Multiple damage mechanisms facilitated by planar dislocation glide in a commercial-grade precipitation-strengthened Fe–Ni–Cr-based steel
Source abstract
Abstract
Abstract The present study addresses the damage evolution mechanism in precipitation-strengthened Fe–Ni–Cr-based steel (SUH 660) at ambient temperature in air. Specifically, damage quantification and associated microstructure characterization were performed. The damage initiation sites were inclusion and grain boundaries impinging dislocation slip. The early stage of damage evolution was observed before necking of the specimen. Subsequent plastic straining caused damage growth along slip planes and coalescence of damage via localized shear in ligaments between damages, for which the behavior was associated with the planar character of the slip. The damage evolution behavior observed in the post-mortem specimen was consistent with fractographic characteristics.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Microstructure and Mechanical Properties of Steels · Material Properties and Failure Mechanisms
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (28)
Show source-provided references
1. Microstructure evolution and strengthening mechanisms of Fe-23Mn-0.3C-1.5Al twip steel during cold rolling10.1016/j.msea.2014.08.051 ↗
2. Direct observation of dislocation plasticity in high-Mn light weight steel by in-situ TEM10.1038/s41598-019-51586-y ↗
3. Post-uniform elongation and tensile fracture mechanisms of Fe-18Mn-0.6C-xAl twinning induced plasticity steels10.1016/j.actamat.2017.04.011 ↗
4. Dislocation motion at a fatigue crack tip in a high-nitrogen steel clarified through in situ electron channeling contrast imaging
5. Planar-slip driven fatigue crack initiation and propagation in an equiatomic CrMnFeCoNi high-entropy alloy10.1016/j.ijfatigue.2019.105418 ↗
6. Hydrogen embrittlement associated with strain localisation in a precipitation hardened Fe-Mn-Al-C light weight austenitic steel10.1016/j.ijhydene.2013.12.171 ↗
7. Hydrogen-induced ductility loss of precipitation-strengthened Fe-Ni-Cr-based superalloy10.1016/j.msea.2018.10.040 ↗
8. Degradation of fatigue properties in high pressure gaseous hydrogen environment evaluated by cyclic pressurization tests10.1016/j.proeng.2010.03.134 ↗
9. On the origin of planar slip in f.c.c. alloys10.1016/0001-6160(89)90143-0 ↗
10. Hydrogen-induced cracking behavior of twin boundary in γʹ phase strengthened Fe-Ni based austenitic alloys10.1016/j.msea.2012.10.069 ↗
11. Role of γʹ characteristic on the hydrogen embrittlement susceptibility of Fe-Ni-Cr alloys10.1016/j.corsci.2015.09.003 ↗
12. Internal hydrogen effects on tensile properties of iron-and nickel-base superalloys10.1007/BF02782416 ↗
13. Mechanism of hydrogen embrittlement in a gamma-prime phase strengthened Fe-Ni based austenitic alloy10.1016/j.msea.2012.06.036 ↗
14. Effect of grain size on the hydrogen embrittlement sensitivity of a precipitation strengthened Fe-Ni based alloy10.1016/j.msea.2013.11.062 ↗
15. Identification of the continuum damage parameter: an experimental challenge in modeling damage evolution10.1016/j.actamat.2012.03.017 ↗
16. Hydrogen-assisted decohesion and localized plasticity in dual-phase steel10.1016/j.actamat.2014.01.048 ↗
17. Combined multi-scale analyses on strain/damage/microstructure in steel: example of damage evolution associated with ε-martensitic transformation10.2355/isijinternational.ISIJINT-2016-272 ↗
18. Microstructure and hydrogen effects on fracture in the alloy A-28610.1007/BF02666333 ↗
19. Microstructural damage evolution and arrest in binary Fe-high-Mn alloys with different deformation temperatures10.1007/s10704-018-0307-6 ↗
20. Evolution of quasi-brittle hydrogen-assisted damages in a dual-phase steel10.2320/matertrans.MT-M2019196 ↗
21. Small fatigue crack growth in a high entropy alloy
22. Electron channeling contrast imaging of twins and dislocations in twinning-induced plasticity steels under controlled diffraction conditions in a scanning electron microscope10.1016/j.scriptamat.2009.06.018 ↗
23. Theory and application of electron channelling contrast imaging under controlled diffraction conditions10.1016/j.actamat.2014.04.018 ↗
24. On the ductile enlargement of voids in triaxial stress fields10.1016/0022-5096(69)90033-7 ↗
25. Dislocation and grain boundary interactions in metals10.1016/0001-6160(88)90058-2 ↗
26. The role of localized deformation in hydrogen-assisted crack propagation in 21Cr–6Ni–9Mn stainless steel10.1016/j.actamat.2009.04.027 ↗
27. Brittle fracture in austenitic steel10.1016/0956-7151(94)90300-X ↗
28. Hydrogen-assisted failure in a twinning-induced plasticity steel studied under in situ hydrogen charging by electron channeling contrast imaging10.1016/j.actamat.2013.04.030 ↗