Abstract

Abstract Carbon/carbon (C/C) composites with characteristic matrix-crack pattern are key intermediate materials for preparation of carbon/silicon carbide (C/C–SiC) composites. The C/C composites were prepared by pyrolyzing carbon fiber/phenolic resin preform. The change of density, open porosity, mass loss and specially the microstructural evolution of the composites during pyrolysis at 200–900 °C was analyzed, which provided important information for preparation of C/SiC composites by infiltration of silicon. An increasing number of regular spacing cracks were formed above 400 °C. After pyrolysis at 900 °C, the pore volume was 0.17 cm 3 /g, and the pores in the radius range of 2.44–122.19 μm occupied 81% of the pore volume.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Diamond and Carbon-based Materials Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (9)

Show source-provided references
1. Kochendorfer · 2001 · 277
2. Nannetti · 2001 · 368
3. Imuta · Key Eng. Mater. · 1999 · 164–165 · 43910.4028/www.scientific.net/KEM.164-165.439 ↗
4. Kochendorfer · Key Eng. Mater. · 1999 · 164–165 · 45110.4028/www.scientific.net/KEM.164-165.451 ↗
5. Krenkel · Ceram. Eng. Sci. Proc. · 2001 · 22 · 442
6. Hald · 2003 · 1
7. Krenkel · Adv. Eng. Mater. · 2002 · 4 · 42710.1002/1527-2648(20020717)4:7<427::AID-ADEM427>3.0.CO;2-C ↗
8. Trick · Carbon · 1995 · 3 · 150910.1016/0008-6223(95)00092-R ↗
9. Schulte-Fischedick · Mater. Sci. Eng. · 2002 · 332 · 14610.1016/S0921-5093(01)01719-1 ↗