics10.1016/j.actamat.2014.01.030 ↗
2. Enhancing the age-hardening response of rolled AZ80 alloy by pre-twinning deformation10.1016/j.msea.2016.10.094 ↗
3. Crystal plasticity modeling and characterization of the deformation twinning and strain hardening in Hadfield steels10.1016/j.msea.2018.02.028 ↗
4. The role of dislocations in strain hardening of an extension twinning predominant deformation10.1016/j.msea.2015.04.007 ↗
5. Superior thermal stability of coherent twin boundaries in nanotwinned metals10.1016/j.scriptamat.2012.01.026 ↗
6. Enhanced fracture toughness of bulk nanocrystalline Cu with embedded nanoscale twins10.1016/j.scriptamat.2008.12.012 ↗
7. Ultrahard nanotwinned cubic boron nitride10.1038/nature11728 ↗
8. Nanotwin-governed toughening mechanism in hierarchically structured biological materials10.1038/ncomms10772 ↗
9. In-situ observations of deformation twins and crack propagation in a CoCrFeNiMn high-entropy alloy10.1016/j.msea.2018.01.121 ↗
10. Effects of nano-graphite content on the characteristics of spark plasma sintered ZrB2–SiC composites10.1016/j.msea.2018.01.038 ↗
11. Modification and toughening of 3D needled C/SiC composite by deformable MAX phase-based matrix10.1016/j.msea.2017.11.110 ↗
12. Effect of heat treatment on microstructure and mechanical properties of PIP-SiC/SiC composites10.1016/j.msea.2012.09.027 ↗
13. A fracture mechanics analysis of indentation-induced {Palmqvist} cracks in ceramics10.1007/BF00725625 ↗
14. Twinning induced enhancement of fracture toughness in ultrafine grained hydroxyapatite–calcium titanate composites10.1016/j.jeurceramsoc.2015.10.044 ↗
15. Mechanical characterization of fine grained silicon carbide consolidated using polymer pyrolysis and spark plasma sintering10.1016/j.ceramint.2014.04.048 ↗
16. Toughening behavior in whisker-reinforced ceramic matrix composites10.1111/j.1151-2916.1988.tb05791.x ↗