Abstract
Abstract Fatigue crack growth experiments were conducted on highly sensitized AA5456-H116 in laboratory air and 0.6 M NaCl at two applied potentials (−900 mVSCE and −1300 mVSCE; vs. saturated calomel electrode) using frequencies of 5 and 0.1 Hz. At 5 Hz, the fatigue crack growth rate (da/dN) was similar between −900 mVSCE and −1300 mVSCE (~1.5 × 10−4 mm/cycle), which were both approximately 10-fold faster than the da/dN measured in laboratory air. However, significant differences in da/dN were observed between −900 and −1300 mVSCE for testing at 0.1 Hz. Specifically, while a nominally similar da/dN to the 5 Hz data was observed for −900 mVSCE, a 1000-fold decrease in da/dN was noted for −1300 mVSCE at 0.1 Hz. Microscopy of the crack tip region on interrupted fatigue experiments conducted at −1300 mVSCE revealed significant blunting of the crack tip at 0.1 Hz, while the crack tip cycled at 5 Hz remained sharp. A stepped potential experiment demonstrated that the measured da/dN at −1100 mVSCE decreased by multiple orders of magnitude when this potential was approached from the cathodic versus the anodic direction. Collectively, these data suggest a salient role of corrosion-induced blunting on the measured da/dN for highly sensitized AA5xxx-series alloys immersed in marine environments at highly cathodic potentials and low loading frequency.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Non-Destructive Testing Techniques · Corrosion Behavior and Inhibition · Hydrogen embrittlement and corrosion behaviors in metals
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (90)
Show source-provided references
1. Environmental degradation of marine aluminum alloys-Past, present, and future10.5006/1927 ↗
2. Aluminum alloys in marine construction: characteristics, application, and problems from a fabrication viewpoint
3. Survey of detection, mitigation, and repair technologies to address problems caused by sensitization of Al-Mg alloys on navy ships
4. Kaufman · 2000
5. Experiment-based modelling of grain boundary β-phase (Mg2Al3) evolution during sensitisation of aluminium alloy AA5083
6. Modeling sensitization of Al-Mg alloys via β-phase precipitation kinetics10.1016/j.scriptamat.2015.02.012 ↗
7. Predictive sensitization modeling for AA5xxx aluminum alloys including non-isothermal cases10.5006/1675 ↗
8. Sensitization prediction and validation for Al 5xxx alloys exposed to long-term cyclical and constant heating at low temperatures10.5006/1918 ↗
9. Imparting sensitization resistance to an Al-5Mg alloy via neodymium additions10.5006/0833 ↗
10. A survey of sensitization in 5xxx series aluminum alloys10.5006/1787 ↗
11. The effect of temper and composition on the stress corrosion cracking of Al-Mg alloys10.5006/2317 ↗
12. Standard test method for determining the susceptibility to intergranular corrosion of 5XXX series aluminum alloys by Mass Loss after exposure to nitric Acid (NAMLT test)
13. Influence of Mg content on the sensitization and corrosion of Al-xMg(-Mn) alloys10.5006/0948 ↗
14. Overview of intergranular corrosion mechanisms, phenomenological observations, and modeling of AA508310.5006/1818 ↗
15. Corrosion and stress corrosion of 5000-series Al alloys in marine environments10.5006/0010-9312-22.3.68 ↗
16. Influence of service temperature on the resistance of wrought aluminum-magnesium alloys to corrosion10.5006/0010-9312-15.2.19 ↗
17. Stress corrosion cracking and anodic dissolution behavior of 5083 aluminum alloy
18. Strained electrode reactions and stress-corrosion cracking of 5083 alloy10.2464/jilm.27.138 ↗
19. Stress corrosion testing of 5083 aluminum10.5006/1.3585991 ↗
20. Stress corrosion cracking of Al-Mg alloy 5083 sensitized at low temperature10.5006/1766 ↗
21. Crack chemistry control of intergranular stress corrosion cracking in sensitized Al-Mg
22. Improved understanding of environment-induced cracking (EIC) of sensitized 5XXX series aluminium alloys10.1016/j.msea.2016.11.088 ↗
23. Pre-exposure embrittlement of a commercial Al-Mg-Mn alloy, AA5083-H13110.1515/corrrev-2017-0037 ↗
24. Estimation of environment-induced crack growth rate as a function of stress intensity factors generated during slow strain rate testing of aluminum alloys10.1515/corrrev-2019-0031 ↗
25. Stress corrosion cracking of sensitized AA5083 (Al-4.5Mg-1.0Mn)10.1007/s11661-001-1036-3 ↗
26. Initiation and short crack growth behaviour of environmentally induced cracks in AA5083 H131 investigated across time and length scales10.1515/corrrev-2019-0044 ↗
27. Role of Mg in the stress corrosion cracking of an Al-Mg alloy10.1007/s11661-001-0148-0 ↗
28. Crack-particle interactions during intergranular stress corrosion of AA5083 as observed by cross-section transmission electron microscopy10.1016/j.scriptamat.2004.01.038 ↗
29. Stress corrosion cracking of Al-Mg and Mg-Al alloys10.5006/1.3299228 ↗
30. The influence of hydrogen on the stress-corrosion cracking of low-strength Al-Mg alloys
31. Cormack · 2012
32. Microstructural evolution and stress corrosion cracking behavior of Al-508310.1007/s11661-010-0262-y ↗
33. Deformation rate and sensitization effects on environmentally assisted cracking of Al-Mg naval alloys10.5006/1949 ↗
34. Sensitization and remediation effects on environmentally assisted cracking of Al-Mg naval alloys10.1016/j.corsci.2018.03.027 ↗
35. Stress-corrosion cracking susceptibility of the superplastically formed 5083 aluminum alloy in 3.5 pct NaCl solution10.1007/s11661-999-0229-z ↗
36. Through-thickness inhomogeneity of environmentally assisted cracking (EAC) in AA5083-H128 alloy10.1016/j.msea.2018.10.079 ↗
37. Slow strain rate testing and stress corrosion cracking of ultra-fine grained and conventional Al-Mg alloy10.1016/j.msea.2014.09.062 ↗
38. Effects of stabilization treatment on the precipitation behavior of β phase and stress corrosion for AA5383-H15 alloys10.1557/jmr.2019.152 ↗
39. The effect of loading orientation on the stress corrosion cracking of Al-Mg alloys10.5006/2343 ↗
40. Investigation of the stress corrosion cracking behavior in annealed 5083 aluminum alloy sheets with different texture types10.1016/j.jallcom.2019.152690 ↗
41. Anisotropy of corrosion and environmental cracking in AA5083-H128 Al-Mg alloy10.1016/j.msea.2018.06.021 ↗
42. The effect of loading mode on the stress-corrosion cracking of aluminum alloy 508310.1007/BF02644298 ↗
43. Mechanistic studies of intergranular stress corrosion cracking under atmospheric exposure conditions10.5006/2853 ↗
44. The effect of electrode potential on stress corrosion cracking in highly sensitized Al–Mg alloys10.1016/j.msea.2019.138399 ↗
45. Mitigation of intergranular stress corrosion cracking in Al–Mg by electrochemical potential control
46. Effect of sensitization heat treatment on properties of Al-Mg alloy AA5083-H11610.1007/s10853-008-2606-1 ↗
47. Hydrogen effects during IGSCC of pure Al-5Mg alloy in NaCl media10.1016/S0010-938X(01)00140-8 ↗
48. A mechanistic theory of hydrogen embrittlement of steels10.1002/bbpc.19720760864 ↗
49. The role of hydrogen and other interstitials in the mechanical behavior of metals: (1959 edward de mille campbell memorial lecture)10.1007/s13632-016-0319-4 ↗
50. Elucidating the contribution of mobile hydrogen-deformation interactions to hydrogen-induced intergranular cracking in polycrystalline nickel10.1016/j.actamat.2018.07.043 ↗
51. Optimization of corrosion protection potential for stress corrosion cracking and hydrogen embrittlement of 5083-H112 alloy in seawater10.3365/met.mat.2008.04.203 ↗
52. Mitigation of intergranular cracking in Al-Mg alloys via Zn-based electrode potential control in sodium chloride solution10.5006/3185 ↗
53. Inhibition of stress corrosion cracking of sensitized AA508310.5006/1798 ↗
54. Evaluating the electrochemical properties in the protection potential of material for use in Al vessels in seawater10.4028/www.scientific.net/MSF.510-511.158 ↗
55. Stress corrosion and hydrogen embrittlement in an aluminum alloy10.5006/0010-9312-30.8.274 ↗
56. Role of hydrogen embrittlement in the corrosion cracking of aluminum alloys10.1007/BF00726550 ↗
57. Effect of cathodic charging on the mechanical properties of aluminum10.1007/BF02645053 ↗
58. Hydrogen embrittlement and trapping in Al6%Zn-3%Mg10.1016/0001-6160(80)90138-8 ↗
59. Electron microscopy of hydrogen embrittlement in a high purity Al-Zn-Mg alloy
60. Stress corrosion cracking of high strength aluminum alloys
61. Laboratory accelerated and field exposure testing of MgRP and MgORP on AA2024-T351: chemical and electrochemical protection effects10.1016/j.surfcoat.2019.125245 ↗
62. Electrochemical diagnostic cycle testing of magnesium and magnesium oxide-pigmented primers on AA2024-t35110.5006/2547 ↗
63. Scientific investigation of the corrosion performance of magnesium and magnesium oxide primers on Al alloy 2024-t351 in field exposures10.5006/2879 ↗
64. Mg-rich coatings: a new paradigm for Cr-free corrosion protection of Al aerospace alloys10.1007/s11998-004-0001-7 ↗
65. Electrochemical behaviour of a Mg-rich primer in the protection of Al alloys10.1016/j.corsci.2005.04.008 ↗
66. Environmental degradation of a Mg-rich primer in selected field and laboratory environments: Part 1—without a topcoat10.5006/0988 ↗
67. H-enhanced deformation and fracture in the crack tip process zone
68. Hydrogen embrittlement in a 2000-series aluminum alloy10.1007/BF02643313 ↗
69. Corrosion-fatigue behavior of aluminum alloy 5083-H131 sensitized at 448 K (175 C)10.1007/s11661-011-0866-x ↗
70. The effect of sensitization and fatigue loading frequency on corrosion fatigue of AA5083-H13110.1016/j.ijfatigue.2019.02.044 ↗
71. The effects of loading frequency, sensitization, and crack length on corrosion fatigue of AA5456-H11610.5006/3366 ↗
72. Intergranular corrosion penetration in AA5083 (UNS # A95083) as a function of electrochemical and metallurgical conditions10.1149/1.3697588 ↗
73. Tada · 1985
74. Gangloff · 1992
75. Direct current potential difference fatigue crack measurement techniques
76. Calibrating the electric potential method for studying slow crack growth
77. Wide range stress intensity factor expressions for ASTM E399 standard fracture toughness specimens10.1007/BF00032844 ↗
78. Application of the electrical potential method to crack length measurements using Johnson's formula10.1520/JTE11560J ↗
79. Corrosion-fatigue behavior of aluminum alloy 5083-H131 sensitized at 175C10.1007/s11661-011-0866-x ↗
80. Electrochemical characteristics of Al-Mg alloy in seawater for leisure ship: stress corrosion cracking and hydrogen embrittlement10.1007/s11814-009-0042-9 ↗
81. New insights into the cathodic dissolution of aluminium using electrochemical methods10.1016/j.electacta.2016.09.011 ↗
82. The cathodic corrosion of aluminum10.1149/1.2132749 ↗
83. The corrosion of pure aluminium during cathodic polarization in aqueous solutions10.1016/S0010-938X(97)83354-9 ↗
84. Pourbaix · 1974
85. Electrochemical behavior of high purity aluminum in chloride containing solutions10.5006/0010-9312-27.11.483 ↗
86. The mechanism of aluminium corrosion in alkaline solutions10.1016/0010-938X(96)00037-6 ↗
87. Crack size effects on the chemical driving force for aqueous corrosion fatigue10.1007/BF02814848 ↗
88. Chemical and electrochemical conditions within stress corrosion and corrosion fatigue cracks10.1038/s41529-017-0015-0 ↗
89. Mathematical modelling of the electrochemistry in corrosion fatigue cracks in structural steel cathodically protected in sea water10.1016/0010-938X(86)90027-2 ↗
90. Steady state electrochemical kinetics of BS 4360 50D structural steel in deaerated 3·5%NaCl solution of varying pH10.1179/000705987798271479 ↗