Abstract
Abstract The deleterious effect of hydrogen on steel is a long-standing problem. Embrittlement in the presence of hydrogen is, in part, a consequence of the fast diffusion of hydrogen in ferritic steels. Because of the identical chemical properties but large differences in mass between hydrogen isotopes, interaction of hydrogen isotopes with steel structures are of interest as a tool to study the role of diffusion in hydrogen embrittlement under all-else-equal conditions. In this paper, we present tensile and fatigue data for steel samples measured in air, in hydrogen, and in deuterium. Tensile measurements show deuterium causes a loss of ductility comparable to the loss due to hydrogen. In fatigue, a large pressure effect on deuterium-assisted fatigue crack growth was observed, an effect which is not exhibited in uniaxial tensile measurements. With sufficient pressure to show an enhanced fatigue crack growth effect, the fatigue crack growth rate is well-predicted assuming a scaling of the diffusion coefficient by 1 / 2 . These results suggest surface adsorption kinetics play a large role in hydrogen-assisted fatigue crack growth at low pressure. At higher pressures, hydrogen-assisted fatigue crack growth is primarily affected by the kinetics of diffusion of hydrogen within the steel lattice.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Nuclear Materials and Properties · Fatigue and fracture mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (41)
Show source-provided references
1. On some remarkable changes produced in iron and steel by the action of hydrogen and acids
2. Fatigue crack growth of two pipeline steels in a pressurized hydrogen environment10.1016/j.corsci.2013.10.014 ↗
3. A review of fatigue crack growth for pipeline steels exposed to hydrogen10.6028/jres.115.030 ↗
4. Comparison of hydrogen embrittlement in three pipeline steels in high pressure gaseous hydrogen environments10.1016/j.corsci.2012.01.028 ↗
5. Modeling the fatigue crack growth of x100 pipeline steel in gaseous hydrogen10.1016/j.ijfatigue.2013.08.010 ↗
6. Effect of hydrogen and low temperature on fatigue crack growth of pipeline steels10.1016/j.engfracmech.2012.09.023 ↗
7. A study of embrittlement of high strength steels by hydrogen isotopes i. testing of steel rings as specimens, a comparison of hydrogen and deuterium embrittlement, and permeation studies10.1149/1.2425892 ↗
8. Ratio of the diffusion coefficients for the diffusion of hydrogen and deuterium in steel10.1063/1.1723325 ↗
9. Observation of trapping sites of hydrogen and deuterium in high-strength steels by using secondary ion mass spectrometry10.2320/matertrans1989.36.1134 ↗
10. Deuterium concentration profiles in Fe Ni Co alloys electrochemically charged at room temperature10.1016/0001-6160(89)90286-1 ↗
11. A sims study of the diffusion and trapping of deuterium in 302 stainless steel10.1007/BF02644422 ↗
12. Deuterium transport and trapping in aluminum alloys10.1007/BF02664813 ↗
13. ASTM Standard E415 · 2015
14. ASTM Standard E1019 · 2018
15. ASTM Standard E647, 2015e1 · 2004
16. ASTM Standard E8 · 2016
17. Effects of hydrogen pressure, test frequency and test temperature on fatigue crack growth properties of low-carbon steel in gaseous hydrogen10.1016/j.prostr.2016.06.068 ↗
18. Recent advances on hydrogen embrittlement of structural materials10.1007/s10704-015-0068-4 ↗
19. An adsorption study of hydrogen on iron and its relation to hydrogen embrittlement10.1007/BF02661209 ↗
20. The isothermal kinetics of hydrogen adsorption onto iron films observed with the chemisorption-induced resistance change10.1016/0039-6028(85)90658-2 ↗
21. Gas phase reactions of iron clusters with hydrogen. i. kinetics10.1063/1.448901 ↗
22. The dissociation energies of the H2, HD, and D2 molecules10.1016/0022-2852(61)90111-4 ↗
23. Nelson · 1973
24. Das absorptionsvermögen des festen kobaltes für wasserstoff und stickstoff10.1515/zpch-1934-16927 ↗
25. Review of recent studies on the mechanism of stress-corrosion cracking in austenitic stainless steels
26. Mechanics and thermodynamics on the stress and hydrogen interaction in crack tip stress corrosion: experiment and theory10.1016/S0022-5096(97)00054-9 ↗
27. Hydrogen and deuterium in iron, 49–506 c10.1016/0001-6160(78)90041-X ↗
28. Anderson · 2017
29. Crank · 1979
30. McCarty · 1981
31. Chapman · 1970
32. Hydrogen-enhanced plasticity and failure revisited 2012
33. Interpretation of hydrogen-assisted fatigue crack propagation in bcc iron based on dislocation structure evolution around the crack wake10.1016/j.actamat.2018.06.041 ↗
34. Milne · 2003 · vol. 4
35. Moody · 2003
36. Gangloff · 2006
37. Hydrogen-induced intergranular fracture of steels10.1016/S0013-7944(00)00124-7 ↗
38. Gangloff · 1990
39. The effect of hydrogen on dislocation dynamics10.1016/S0013-7944(01)00011-X ↗
40. Hydrogen-enhanced localized plasticitya mechanism for hydrogen-related fracture10.1016/0921-5093(94)90975-X ↗
41. Hydrogen-assisted fatigue crack growth in structural steel