Abstract
Abstract Fusing of bonding interface which could lead to the combination of grains at the both sides of bonding interface, and transition of bonding interface into grain boundary occurred during heating. Both they could strengthen interface bonding, and interface bonding strength was more than doubled after heating for 6 h.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced Welding Techniques Analysis · Aluminum Alloys Composites Properties · Aluminum Alloy Microstructure Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (10)
Show source-provided references
1. Evaluation of copper coating ratio in steel/copper clad wire drawing10.1016/j.jmatprotec.2006.11.131 ↗
2. Effects of annealing process on interface and mechanical properties of silver clad aluminum wires10.1016/j.proeng.2011.12.479 ↗
3. Study of the intermetallic growth in copper-clad aluminum wires after thermal aging10.1016/j.intermet.2014.02.007 ↗
4. Failure analysis of aluminum cable steel reinforced (ACSR) conductor of the transmission line crossing the Parana River10.1016/S1350-6307(02)00021-3 ↗
5. Electrical conductibility of copper clad steel wire by drawing at room temperature10.4028/www.scientific.net/KEM.334-335.321 ↗
6. Development of an 8090/3003 bimetal slab using a modified direct-chill casting process10.1016/j.jmatprotec.2014.03.029 ↗
7. Damage investigation of the aged aluminium cable steel reinforced (ACSR) conductors in a high-voltage transmission line10.1016/j.engfailanal.2011.09.002 ↗
8. Numerical analyses of cladding processes by twin-roll casting: Mg-az31 with aluminum alloys10.1016/j.ijheatmasstransfer.2015.10.002 ↗
9. Interfacial diffusion reaction and mechanical characterization of 316L stainless steel-hydroxyapatite functionally graded materials for joint prostheses10.1016/j.ceramint.2015.07.082 ↗
10. Microstructure evolution and properties of Al/Al–Mg–Si alloy clad wire during heat treatment10.1007/s00339-016-0150-4 ↗