Role of pre-existing shear band morphology in controlling the fracture behavior of a Zr–Ti–Cu–Ni–Al bulk metallic glass
Source abstract
Abstract
Abstract Shear bands were introduced into a Zr–Ti–Cu–Ni–Al bulk metallic glass (BMG) by one-directional cold rolling and the effect on fracture toughness anisotropy was examined. Two different rolling and shear band orientations relative to the crack plane were used, with the rolling force oriented along either the width (CR-W) or thickness (CR-T) direction of single edge notched bend specimens. The results showed the CR-W samples demonstrated a 50% reduction in KQ relative to the as-cast material while the CR-T samples demonstrated the highest fracture toughness. The low fracture toughness of the CR-W samples was attributed to easy crack propagation paths formed by the shear bands. In contrast, the higher fracture toughness of the CR-T samples was attributed to the difficulty of crack twisting out of the mode I precrack plane onto the shear band planes and the high energy absorption of mode III tearing between the parallel crack planes. Overall, when cold rolling BMGs for structural applications, care must be taken to design the shear band morphologies to achieve the desired fracture toughness properties rather than solely focusing on increasing the average relaxation enthalpy/free volume.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metallic Glasses and Amorphous Alloys
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (51)
Show source-provided references
1. Bulk metallic glasses as structural materials: a review10.1002/adem.201600066 ↗
2. Overview No.144 - mechanical behavior of amorphous alloys10.1016/j.actamat.2007.01.052 ↗
3. A microscopic mechanism for steady state inhomogeneous flow in metallic glasses10.1016/0001-6160(77)90232-2 ↗
4. Strain localization in amorphous metals10.1016/0001-6160(82)90225-5 ↗
5. Plastic-Flow and fracture of metallic glass10.1007/BF02642754 ↗
6. Effect of free volume changes and residual stresses on the fatigue and fracture behavior of a Zr-Ti-Ni-Cu-Be bulk metallic glass10.1016/j.actamat.2007.10.007 ↗
7. Embrittlement of a bulk metallic glass due to sub-Tg annealing10.1016/j.actamat.2004.11.040 ↗
8. Shear bands in metallic glasses10.1016/j.mser.2013.04.001 ↗
9. Deformation of metallic glasses: recent developments in theory, simulations, and experiments10.1016/j.actamat.2016.01.049 ↗
10. Inducing strain hardening in a Zr-based bulk metallic glass via cobalt mediated phase separations10.1016/j.jallcom.2017.11.223 ↗
11. Designing Zr-Cu-Co-Al bulk metallic glasses with phase separation mediated plasticity10.1007/s11661-011-1050-z ↗
12. Designing metallic glass matrix composites with high toughness and tensile ductility10.1038/nature06598 ↗
13. The effect of nanocrystallization and free volume on the room temperature plasticity of Zr-based bulk metallic glasses10.1016/j.actamat.2008.07.012 ↗
14. Introducing a strain-hardening capability to improve the ductility of bulk metallic glasses via severe plastic deformation10.1016/j.actamat.2011.09.026 ↗
15. Controlling the distribution of structural heterogeneities in severely deformed metallic glass10.1016/j.msea.2019.02.092 ↗
16. Work-hardening induced tensile ductility of bulk metallic glasses via high-pressure torsion10.1038/srep09660 ↗
17. Observation of shear bands in the Vitreloy metallic glass subjected to HPT processing10.1016/j.jallcom.2019.06.043 ↗
18. Ductile bulk metallic glasses produced through designed heterogeneities10.1016/j.scriptamat.2011.07.039 ↗
19. Ductile bulk metallic glass by controlling structural heterogeneities10.1038/s41598-018-27285-5 ↗
20. Improved plasticity of bulk metallic glasses upon cold rolling10.1016/j.scriptamat.2010.01.024 ↗
21. Ductility improvement of Zr55Cu30Al10Ni5 bulk amorphous alloy10.1016/S1359-6462(01)00723-0 ↗
22. Cold-rolled Zr50Cu30Ni10Al10 bulk amorphous alloys with tensile plastic elongation at room temperature10.2320/matertrans.43.3199 ↗
23. Effect of pre-existing shear bands on the tensile mechanical properties of a bulk metallic glass10.1016/j.actamat.2009.10.032 ↗
24. Effect of cold rolling on compressive and tensile mechanical properties of Zr52.5Ti5Cu18Ni14.5Al10 bulk metallic glass10.1016/j.jallcom.2011.01.022 ↗
25. Effect of pre-introduced shear bands direction on deformation behavior in Zr55Al10Ni5Cu30 bulk metallic glass10.2320/matertrans.MAW200920 ↗
26. Orientation effect of pre-introduced shear bands in a bulk-metallic glass on its "work-ductilising"10.1016/j.msea.2008.05.038 ↗
27. Cold rolling improves the fracture toughness of a Zr-based bulk metallic glass10.1016/j.jallcom.2016.10.134 ↗
28. Toughness enhancement and heterogeneous softening of a cryogenically cycled Zr–Cu–Ni–Al–Nb bulk metallic glass10.1016/j.actamat.2019.07.012 ↗
29. Guiding and deflecting cracks in bulk metallic glasses to increase damage tolerance10.1002/adem.201400209 ↗
30. Improvement of dynamic notch toughness for the Zr56Co28Al16 bulk metallic glass by local pre-deformation10.1016/j.jnoncrysol.2017.07.034 ↗
31. ASTM · 2018
32. Fracture toughness, fracture morphology, and crack-tip plastic zone of a Zr-based bulk amorphous alloy10.1007/s11661-001-1032-7 ↗
33. Enthalpy recovery and free volume relaxation in a Zr44Ti11Ni10Cu10Be25 bulk metallic glass10.1016/j.jallcom.2010.12.044 ↗
34. Equilibrium viscosity, enthalpy recovery and free volume relaxation in a Zr44Ti11Ni10Cu10Be25 bulk metallic glass10.1016/j.actamat.2011.03.064 ↗
35. Quantification of free volume differences in a Zr44Ti11Ni10Cu10Be25 bulk amorphous alloy10.1063/1.2766659 ↗
36. ASTM · 2017
37. Designed heterogeneities improve the fracture reliability of a Zr-based bulk metallic glass10.1016/j.msea.2015.08.055 ↗
38. Size-dependent fracture toughness of bulk metallic glasses10.1016/j.actamat.2014.01.062 ↗
39. Significant tensile ductility induced by cold rolling in Cu47.5Zr47.5Al5 bulk metallic glass10.1016/j.intermet.2011.05.001 ↗
40. Modeling and measurement of residual stresses in a bulk metallic glass plate10.1016/S0022-3093(02)01940-3 ↗
41. Slightly curved or kinked cracks10.1007/BF00012619 ↗
42. Mechanism of shear banding during cold rolling of a bulk metallic glass10.1016/j.jallcom.2018.09.302 ↗
43. Twisting cracks in Bouligand structures10.1016/j.jmbbm.2017.06.010 ↗
44. Shear band morphology and fracture behavior of cold-rolled Zr52.5Ti5Cu18Ni14.5Al10 bulk metallic glass under tensile loading10.1016/j.jallcom.2017.03.015 ↗
45. Evolution of shear bands, free volume and hardness during cold rolling of a Zr-based bulk metallic glass10.1016/j.actamat.2013.10.035 ↗
46. On room-temperature quasi-elastic mechanical behaviour of bulk metallic glasses10.1016/j.actamat.2017.02.049 ↗
47. Mechanical annealing in the homogeneous deformation of bulk metallic glass under elastostatic compression10.1016/j.scriptamat.2015.02.015 ↗
48. Mechanical relaxation-to-rejuvenation transition in a Zr-based bulk metallic glass10.1038/s41598-017-00768-7 ↗
49. Hardening of a metallic glass during cyclic loading in the elastic range10.1063/1.2919722 ↗
50. Atomistic mechanisms of cyclic hardening in metallic glass10.1063/1.4729941 ↗
51. Structural relaxation and rejuvenation in a metallic glass induced by shot-peening10.1080/09500830903337919 ↗