journal article·2018-01

Effect of pre-deformation cooling rate on the age-hardening response of ultrafine grained AA6063

A. Yousefi, A.R. Eivani, S.M.A. Boutorabi, H.R. Jafarian

Publisher page

Abstract

Abstract In this article, effect of pre-deformation cooling rate after solution heat treatment on the evolution of microstructure and tensile properties of AA6063 aluminum alloy is investigated. For this purpose, samples of AA6063 are solution heat treated at 550 °C for 6 h. Followed by this treatment, some samples are furnace cooled (FC), some air cooled (AC) and the rest water quenched (WQ). After 2, 6 and 10 passes equal channel angular pressing (ECAP), significantly finer nanostructure was observed in the WQ samples. This was attributed to the effect of higher concentration of Mg in solid solution. In addition, the WQ samples showed higher initial tensile strength being attributed to the more enriched solid solution and more significant strengthening during severe plastic deformation which was attributed to higher dislocation density generated during deformation. In addition, it was found that the WQ samples in un-deformed and deformed conditions show a more significant response to aging in terms of strengthening. In fact, age hardening was observed for both AC and WQ samples in un-deformed condition and after 2 passes ECAP. Age hardening was as well observed in the WQ samples which were deformed for 6 and 10 passes. However, age softening was observed in the AC samples when the number of ECAP passes was increased to 6 and 10.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Microstructure and mechanical properties · Aluminum Alloys Composites Properties · Aluminum Alloy Microstructure Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (36)

Show source-provided references
1. Influence of aging parameters on the mechanical properties of 6063 aluminium alloy10.1016/S0924-0136(99)00476-8 ↗
2. The quench sensitivity of cast Al-7 wt pct Si-0.4 wt pct Mg alloy10.1007/BF02595647 ↗
3. Investigation extrusion ratio effect on mechanical behaviour of extruded alloy AA-606310.1016/S0924-0136(02)01110-X ↗
4. Quench sensitivity of a heat treatable aluminum alloy10.1016/S0921-5093(03)00616-6 ↗
5. Nanostructuring of metals by severe plastic deformation for advanced properties10.1038/nmat1180 ↗
6. Producing bulk ultrafine-grained materials by severe plastic deformation10.1007/s11837-006-0213-7 ↗
7. Bulk nanostructured materials from severe plastic deformation10.1016/S0079-6425(99)00007-9 ↗
8. Structure and properties of ultrafine-grained materials produced by severe plastic deformation10.1016/0921-5093(93)90717-S ↗
9. Developing superplastic properties in an aluminum alloy through severe plastic deformation10.1016/S0921-5093(99)00470-0 ↗
10. Nanostructure and related mechanical properties of an Al–Mg–Si alloy processed by severe plastic deformation10.1080/09500830802186938 ↗
11. Dynamic precipitation during severe plastic deformation of an Al–Mg–Si aluminium alloy10.1016/j.msea.2006.09.142 ↗
12. Nanostructured aluminium alloys produced by severe plastic deformation: new horizons in development10.1016/j.msea.2012.09.020 ↗
13. Microstructure and microhardness of an Al⍰ Fe alloy subjected to severe plastic deformation and aging10.1016/S0965-9773(98)00107-X ↗
14. Microstructure of aluminum-iron alloys subjected to severe plastic deformation10.1016/S1359-6462(98)00073-6 ↗
15. Microstructures and mechanical properties of HPT processed 6063 Al alloy10.1016/j.msea.2012.08.040 ↗
16. A DSC study on the precipitation kinetics of cryorolled Al 6063 alloy10.1016/j.matchemphys.2010.02.032 ↗
17. Effect of rolling temperature on microstructure and mechanical properties of 6063 Al alloy10.1016/j.msea.2008.03.029 ↗
18. Development of ultrafine-grained Al 6063 alloy by cryorolling with the optimized initial heat treatment conditions10.1016/j.matdes.2010.11.027 ↗
19. Influence of solutes and second phase particles on work hardening behavior of Al 6063 alloy processed by cryorolling10.1016/j.msea.2011.01.010 ↗
20. Optimization of interpass annealing for a minimum recrystallized grain size and further grain refinement towards nanostructured AA6063 during equal channel angular pressing10.1016/j.matchar.2015.12.018 ↗
21. Effect of pre-deformation thermomechanical processing on the development of ultrafine grain structure during equal channel angular extrusion10.1016/j.matdes.2015.09.161 ↗
22. Simultaneous improvements of the strength and ductility of fine-grained AA6063 alloy with increasing number of ECAP passes10.1016/j.msea.2016.05.070 ↗
23. Correlative evolution of microstructure, particle dissolution, hardness and strength of ultrafine grained AA6063 alloy during annealing10.1016/j.msea.2015.06.074 ↗
24. Effects of warm rolling and ageing after cryogenic rolling on mechanical properties and microstructure of Al 6061 alloy10.1016/j.matdes.2012.02.010 ↗
25. Effect of plastic deformation conditions on microstructural characteristics and mechanical properties of Al 6063 alloy10.1016/j.matdes.2008.09.022 ↗
26. Effect of annealing and aging treatment on mechanical properties of ultrafine grained Al 6061 alloy10.1179/174328409X443227 ↗
27. Influence of severe plastic deformation on aging effect of Al-Zn-Mg-Cu-Zr alloy10.1016/S0921-5093(97)00210-4 ↗
28. Combination of sever plastic deformation and precipitation hardening processes affecting the mechanical properties in Al–Mg–Si alloy10.1016/j.matdes.2014.12.011 ↗
29. Aging behaviour of Al-Mg-Si alloys subjected to severe plastic deformation by ECAP and cold asymmetric rolling10.1155/2011/959643 ↗
30. X-ray line broadening from filed aluminium and wolfram10.1016/0001-6160(53)90006-6 ↗
31. Verlinden · 2007
32. A. Standard, E8−04, Stand. Test Methods Tens. Test. Met. Mater. Annu. Book ASTM Stand. 3, 2004.
33. Extreme grain refinement by severe plastic deformation: a wealth of challenging science10.1016/j.actamat.2012.10.038 ↗
34. High-pressure torsion using ring specimens10.1016/j.scriptamat.2007.10.037 ↗
35. Microstructural evolution in pure aluminum processed by high-pressure torsion10.1016/j.msea.2008.03.055 ↗
36. Microstructure and mechanical properties of pure Cu processed by high-pressure torsion10.1016/j.msea.2008.06.039 ↗