On the hydrogen environment-assisted cracking resistance of a compositionally complex Co–Ni–Cr–Fe–Mo–Ti alloy
Source abstract
Abstract
Abstract The hydrogen environment-assisted cracking (HEAC) behavior of a compositionally complex Co–Ni–Cr–Mo–Fe–Ti–Al alloy (MP98T) proposed for marine fastener applications was evaluated via slow-rising stress intensity testing while immersed in 0.6 M NaCl at applied potentials ranging from −1.0 to −1.2 VSCE (vs. saturated calomel electrode). Results indicate that MP98T is resistant to HEAC at applied potentials representative of cathodic protection. In particular, minimal crack growth was observed across the tested applied potential range, which represented conditions known to promote aggressive HEAC in legacy Ni-based fastener alloys, such as Monel K-500. Measurement of the diffusible hydrogen concentration (CH,Diff) of MP98T as a function of applied potential in 0.6 M NaCl suggests this improved susceptibility may be linked to a reduced efficacy for hydrogen uptake in MP98T at hydrogen overpotentials where Monel K-500 is susceptible. Specifically, the CH,Diff of MP98T at a given applied potential was consistently observed to be less than 50% of that measured for Monel K-500.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Material Properties and Failure Mechanisms
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (92)
Show source-provided references
1. A century of Monel metal: 1906 – 2006
2. Stress corrosion cracking and hydrogen embrittlement of high-strength nonmagnetic alloys in brine
3. Studbolting experience in the underwater environment of the north sea, 17th offshore
4. The hydrogen embrittlement susceptibility of Monel alloy K-500
5. Failures of nickel/copper bolts in subsea applications
6. Effects of hydrogen on engineering properties of MONEL nickel-copper alloy K-50010.5006/0010-9312-28.2.57 ↗
7. Hydrogen embrittlement of cathodically protected subsea bolting alloys
8. Failure of Monel Ni-Cu-Al alloy K-500 bolts in seawater, mater
9. The effect of isothermal heat treatment on hydrogen environment-assisted cracking susceptibility in Monel K-50010.1016/j.msea.2019.138249 ↗
10. Measurement and modeling of hydrogen environment-assisted cracking in Monel K-50010.1007/s11661-014-2324-z ↗
11. Hydrogen diffusion and trapping in a precipitation-hardened nickel–copper–aluminum alloy Monel K-500 (UNS N05500)10.1016/j.actamat.2013.02.007 ↗
12. Measurement and modeling of hydrogen environment assisted cracking in a Ni-Cu-Al-Ti superalloy10.1007/s11661-015-3315-4 ↗
13. On the suitability of slow strain rate tensile testing for assessing hydrogen embrittlement susceptibility10.1016/j.corsci.2019.108291 ↗
14. Elucidating the loading rate dependence of hydrogen environment-assisted cracking in a Ni-Cu superalloy
15. The effect of microstructural variation on the hydrogen environment-assisted cracking of Monel K-50010.1007/s11661-016-3486-7 ↗
16. The effect of heat-to-heat variations in metallurgy and hydrogen-metal interactions on the hydrogen embrittlement of Monel K-50010.1016/j.msea.2017.07.019 ↗
17. The combined effects of hydrogen and aging condition on the deformation and fracture behavior of a precipitation-hardened nickel-base superalloy10.1016/j.actamat.2020.01.033 ↗
18. Multiscale Assessment of deformation induced by hydrogen environment-assisted cracking in a peak-aged Ni-Cu superalloy
19. Focht · 2002
20. Development of a fastener structural element test for certifying navy fastener materials
21. Assessment of Co-Cr-Ni ternary system by CALPHAD technique10.1007/s12598-012-0466-y ↗
22. Development of multiphase alloy MP159 using experimental statistics10.1016/0026-0800(83)90002-2 ↗
23. Strain induced transformation in MP alloys10.1016/0036-9748(80)90376-2 ↗
24. The secondary hardening phenomenon in strain-hardened MP35N alloy
25. Strengthening in MULTIPHASE (MP35N) alloy: Part I. ambient temperature deformation and recrystallization10.1007/BF02660873 ↗
26. Work strengthening by a deformation-induced phase transformation in “MP alloys10.1007/BF02811551 ↗
27. Investigation on the cold deformation strengthening mechanism in MP159 alloy10.1007/s11661-000-0046-x ↗
28. Investigation of secondary hardening in Co-35Ni-20Cr-10Mo alloy using analytical scanning transmission electron microscopy10.1016/j.actamat.2013.10.005 ↗
29. A transmission electron microscopic investigation of phase transformations in MP35N10.1007/BF02700461 ↗
30. Effect of the thermal exposure on microstructure of MP159 alloy10.1023/A:1004791807509 ↗
31. Influence of cold-work and aging heat treatment on strength and ductility of MP35N10.1016/S0921-5093(99)00502-X ↗
32. Prevention of failures of high strength fasteners in use in offshore and subsea applications10.1016/j.engfailanal.2008.07.012 ↗
33. Stress-corrosion cracking evaluation of aerospace bolting alloys
34. Effect of heat treatment and impurities on the hydrogen embrittlement of a nickel cobalt base alloy10.5006/0010-9312-36.1.29 ↗
35. Hydrogen embrittlement of nickel, cobalt and iron-based superalloys
36. Lee · 2016
37. Environmentally assisted cracking of high strength nickel based alloys under cathodic protection
38. Qq-N-286G · 2000
39. Monel K-500 hydrogen embrittlement
40. Courtney · 2000
41. Tada · 1985
42. Fatigue at notches and the local strain and fracture mechanics approaches
43. Fatigue cracks at notches10.1016/0020-7403(77)90011-X ↗
44. Calibrating the electric potential method for studying slow crack growth
45. Application of the electrical potential method to crack length measurements using Johnson's formula10.1520/JTE11560J ↗
46. 2013
47. Kumar · 1981
48. Anderson · 2005
49. Crank · Mathematics of Diffusion · 1975
50. An electrochemical technique to measure diffusible hydrogen in metals (barnacle electrode)
51. Popernack · 2017
52. Hydrogen assisted cracking of high strength alloys
53. Diffusion coefficients of hydrogen in Ni-Cu and Ni-Co alloys10.2320/matertrans1960.27.233 ↗
54. H-enhanced deformation and fracture in the crack tip process zone
55. On the relationship between critical tensile stress and fracture toughness in mild steel10.1016/0022-5096(73)90008-2 ↗
56. On macroscopic and microscopic analyses for crack initiation and crack growth toughness in ductile alloys10.1007/BF02815305 ↗
57. Predicting the effect of applied potential on crack tip hydrogen concentration in low-alloy martensitic steels (Reprinted from Proceedings of the CORROSION/2007 research topical symposium “Advances in Environmentally Assisted Cracking”10.5006/1.3278484 ↗
58. Strain rate dependent environment assisted cracking of α/β-Ti alloys in chloride solution
59. Crack tip mechanics effects on environment-assisted cracking of beta-titanium alloys in aqueous NaCl10.1046/j.1460-2695.2000.00243.x ↗
60. The predominant role of strain-induced vacancies in hydrogen embrittlement of steels: Overview10.1016/j.actamat.2018.12.013 ↗
61. Mechanisms and kinetics of environmentally assisted cracking: current status, issues, and suggestions for further work10.1007/s11661-012-1359-2 ↗
62. Modelling hydrogen induced damage mechanisms in metals
63. Hydrogen embrittlement understood10.1007/s11663-015-0325-y ↗
64. A mechanistic theory of hydrogen embrittlement of steels10.1002/bbpc.19720760864 ↗
65. Hydrogen-enhanced localized plasticity—a mechanism for hydrogen-related fracture10.1016/0921-5093(94)90975-X ↗
66. The synergistic action and interplay of hydrogen embrittlement mechanisms in steels and iron: localized plasticity and decohesion10.1016/j.engfracmech.2019.106528 ↗
67. Elucidating the contribution of mobile hydrogen-deformation interactions to hydrogen-induced intergranular cracking in polycrystalline nickel10.1016/j.actamat.2018.07.043 ↗
68. Hydrogen-induced intergranular failure in nickel revisited10.1016/j.actamat.2012.01.040 ↗
69. Electrochemical aspects of hydrogen in metals
70. Surface effects on hydrogen entry into metals
71. Internal hydrogen embrittlement of ultrahigh-strength AERMET 100 steel10.1007/s11661-003-0334-3 ↗
72. A critical-strain criterion for hydrogen embrittlement of cold-drawn, ultrafine pearlitic steel10.1007/s11661-002-0217-z ↗
73. Effect of hydrogen content on the embrittlement in a Fe-Mn-C twinning-induced plasticity steel10.1016/j.corsci.2012.03.009 ↗
74. The necessity of both plasticity and brittleness in the fracture thresholds of iron10.1080/01418619108204854 ↗
75. Grain boundary energy effect on grain boundary segregation in an equiatomic high-entropy alloy10.1103/PhysRevMaterials.4.053603 ↗
76. Grain boundary decohesion by nanoclustering Ni and Cr separately in CrMnFeCoNi high-entropy alloys10.1126/sciadv.aay0639 ↗
77. Sulfur induced fracture mode transition of nickel at cathodic potentials10.1016/0036-9748(80)90263-X ↗
78. Influence of sulfur, phosphorus, and antimony segregation on the intergranular hydrogen embrittlement of nickel10.1007/BF02651619 ↗
79. Grain boundary decohesion by impurity segregation in a nickel-sulfur system10.1126/science.1104624 ↗
80. Intergranular fracture of nickel: the effect of hydrogen-sulfur co-segregation10.1016/0001-6160(87)90127-1 ↗
81. Effect of low-pressure hydrogen on the room-temperature tensile ductility and fracture behavior of Ni3Al10.1016/0966-9795(96)00039-8 ↗
82. Boron doped ultrastrong and ductile high-entropy alloys10.1016/j.actamat.2018.04.004 ↗
83. Surface and grain-boundary segregation of sulfur and boron in nickel10.1016/0001-6160(88)90108-3 ↗
84. Dislocation substructure vs transgranular stress corrosion susceptibility of single phase Alloys10.5006/0010-9312-19.3.102 ↗
85. The role of metallurgical variables in hydrogen-assisted environmental fracture
86. Effect of strain-induced martensite on hydrogen environment embrittlement of sensitized austenitic stainless steels at low temperatures10.1016/S1359-6454(98)00136-0 ↗
87. Hydrogen embrittlement associated with strain localization in a precipitation-hardened Fe–Mn–Al–C light weight austenitic steel10.1016/j.ijhydene.2013.12.171 ↗
88. Hydrogen embrittlement in a Fe -Mn-C ternary twinning-induced plasticity steel
89. Hydrogen environment embrittlement of stable austenitic steels10.1016/j.ijhydene.2012.08.071 ↗
90. The role of intergranular fracture on hydrogen-assisted fatigue crack propagation in pure iron at a low stress intensity range10.1016/j.msea.2018.07.014 ↗
91. Pronounced transition of crack initiation and propagation modes in the hydrogen-related failure of a Ni-based superalloy 718 under internal and external hydrogen conditions10.1016/j.corsci.2019.108186 ↗
92. Hydrogen-induced compatibility constraints across grain boundaries drive intergranular failure of Ni10.1016/j.msea.2019.05.036 ↗