Abstract In this study, a series of the W/Ta multilayer composites are prepared by spark plasma sintering (SPS) at different temperature. The relationship between the sintering temperature and tensile properties are investigated in detail. Large equiaxed recrystallization grains appear in the W layers when the sintering temperature reaches 1200 °C. The W/Ta multilayer composites have a better comprehensive performance when the sintering temperature is 1100 °C. The fracture mechanisms of the W/Ta multilayer composites can be divided into two types based on the bonding strength of the interface. When the sintering temperature is lower than 1200 °C, delamination cracks can be seen. Meanwhile, necks and shear cracks appear in the Ta layers. When the sintering temperature reaches 1200 °C, delamination cracks disappear. Meanwhile, a lot of shear bands can be observed in the Ta layers. As the sintering temperature increases, the fracture mode of the W layers changes from transgranular cleavage fracture to intergranular fracture. And the fracture mode of the Ta layers is always ductility fracture. However, the ductility of the Ta layers decreases since the stress state changes from plane stress state to plane strain state. The tensile strength of the W/Ta multilayer composites can be calculated by the proposed model considering the stress concentration factor in the interface.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Metal and Thin Film Mechanics · Fusion materials and technologies · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (30)

Show source-provided references
1. Tungsten as material for plasma-facing components in fusion devices10.1016/j.jnucmat.2011.01.110 ↗
2. Tritium inventory and recovery in next-step fusion devices
3. Structural materials for fission & fusion energy10.1016/S1369-7021(09)70294-9 ↗
4. Research status and issues of tungsten plasma facing materials for ITER and beyond10.1016/j.fusengdes.2014.02.078 ↗
5. Review of recent works in development and evaluation of high-Z plasma facing materials10.1016/S0022-3115(98)00817-4 ↗
6. Brittle fracture and the brittle-to-ductile transition of tungsten10.1016/j.jnucmat.2003.08.009 ↗
7. Effect of rhenium on the dislocation core structure in tungsten10.1103/PhysRevLett.104.195503 ↗
8. Fracture toughness and microstructural characterization of polycrystalline rolled tungsten10.1016/j.ijrmhm.2010.05.006 ↗
9. Observations on the ductile-to-brittle transition in ultrafine-grained tungsten of commercial purity10.1016/j.msea.2008.07.074 ↗
10. Extraordinary high ductility/strength of the interface designed bulk W-ZrC alloy plate at relatively low temperature10.1038/srep16014 ↗
11. Microstructure and performance of rare earth element-strengthened plasma-facing tungsten material10.1038/srep32701 ↗
12. Ch. Linsmeier, C. Broeckmann, Influence of the interface strength on the mechanical properties of discontinuous tungsten fiber-reinforced tungsten composites produced by field assisted sintering technology10.1016/j.compositesa.2018.01.022 ↗
13. Toughening of a low-activation tungsten alloy using tungsten short fibers and particles reinforcement for fusion plasma-facing applications10.1088/1741-4326/aaf43f ↗
14. Effect of thickness ratio on toughening mechanisms of Ta/W multilayers10.1016/j.jallcom.2016.01.084 ↗
15. The microstructure and tensile properties of W/Ti multilayer composites prepared by spark plasma sintering10.1016/j.jallcom.2018.11.346 ↗
16. Deformation behavior of brittle/ductile multilayered composites under interface constraint effect10.1016/j.ijplas.2016.11.005 ↗
17. Resistance-curve and fracture behavior of Ti-Al3Ti metallic–intermetallic laminate (MIL) composites10.1016/S1359-6454(03)00108-3 ↗
18. Ductilisation of tungsten (W): tungsten laminated composites10.1016/j.ijrmhm.2017.07.013 ↗
19. Cold rolled tungsten (W) plates and foils: evolution of the tensile properties and their indication towards deformation mechanisms10.1016/j.ijrmhm.2017.09.007 ↗
20. Plasma-facing material alternatives to tungsten10.1088/0029-5515/55/4/043002 ↗
21. Effect of high-flux, low-energy He+ ion irradiation on Ta as a plasma-facing material10.1038/srep39746 ↗
22. First-principles study of the interaction between helium and the defects in tantalum10.1016/j.jnucmat.2016.08.003 ↗
23. EBSD image quality mapping10.1017/S1431927606060090 ↗
24. Application of orientation imaging microscopy to study phase transformations in steels10.1016/S1044-5803(01)00140-1 ↗
25. Size effects on tensile properties and deformation mechanism of commercial pure tantalum foils10.1016/j.ijrmhm.2019.01.015 ↗
26. Chapter 2-griffith theory of fracture
27. Crack propagation in single crystals of tungsten10.1080/14786436508228132 ↗
28. Designing laminated metal composites for tensile ductility10.1016/j.matdes.2014.08.061 ↗
29. Heywood · 1969
30. Tabor · 1951