Preparation and anisotropic compressive deformation behaviors of tungsten fiber reinforced Cu-Zn matrix composite
Source abstract
Abstract
Abstract For the purpose of fabricating materials with a good “self-sharpening” capacity, the tungsten fiber reinforced Cu-Zn matrix composite was successfully fabricated by the pressureless infiltration method, and the microstructure of the prepared composite was investigated. To investigate the anisotropic mechanical properties, the quasi-static and the dynamic compressive deformation behaviors of the composite in different loading directions were investigated. The angles between the loading direction and the tungsten fiber orientation are 0°, 45° and 90°, respectively. The failure mechanisms of the composite loaded in different directions were investigated systematically. Finally, the “self-sharpening” capacity of the composite was investigated by a ballistic impact experiment, and the mechanism of the “self-sharpening” capacity was discussed.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High-Velocity Impact and Material Behavior · Aluminum Alloys Composites Properties · Microstructure and mechanical properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (39)
Show source-provided references
1. A review of tungsten-based alloys as kinetic energy penetrator materials
2. Effect of processing parameters on microstructure and mechanical properties of 90W–6Ni–4Mn heavy alloy10.1016/j.ijrmhm.2014.09.024 ↗
3. Adiabatic shear bands in the Taylor impact test for a WHA rod10.1016/S0749-6419(98)00026-6 ↗
4. Dynamic deformation behavior of tungsten-fiber/metallic–glass matrix composites10.1016/S0734-743X(99)00176-1 ↗
5. Microstructure and mechanical properties of mechanically alloyed and solid-state sintered tungsten heavy alloys10.1016/S0921-5093(00)00968-0 ↗
6. Microstructure and mechanical properties of tungsten heavy alloys10.1016/j.msea.2010.08.071 ↗
7. Deformation twins in oriented, columnar-grained tungsten rod ballistic penetrators10.1016/S0921-5093(00)01280-6 ↗
8. Matrix pools in a partially mechanically alloyed tungsten heavy alloy for localized shear deformation10.1016/S0921-5093(01)01839-1 ↗
9. Characterisation of depleted uranium (DU) from an unfired C etween material properties of long-roHARM-3 penetrator10.1016/S0048-9697(03)00401-7 ↗
10. Preparation of fine-grained tungsten heavy alloys by spark plasma sintered W–7Ni–3Fe composite powders with different ball milling time10.1016/j.jallcom.2013.02.014 ↗
11. Effect of heat treatment on microstructure and mechanical properties of hot-hydrostatically extruded 93W–4.9Ni–2.1Fe alloy10.1016/j.jallcom.2014.11.009 ↗
12. strain rate deformation behaviors of kinetic energy penetrator materials during ballistic impact10.1016/0167-6636(94)90055-8 ↗
13. Properties, use and health effects of depleted uranium (DU): a general overview10.1016/S0265-931X(02)00041-3 ↗
14. A computational study of the relations bd penetrators and their ballistic performance10.1016/S0734-743X(97)00068-7 ↗
15. Self-sharpening behavior during ballistic impact of the tungsten heavy alloy rod penetrators processed by hot-hydrostatic extrusion and hot torsion10.1016/j.msea.2010.04.050 ↗
16. Microstructure analysis and comparison of tungsten alloy rod and [001] oriented columnar-grained tungsten rod ballistic penetrators10.1016/S0921-5093(98)00997-6 ↗
17. Penetration of boron carbide, aluminum, and beryllium alloys by depleted uranium rods: modeling and experimentation10.1016/j.ijimpeng.2006.09.059 ↗
18. Effect of fibrous orientation on dynamic mechanical properties and susceptibility to adiabatic shear band of tungsten heavy alloy fabricated through hot-hydrostatic extrusion10.1016/j.msea.2007.10.012 ↗
19. Adiabatic shear banding in a tungsten heavy alloy processed by hot-hydrostatic extrusion and hot torsion10.1016/j.scriptamat.2008.08.036 ↗
20. Susceptibility to adiabatic shear band of tungsten heavy alloy fabricated through hot-hydrostatic extrusion and cold torsion10.1016/S1875-5372(09)60037-0 ↗
21. Wf/Zr41.2Ti13.8Cu12.5Ni10Be22.5 bulk metallic glass composites prepared by a new melt infiltrating method10.1016/j.jallcom.2010.02.045 ↗
22. Simulation of shear banding and crack propagation in bulk metallic glass matrix composites10.1016/j.jallcom.2010.08.131 ↗
23. Dynamic shear punch behavior of tungsten fiber reinforced Zr-based bulk metallic glass matrix composites10.1016/j.ijimpeng.2014.07.006 ↗
24. Anisotropic compressive deformation behaviors of tungsten fiber reinforced Zr-based metallic glass composites10.1016/j.msea.2012.12.080 ↗
25. Anisotropic tensile properties of tungsten fiber reinforced Zr based metallic glass composites10.1016/j.msea.2014.09.084 ↗
26. Penetrating behaviors of Zr-based metallic glass composite rods reinforced by tungsten fibers10.1016/j.tafmec.2012.02.003 ↗
27. Experimental research on the long rod penetration of tungsten-fiber/Zr-based metallic glass matrix composite into Q235 steel target10.1016/j.ijimpeng.2014.11.007 ↗
28. High-strength tungsten wire reinforced Zr-based bulk metallic glass matrix composites prepared by continuous infiltration process10.1016/j.matlet.2012.11.086 ↗
29. Atomic interaction mechanism for designing the interface of W/Zr-based bulk metallic glass composites10.1038/srep08967 ↗
30. Interfacial optimization of tungsten fibre-reinforced copper for high-temperature heat sink material for fusion application10.1016/j.jnucmat.2008.12.138 ↗
31. High temperature fracture behavior of tungsten fiber reinforced copper matrix composites under dynamic compression10.1016/j.matdes.2011.06.006 ↗
32. The effect of interface modification on fracture behavior of tungsten fiber reinforced copper matrix composites10.1016/j.msea.2011.11.088 ↗
33. Thermal properties of W–Cu composites manufactured by copper infiltration into tungsten fiber matrix10.1016/j.ijrmhm.2014.05.022 ↗
34. Interfacial failure mechanism in tungsten fiber reinforced copper-based composites fabricated by combustion synthesis melt infiltration under ultra-high gravity10.1016/j.matdes.2015.08.115 ↗
35. Study on improving “self-sharpening” capacity of W–Cu–Zn alloy by the pressureless infiltration method10.1016/j.msea.2014.04.015 ↗
36. Investigation on the penetration performance and “self-sharpening” behavior of the 80W–14Cu–6Zn penetrators10.1016/j.ijrmhm.2015.08.001 ↗
37. Deformation twins and related softening behavior in nanocrystalline Cu–30% Zn alloy10.1016/j.actamat.2012.02.036 ↗
38. Effects of processing parameters of tungsten–copper composites10.1016/j.ijrmhm.2012.02.015 ↗
39. Effects of Zn additions on the solid-state sintering of W–Cu composites10.1016/j.matdes.2011.10.006 ↗