Cyclic deformation responses in α-phase of a lamellar near β-Ti alloy
Source abstract
Abstract
Abstract A lamellar near β-Ti alloy was subjected to cyclic tensile loading at room temperature. Transmission electron microscopy (TEM) and high resolution TEM (HRTEM) investigation revealed that the deformation mechanisms of α-phase were found to be changing with increasing loading cycles, from mechanical twinning to martensite transformation. To be specific, at the beginning of straining, the formation of mechanical α-twins was the dominant deformation mechanism to accommodate the applied strain. As the increasing cycles, the secondary twin and hierarchical structure formed in α laths. During further straining, the noticeable groove was observed at the α/β grain boundary. Meanwhile, dispersed nanosized α" martensite phase formed in the α plate and the number of α-twins sharply decreased at this stage. This work will provide a basis for the enhancement of load bearing capabilities of near β-Ti alloys.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Titanium Alloys Microstructure and Properties · Microstructure and Mechanical Properties of Steels · Microstructure and mechanical properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (25)
Show source-provided references
1. Cyclic deformation response and micromechanisms of Ti alloy Ti–5Al–5V–5Mo–3Cr–0.5Fe10.1016/j.msea.2011.08.045 ↗
2. Cyclic deformation response of β-Annealed Ti–5Al–5V–5Mo–3Cr alloy under compressive loading conditions10.1007/s11661-011-0705-0 ↗
3. On the role of twinning and stacking faults on the crystal plasticity and grain refinement in magnesium alloys10.1016/j.actamat.2017.11.004 ↗
4. Twinning-induced softening in polycrystalline AM30 Mg alloy at moderate temperatures10.1016/j.scriptamat.2005.11.029 ↗
5. Secondary twin variant selection in four types of double twins in titanium10.1016/j.actamat.2018.03.068 ↗
6. Deformation-induced variations in microstructure evolution and mechanical properties of bi-modal Ti-55511 titanium alloy10.1016/j.jallcom.2018.12.262 ↗
7. Origin of the twinning to slip transition with grain size refinement, with decreasing strain rate and with increasing temperature in magnesium10.1016/j.actamat.2015.01.032 ↗
8. 2012
9. Temperature dependency of slip and twinning in plane strain compressed magnesium single crystals10.1016/j.actamat.2010.11.064 ↗
10. On the {101¯1}twin-accommodated mechanisms in equiaxed near β-Ti alloys operating by unidirectional and cross rolling10.1016/j.msea.2019.138516 ↗
11. Comparing the evolution and deformation mechanisms of lamellar and equiaxed microstructures in near β-Ti alloys during hot deformation10.1016/j.msea.2019.05.015 ↗
12. Role of martensite decomposition in tensile properties of selective laser melted Ti–6Al–4V10.1016/j.jallcom.2018.02.111 ↗
13. Room-temperature ductility of Ti–6Al–4V alloy with αʹ martensite microstructure10.1016/j.msea.2006.11.022 ↗
14. Stress accommodation by α to α" transformation at the {101¯1}twin boundary in a cold-rolled Ti-5at.% Al alloy10.1016/j.mtla.2019.100469 ↗
15. Effect of strain ratio and strain rate on low cycle fatigue behavior of AZ31 wrought magnesium alloy10.1016/j.msea.2009.04.051 ↗
16. Investigation of early stage deformation mechanisms in a metastable β titanium alloy showing combined twinning-induced plasticity and transformation-induced plasticity effects10.1016/j.actamat.2013.07.019 ↗
17. Achieving high strength and ductility in magnesium alloys via densely hierarchical double contraction nanotwins10.1021/acs.nanolett.7b02641 ↗
18. Interactive contraction nanotwins-stacking faults strengthening mechanism of Mg alloys10.1016/j.actamat.2019.02.040 ↗
19. The effect of grain size on the twin initiation stress in a TWIP steel10.1016/j.actamat.2015.02.008 ↗
20. Kinetics of strain-induced martensitic nucleation10.1007/BF02672301 ↗
21. Origin of shear induced b to u transition in TieNb-based alloys10.1016/j.actamat.2015.03.040 ↗
22. Reversible displacive transformation with continuous transition interface in a metastable b titanium alloy10.1016/j.actamat.2019.05.045 ↗
23. Grain size and reversible beta-to-omega phase transformation in a Ti alloy10.1016/j.scriptamat.2010.05.045 ↗
24. Relationship between fatigue crack initiation and activated {101¯1}twins in as-extruded pure magnesium10.1016/j.scriptamat.2013.08.006 ↗
25. The room temperature tensile deformation behavior of thermomechanically processed β-metastable Ti-Nb-Ta-Zr bio-alloy: the role of deformation-induced martensite10.1016/j.msea.2018.09.038 ↗