Abstract
Abstract In this work, novel warm deep drawing and redrawing test setups were designed and developed, and a process sequence was proposed to enhance the forming depth of AA6082 sheet. The complete redrawing of the cup was ensured by maintaining the temperature of redrawing die and binder at 200 °C and water-circulated cooling punch near to room temperature. The warm redrawing negated the sudden thinning and strain localization at cup corner, producing an overall draw ratio of 3.38. Further, the fully redrawn cups were subjected to solution heat treatment (SHT) and subsequent different artificial aging cycle to evaluate the impact on post-forming strength. The post-forming cup wall strength was characterized using Vickers microhardness test and ring hoop tensile test (RHTT). Approximately 30% improvement in microhardness of redrawn cup wall was obtained as compared to that of the undeformed sheet, and it was due to the significant grain refinement occurred during the warm deep drawing and subsequent redrawing process as characterized by SEM and EBSD techniques. Moreover, it was observed that the heat treatment had a pronounced effect on both the hardness and ultimate hoop tensile strength of the cup wall, and the peak aged cup wall hardness and tensile strength were 119 VHN and 316.8 MPa, respectively. As verified by TEM micrographs, the precipitation of coherent large needle-shaped β′′ precipitate was responsible for the significant improvement in the strength during the aging treatment. However, the presence of plate-shaped incoherent β-Mg2Si precipitate marginally decreased the total elongation at peak aged condition. Finally, the fractographs of redrawn and different artificially aged RHTT samples were analyzed to comprehend the nature of failure.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metal Forming Simulation Techniques · Aluminum Alloy Microstructure Properties · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (60)
Show source-provided references
1. Aluminium in innovative light-weight car design10.2320/matertrans.L-MZ201132 ↗
2. Review of warm forming of aluminum-magnesium alloys10.1016/j.jmatprotec.2008.03.057 ↗
3. Heat treatment selection and forming strategies for 6082 aluminum alloy10.1115/1.3120384 ↗
4. Mohamed · 2010
5. Recent development in aluminium for automotive applications10.1016/S1003-6326(14)63305-7 ↗
6. Counter-pressure deep drawing and its application in the forming of automobile parts10.1016/0924-0136(90)90244-O ↗
7. Direct redrawing of cups using an annular urethane pad10.1016/S0924-0136(02)00079-1 ↗
8. Identification of two aluminum alloys and springback behaviors in cold bending
9. Characterization of tensile properties, limiting strains, and deep drawing behavior of AA5754-H22 sheet at elevated temperature10.1007/s11665-015-1740-6 ↗
10. Tensile deformation behavior of aluminum alloys at warm forming temperatures10.1016/S0921-5093(02)00915-2 ↗
11. Experimental and numerical studies on the warm deep drawing of an Al–Mg alloy10.1016/j.ijmecsci.2015.01.009 ↗
12. Biaxial warm forming behavior of aluminum sheet alloys10.1016/j.jmatprotec.2003.07.003 ↗
13. Analysis of thickness variation of reverse deep drawing of preformed 5A06 aluminum alloy cup under different temperatures10.1007/s00170-015-8179-7 ↗
14. Kaya · 2008
15. Deep drawability of type 5083 aluminium–magnesium alloy sheet under various conditions of temperature and forming speed10.1016/S0924-0136(99)00057-6 ↗
16. Investigations into improvement in formability of AA5754 and AA6082 sheets at elevated temperatures10.1007/s11665-019-04030-1 ↗
17. Experimental and finite element studies of redrawing for ASS 316 at elevated temperatures10.1016/j.matpr.2017.05.037 ↗
18. Experimental investigation of failures in redrawing of Ti-6Al-4V alloy at warm conditions10.1016/j.matpr.2017.07.194 ↗
19. Redrawing of EDD steel at elevated temperature
20. Finite element simulation of direct redrawing process of EDD steel at elevated temperatures10.1016/j.matpr.2015.07.164 ↗
21. Microstructure development in hot deformed AA608210.1016/j.msea.2010.11.048 ↗
22. Local deformation and processing maps of as-cast AZ31 alloy10.1016/j.msea.2009.03.007 ↗
23. Dynamic continuous recrystallization characteristics in two stage deformation of Mg–3Al–1Zn alloy sheet10.1016/S0921-5093(02)00096-5 ↗
24. An experimental study of the recrystallization mechanism during hot deformation of aluminium10.1016/S0921-5093(00)00733-4 ↗
25. Continuous dynamic recrystallization during the transient severe deformation of aluminum alloy 747510.1016/j.actamat.2008.09.001 ↗
26. Comprehensive analysis of minimum grain size in pure aluminum using friction stir processing10.1016/j.matlet.2010.06.003 ↗
27. Microstructural control of aluminum sheet used in automotive applications10.1016/1044-5803(95)00065-8 ↗
28. Benchmark 1 - failure prediction after cup drawing, reverse redrawing and expansion Part A: benchmark description10.1088/1742-6596/734/2/022001 ↗
29. Prediction of fracture and deep drawing behavior of solution treated Inconel-718 sheets: numerical modeling and experimental validation10.1016/j.msea.2018.07.007 ↗
30. An improved relationship between Vickers hardness and yield stress for cold formed materials and its experimental verification10.1016/S0007-8506(07)62929-1 ↗
31. Investigations on warm forming of AW-7020-T6 alloy sheet10.1016/j.jmatprotec.2014.03.024 ↗
32. Examination of the strength and ductility of AA-1050 material shaped with the multi-stage deep drawing method10.2478/v10172-011-0026-8 ↗
33. Strength and ductility evaluation of cold-welded seams in aluminum tubes extruded through porthole dies10.1016/j.matdes.2014.11.013 ↗
34. Mechanics and full-field deformation study of the ring hoop tension test10.1016/j.ijsolstr.2014.04.023 ↗
35. The influence of Mg/Si ratio on the negative natural aging effect in Al–Mg–Si–Cu alloys10.1016/j.msea.2015.06.090 ↗
36. Influence of heat treatment on the microstructure and mechanical properties of 6005 and 6082 aluminium alloys10.1016/j.jmatprotec.2005.02.115 ↗
37. The influence of temperature and storage time at RT on nucleation of the β″ phase in a 6082 Al–Mg–Si alloy10.1016/S1359-6454(02)00470-6 ↗
38. Fakult · 2011
39. Improvement in material flow during nonisothermal warm deep drawing of nonheat treatable Aluminum alloy sheets10.1115/1.4034594 ↗
40. Effect of solution treatment on deep drawability of IN718 sheets: experimental analysis and metallurgical characterization10.1016/j.msea.2018.04.110 ↗
41. Dieter · 1986
42. Ring hoop tension test (RHTT): a test for transverse tensile properties of tubular materials10.1520/JTE12328J ↗
43. Microstructural evolution and mechanical properties during homogenization and ageing treatment of Al-Mg-Si alloy wire cold drawn10.4028/www.scientific.net/JERA.36.60 ↗
44. Samuels · 2003
45. Effect of solution treatment on the formability and part performance of IN718 sheet material
46. Microstructures, forming limit and failure analyses of inconel 718 sheets for fabrication of aerospace components10.1007/s11665-017-2547-4 ↗
47. Finite element validation of forming limit diagram of IN-718 sheet metal, mater
48. Formability and strengthening mechanism of solution treated Al–Mg–Si alloy sheet under hot stamping conditions10.1016/j.jmatprotec.2015.10.016 ↗
49. Mehtonen · 2014
50. Effect of rolling temperature on microstructure and mechanical properties of 6063 Al alloy10.1016/j.msea.2008.03.029 ↗
51. Influence of solutes and second phase particles on work hardening behavior of Al 6063 alloy processed by cryorolling10.1016/j.msea.2011.01.010 ↗
52. Analysis of precipitate density of an aluminium alloy by TEM and AFM
53. Verhoeven · 1975
54. Krog · 2016
55. The effect of the initial rolling temperature on the microstructure evolution during and after hot rolling of AA608210.1007/s12289-008-0078-0 ↗
56. New methods for automatic quantification of microstructural features using digital image processing10.1016/j.matdes.2017.12.049 ↗
57. Formability analysis of pre-strained AA5754-O sheet metal using Yld96 plasticity theory: role of amount and direction of uni-axial pre-strain10.1016/j.jmapro.2016.09.014 ↗
58. Effect of heat treatment on tensile and fracture toughness properties of 6082 alloy
59. Predicting the quench sensitivity of Al–Zn–Mg–Cu alloys: a model for linear cooling and strengthening10.1016/j.matdes.2015.09.058 ↗
60. A modified mechanical threshold stress constitutive model for austenitic stainless steels10.1007/s11665-016-2389-5 ↗