Joint effects of Ti and Cu additions on microstructure and mechanical properties of Zn-25Sn-xCu-yTi high-temperature Pb-free solders
Source abstract
Abstract
Abstract The aim of the present study is to investigate the joint effects of Ti and Cu additions on mechanical properties of high-temperature Zn–25Sn-x(0.1–0.4)Cu-y(0.01–0.04)Ti Pb-free solders. The microstructures, tensile properties, and micro-hardness of the cast Zn–25Sn-xCu-yTi solders were investigated. The results delineate that the appropriate combination of Cu and Ti additions can enhance the ultimate tensile strength and micro-hardness of the Zn–25Sn solder without a loss of ductility. The enhancement of mechanical properties was attributed to grain refining by Ti addition and solid-solution strengthening by Cu addition. Among the various xCu-yTi compositions investigated, the Zn–25Sn-(0.1–0.2Cu)-0.02Ti appear to be promising high-temperature Pb-free solder alternatives based on the mechanical properties evaluations.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Electronic Packaging and Soldering Technologies · Advanced Welding Techniques Analysis · Intermetallics and Advanced Alloy Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (71)
Show source-provided references
1. Lau · 1997 · 219
2. High melting Pb‐free solder alloys for die‐attach applications10.1002/adem.200500124 ↗
3. A brief review on high-temperature, Pb-free die-attach materials10.1007/s11664-018-6707-6 ↗
4. Experimental investigation of Ge-doped Bi-11Ag as a new Pb-free solder alloy for power die attachment10.1007/s11664-002-0016-8 ↗
5. Interfacial reactions of Si die attachment with Zn-Sn and Au-20Sn high temperature lead-free solders on Cu substrates10.1007/s11664-009-0770-y ↗
6. Improving the reliability of Si Die attachment with Zn-Sn-based high-temperature Pb-Free solder using a TiN diffusion barrier10.1007/s11664-009-0928-7 ↗
7. Improvement in joint reliability of SiC power devices by a diffusion barrier between Au-Ge solder and Cu/Ni(P)-metalized ceramic substrates10.1007/s11664-011-1661-6 ↗
8. High-temperature lead-free solders: properties and possibilities10.1007/s11837-009-0013-y ↗
9. Development of high-temperature solders: review10.1016/j.microrel.2012.02.018 ↗
10. High-temperature lead-free solder alternatives10.1016/j.mee.2010.12.072 ↗
11. Physics and materials challenges for lead-free solders10.1063/1.1517165 ↗
12. High temperature lead-free solder for microelectronics10.1007/s11837-001-0097-5 ↗
13. Design of lead-free candidate alloys for high-temperature soldering based on the Au-Sn system10.1016/j.matdes.2010.05.035 ↗
14. Research and prospect of binary high-temperature Pb-free solders10.1108/SSMT-07-2014-0015 ↗
15. Interface diffusion in eutectic Pb-Sn solder10.1016/S1359-6454(98)00348-6 ↗
16. Effect of alloying elements on the creep behavior of high Pb-based solders10.1016/j.msea.2010.10.083 ↗
17. High lead solder (over 85%) solder in the electronics industry: RoHS exemptions and alternatives10.1007/s10854-015-2940-4 ↗
18. In search of new lead-free electronic solders10.1007/BF02651363 ↗
19. Lead-free solders in microelectronics10.1016/S0927-796X(00)00010-3 ↗
20. Microstructure and mechanical properties of Pb-free solder alloys for low-cost electronic assembly: a review10.1007/BF02651361 ↗
21. Six cases of reliability study of Pb-free solder joints in electronic packaging technology10.1016/S0927-796X(02)00007-4 ↗
22. A review of mechanical properties of lead-free solders for electronic packaging10.1007/s10853-008-3125-9 ↗
23. A review: on the development of low melting temperature Pb-free solders10.1016/j.microrel.2014.02.025 ↗
24. Current problems and possible solutions in high-temperature lead-free soldering10.1007/s11665-012-0125-3 ↗
25. Superplastic creep of AuSn eutectic solder alloy10.1016/j.scriptamat.2016.03.031 ↗
26. Interfacial microstructure evolution and shear behavior of Au-20Sn/(Sn)Cu solder joints bonded at 250 °C10.1016/j.msea.2015.11.025 ↗
27. Au-Sn solder bumps with tungsten silicide based barrier metallization schemes10.1063/1.114347 ↗
28. A corrosion investigation of solder candidates for high-temperature applications10.1007/s11837-009-0089-4 ↗
29. Liquid-state and solid-state interfacial reactions of fluxless-bonded Au-20Sn/ENIG solder joint10.1016/j.jallcom.2008.01.077 ↗
30. The microstructure of eutectic Au-Sn solder bumps on Cu/electroless Ni/Au10.1007/s11664-001-0133-9 ↗
31. Interfacial reactions between Bi-Ag high-temperature solders and metallic substrates10.1007/BF02692565 ↗
32. Effects of Ag content on the mechanical properties of Bi-Ag alloys substitutable for Pb based solder
33. Zn-Al based alloys as Pb-free solders for die attach10.1007/s11664-002-0144-1 ↗
34. Characteristics of Zn-Al-Cu alloys for high temperature solder application10.2320/matertrans.MF200809 ↗
35. Shear strength of the Zn-Sn high-temperature lead-free solders10.1007/s10854-010-0279-4 ↗
36. The microstructure and mechanical properties of Zn-25Sn-XAl (X=0-0.09 wt%) high-temperature lead free solder10.1016/j.msea.2016.09.061 ↗
37. Impression creep behavior of Zn-Sn high-temperature lead-free solders10.1007/s11664-010-1359-1 ↗
38. Microstructural development of hypoeutectic Zn-(10-40)wt%Sn solder alloys and impacts of interphase spacing and macrosegregation pattern on hardness10.1016/j.jallcom.2015.05.195 ↗
39. Ball impact reliability of Zn-Sn high-temperature solder joints bonded with different substrates10.1007/s11664-013-2653-5 ↗
40. Effect of Cr addition on wetting behavior between Cu and high-temperature Zn-25Sn-0.15Al-0.1Ga-xCr Pb-Free Solder10.1007/s11664-014-3449-y ↗
41. Investigations of the wetting behaviors of Zn-25Sn, Zn-25Sn-XPr and Zn-25Sn-YAl high-temperature lead free solders in air and Ar ambient10.1016/j.jallcom.2015.06.185 ↗
42. Effects of Al, Pr additions on the wettability and interfacial reaction of Zn-25Sn solder on Cu substrate10.1007/s10854-016-5498-x ↗
43. Thermal properties and phase stability of Zn-Sn and Zn-In alloys as high temperature lead-free solder10.2320/matertrans.48.584 ↗
44. Effect of Ti addition on early-stage wetting behavior between Zn-25Sn-xTi solder and Cu10.1007/s11664-016-5109-x ↗
45. Effect of Ti addition on the mechanical properties of high temperature Pb-free solders Zn-25Sn-xTi10.1007/s10854-018-9176-z ↗
46. High-temperature mechanical properties of Zn-based high-temperature lead-free solders10.1007/s11664-018-6776-6 ↗
47. Wetting and IMC growth behavior between Cu substrate and Zn-25Sn-xCu-yTi high-temperature solder alloys10.1007/s11664-018-6742-3 ↗
48. The effects of Cu alloying on the microstructure and mechanical properties of Zn-25Sn-xCu (x = 0-1.0 wt%) high temperature Pb-free solders10.1016/j.msea.2019.02.053 ↗
49. Vibration fracture behavior of Sn-9Zn-xCu lead-free solders10.1007/s10853-006-0463-3 ↗
50. Reliability of wire-bonding and solder joint for high temperature operation of power semiconductor device10.1016/j.microrel.2007.07.102 ↗
51. Microstructural evolution of intermetallic compounds in TCNCP Cu pillar solder joints10.1007/s11664-015-4065-1 ↗
52. Zhang · 2006 · 95
53. Enhanced Vickers hardness by quasi-3D boron network in MoB210.1039/c3ra42741b ↗
54. Investigations on microhardness of Sn-Zn based lead-free solder alloys as replacement of Sn-Pb solder10.1016/j.jallcom.2004.08.079 ↗
55. The effect of undercooling on the microstructure and tensile properties of hypoeutectic Sn-6.5Zn-xCu Pb-free solders10.1016/j.matdes.2015.05.016 ↗
56. Effects of small amount of active Ti element additions on microstructure and property of Sn3.5Ag0.5Cu solder10.1016/j.msea.2012.08.031 ↗
57. Massalski · 1986 · vol. 2 · 2140
58. Massalski · 1986 · vol. 2 · 2078
59. Massalski · 1986 · vol. 1 · 986
60. Massalski · 1986 · vol. 1 · 965
61. Shackelford · 2016 · 15
62. Phase diagram of the Sn-Zn-Ti system10.1016/j.jallcom.2005.06.029 ↗
63. Thermodynamic study of the phase equilibria in the Sn-Ti-Zn ternary system10.1361/105497106X92826 ↗
64. The mechanism of grain refinement during solidification of Zn-Ti base alloy10.1007/BF02913842 ↗
65. Grain structures and coupled growth in Zn-Ti alloys10.1016/0022-0248(76)90017-8 ↗
66. Grain refinement of AZ31 magnesium alloy by titanium and low-frequency electromagnetic casting10.1007/s11661-007-9215-5 ↗
67. Effect of Ti addition on the microstructure and mechanical properties of cast Mg-Gd-Y-Zn alloys10.1016/j.msea.2017.10.006 ↗
68. Grain refinement of aluminium and its alloys by heterogeneous nucleation and alloying10.1179/095066001225001049 ↗
69. The effect of carbide and nitride additions on the heterogeneous nucleation behavior of liquid iron10.1007/BF02642799 ↗
70. Mechanical properties of Sn-Zn lead-free solder alloys based on the microstructure array10.1016/j.matchar.2009.11.012 ↗
71. Effect of small additions of alloying elements on the properties of Sn-Zn eutectic alloy10.1007/s11664-006-0227-5 ↗