Thermo-mechanical processing, microstructure and mechanical properties of TiZrB alloy

Chaoqun Xia, Xing Zhang, Shuguang Liu, Bohan Chen, Chunlin Tan, Xinyu Zhang, Mingzhen Ma, Riping Liu

Publisher page

Abstract

Abstract This work was aimed in the relationships investigation among the microstructure, the tensile properties and the thermo-mechanical processing of a novel Ti-25Zr-1B (wt%) alloy. The alloy was evaluated under different conditions (as-cast, hot-rolled and hot-rolled-annealed). The XRD diagrams demonstrated that all specimens were completely consisted of the α and TiB phases. The results of EDS indicated that the TiB phase dissolved a certain amount of Zr, which was in agreement with the existence of TiB peaks shifting towards lower diffraction angles. The as-cast Ti-25Zr-1B alloy microstructure and the size, the morphology, the orientation, and the distribution of the TiB particles could be significantly altered by the hot-rolling process. The hot-rolling process provided an ultimate strength increase of at least 7 pct and the elongation-to-failure increase of 135 pct relatively to the as-cast sample. In addition, the annealing heat treatment could effectively modify the mechanical properties of the hot-rolled sample. The strength decreased and the elongation-to-failure increased as the annealing temperature increased, while the temperature was below 800 °C. In contrast, as the annealing temperature increased to 900 °C, the alloy demonstrated appreciably lower elongation-to-failure and higher strength compared to the annealed form at 800 °C. The mechanical properties variation of the Ti-25Zr-1B alloy series was ascribed to the microstructure evolution of the matrix alloy as well as to the morphology and volume fraction changes of the TiB particles.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Titanium Alloys Microstructure and Properties · Intermetallics and Advanced Alloy Properties · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (31)

Show source-provided references
1. Microstructural effects on the mechanical behavior of B-modified Ti-6Al-4V alloys10.1016/j.actamat.2007.05.009 ↗
2. Importance of slip mode for dispersion-hardened β-Titanium alloys10.1007/BF02643096 ↗
3. Modification of alpha morphology in Ti-6Al-4V by thermomechanical processing10.1007/BF02644991 ↗
4. Effect of zirconium content on the microstructure and corrosion behavior of Ti-6Al-4V-xZr alloys10.1016/j.corsci.2016.09.012 ↗
5. Effects of chromium addition on structure and mechanical properties of Ti-10Zr alloy10.1016/j.jallcom.2009.04.148 ↗
6. Shape memory behavior in Ti-Zr alloys10.1016/j.scriptamat.2010.11.048 ↗
7. The effect of the solute on the structure, selected mechanical properties, and biocompatibility of Ti–Zr system alloys for dental applications10.1016/j.msec.2013.09.032 ↗
8. Phase Diagrams of Binary Titanium Alloys
9. Influence of martensitic transformation on mechanical compatibility of biomedical β type titanium alloy TLM10.1016/j.msea.2005.12.079 ↗
10. Thermal expansion and microstructural analysis of experimental metal-ceramic titanium alloys10.1016/S0022-3913(03)00493-1 ↗
11. Grain refinement of cast titanium alloys via trace boron addition10.1016/j.scriptamat.2005.08.020 ↗
12. Effect of Minor Additions of Boron on Microstructure and Mechanical Properties of As-Cast Near α Titanium Alloy10.1007/s11661-009-0155-0 ↗
13. Microstructure and texture evolution during β extrusion of boron modified Ti–6Al–4V alloy10.1016/j.msea.2012.01.120 ↗
14. Effects of boron on the fracture behavior and ductility of cast Ti-6Al-4V alloys10.1016/j.scriptamat.2014.12.022 ↗
15. 1990 · 547
16. T.E. Eckert, AFML TR-65-2, Part II, Vol. XII, Wright Patterson AFB, Ohio, 1966.
17. ASM Alloy Phase Diagrams Center, 2007, in: E. Rudy, Ti-Zr-B System, Compendium of Phase Diagram Data, Ternary Phase Equilibria in TM-B-C-Si, E. Rudy 528-547, 1969.
18. Structure and mechanical properties of as-cast (ZrTi)100-xBx alloys10.1016/j.jallcom.2015.02.204 ↗
19. Processing, microstructure, texture, and tensile properties of the Ti-6Al-4V-1.55B eutectic alloy, metall10.1007/s11661-007-9425-x ↗
20. A novel Ti-6Al-4V alloy microstructure with very high strength and good ductility10.1016/j.scriptamat.2015.05.008 ↗
21. The structure and mechanical properties of as-cast Zr-Ti alloys10.1016/j.jallcom.2009.08.105 ↗
22. Development of solidfication microstructure in boron-modified alloy Ti-6Al-4V-0.1B10.1016/j.actamat.2011.05.023 ↗
23. Effect of boron on the beta transus of Ti-6Al-4V alloy10.1016/j.scriptamat.2005.03.038 ↗
24. Effects of boron on microstructure in cast titanium alloys10.1016/j.scriptamat.2008.05.002 ↗
25. Nucleation and growth mechanism of α-lamellae of Ti alloy TA15 cooling from an α+β phase field10.1016/j.actamat.2012.12.025 ↗
26. Effect of hot forging on microstructure and tensile properties of Ti-TiB based composites produced by casting10.1016/j.msea.2014.04.091 ↗
27. Effects of annealing treatments on microstructure and mechanical properties of the Zr-45Ti-5Al-3V alloy10.1016/j.msea.2013.06.007 ↗
28. Effect of the annealing temperature on the microstructural evolution and mechanical properties of TiZrAlV alloy10.1016/j.matdes.2013.06.039 ↗
29. Strength and tension/compression asymmetry in nanostructured and ultrafine-grain metals10.1016/S1359-6454(03)00286-6 ↗
30. Deformation mechanism transitions in nanoscale fcc metals10.1080/09500830310001614540 ↗
31. Effect of aspect ratios of in situ formed TiB whiskers on the mechanical properties of TiBw/Ti–6Al–4V composites10.1016/j.scriptamat.2011.12.024 ↗